Comprehensive research of the influence of climatic and operational factors on new generation epoxy binding and polymeric composite materials on its basis

Part 4. Full-scale weathering of polymeric composite materials on the basis of epoxy matrix
Nikolaev E.V., Barbotko S.L., Andreeva N.P., Pavlov M.R., Grachshencov D.V.
Nikolaev E.V., Barbotko S.L., Andreeva N.P., Pavlov M.R., Grachshencov D.V. Comprehensive research of the influence of climatic and operational factors on new generation epoxy binding and polymeric composite materials on its basis. Part 4. Full-scale weathering of polymeric composite materials on the basis of epoxy matrix // Proceedings of VIAM. 2016. No. 6. DOI: 10.18577/2307-6046-2016-0-6-11-11. URL: https://www.viam-works.ru/en/journal/2016/6/11
Keywords
polymeric composite materials, epoxy binding, layered carbon fiber, fiberglass, natural weathering test, surface profile.
Abstract

Stability of strength characteristics of polymeric composite materials (layered carbon fiber and fiberglass based on epoxy binder) by results of natural weathering tests in four climatic zones has been evaluated. Calculation of effective values of temperature and air humidity for each zone of exposure is carried out. The interrelation between change of mechanical characteristics of polymeric composite materials and change of surface profile of the samples determined by method of optical microscopy is shown. The work is executed within implementation of the complex scientific direction 18.3. «Modeling and forecasting of climatic tolerance» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznacheniya. II. Relaksaciya ishodnoj strukturnoj neravnovesnosti i gradient svojstv po tolshhine [Climatic aging of composite materials of aviation assignment. II. Relaxation of initial structural non-equilibrium and gradient of properties on thickness] // Deformaciya i razrushenie materialov. 2010. №12. S. 40–46.
  3. Kirillov V.N., Efimov V.A. Problemy issledovaniya klimaticheskoj stojkosti aviacionnyh nemetallicheskih materialov [Problems of research of climatic firmness of aviation non-metallic materials] // 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: yubilejnyj nauch.-tehnich. sb. M.: VIAM, 2007. S. 379–388.
  4. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznacheniya. I. Mehanizmy stareniya [Climatic aging of composite materials of aviation assignment. I. Aging mechanisms] // Deformaciya i razrushenie materialov. 2010. №11. S. 19–27.
  5. Kablov E.N., Startsev O.V. Fundamentalnye i prikladnye issledovaniya korrozii i stareniya materialov v klimaticheskih usloviyah (obzor) [The basic and applied research in the field of corrosion and ageing of materials in natural environments (review)] // Aviacionnye materialy i tehnologii. 2015. №4 (37). S. 38–52. DOI: 10.18577/2071-9140-2015-0-4-38-52.
  6. Kirillov V.N., Startsev O.V., Efimov V.A. Klimaticheskaya stojkost i povrezhdaemost polimernyh kompozicionnyh materialov, problemy i puti resheniya [Climatic firmness and damageability of polymeric composite materials, problems and solutions] //Aviacionnye materialy i tehnologii. 2012. №S. S. 412–423.
  7. Efimov V.A., Shvedkova A.K., Korenkova T.G., Kirillov V.N. Issledovanie polimernyh konstrukcionnyh materialov pri vozdejstvii klimaticheskih faktorov i nagruzok v laboratornyh i naturnyh usloviyah [Research of polymeric constructional materials at influence of climatic factors and loadings in laboratory and natural conditions] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №1. St. 05. Available at: http://www.viam-works.ru (accessed: February 01, 2016).
  8. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznacheniya. III. Znachimye faktory stareniya [Climatic aging of composite materials of aviation assignment. III. Significant factors of aging] // Deformaciya i razrushenie materialov. 2011. №1. S. 34–40.
  9. Kirillov V.N., Vapirov Yu.M., Drozd E.A. Issledovanie atmosfernoj stojkosti polimernyh kompozicionnyh materialov v usloviyah atmosfery teplogo vlazhnogo i umerenno teplogo klimata [Research of atmospheric firmness of polymeric composite materials in the conditions of the atmosphere of warm wet and moderately warm climate] // Aviacionnye materialy i tehnologii. 2012. №4. S. 31–38.
  10. Kirillov V.N., Efimov V.A., Nikolaev E.V., Shvedkova A.K., Korenkova T.G., Deev I.S. K voprosu o metodike provedeniya naturnyh klimaticheskih ispytanij polimernyh kompozicionnyh materialov [To question of technique of carrying out natural climatic tests of polymeric composite materials] // Sb. dokl. VIII nauch. konf. po gidroaviacii «Gidroaviasalon-2010». M., 2010. Ch. II. S. 102–106.
  11. Kirillov V.N., Efimov V.A., Shvedkova A.K., Aleksashin V.N., Zuev A.V., Nikolaev E.V. Issledovanie vliyaniya klimaticheskih faktorov i mehanicheskogo nagruzheniya na strukturu i mehanicheskie svojstva ugleplastika KMU-11TR [Research of influence of climatic factors and mechanical loading on structure and mechanical properties ugleplastika KMU-11TP] // Sb. dokl. VIII nauch. konf. po gidroaviacii «Gidroaviasalon-2010». M., 2010. Ch. II. S. 111–115.
  12. Nikolaev E.V., Kirillov V.N., Efimov V.A., Grashhenkov D.V. Moskovskij centr klimaticheskih ispytanij FGUP «VIAM» – regionalnyj centr ispytanij materialov v predstavitelnoj zone umerennogo klimata [The Moscow center of climatic tests of VIAM Federal State Unitary Enterprise – the regional center of tests of materials in representative zone of temperate climate] // Sb. dokladov IX nauch. konf. po gidroaviacii «Gidroaviasalon-2012». M., 2012. Ch. II. S. 202–208.
  13. Efimov V.A., Kirillov V.N., Dobryanskaya O.A., Nikolaev E.V., Shvedkova A.K. Metodicheskie voprosy provedeniya naturnyh klimaticheskih ispytanij polimernyh kompozicionnyh materialov [Methodical questions of carrying out natural climatic tests of polymeric composite materials] // Aviacionnye materialy i tehnologii. 2010. №4. S. 25–31.
  14. Kirillov V.N., Efimov V.A., Shvedkova A.K., Nikolaev E.V. Issledovanie vliyaniya klimaticheskih faktorov i mehanicheskogo nagruzheniya na strukturu i mehanicheskie svojstva PKM [Research of influence of climatic factors and mechanical loading on structure and the PCM mechanical properties] //Aviacionnye materialy i tehnologii. 2011. №4. S. 41–45.
  15. Kirillov V.N., Efimov V.A., Barbot'ko S.L., Nikolaev E.V. Metodicheskie osobennosti provedeniya i obrabotki rezultatov klimaticheskih ispytanij polimernyh kompozicionnyh materialov [Methodical features of carrying out and processing of results of climatic tests of polymeric composite materials] // Plasticheskie massy. 2013. №1. S. 37–41.
  16. Kirillov V.N., Efimov V.A., Gunyaev G.M., Krivonos V.V., Vapirov Yu.M. Osobennosti povedeniya nemetallicheskih materialov v morskih usloviyah [Features of behavior of non-metallic materials in sea conditions] // Gelendzhik-96: sb. dokl. M., 1996. S. 124–129.
  17. Kirillov V.N., Efimov V.A., Vapirov Yu.M., Hanin A.G. Vliyanie vlagi na svojstva polimernyh kompozicionnyh materialov [Influence of moisture on properties of polymeric composite materials] // Gelendzhik-98: sb. dokl. M.: VIAM, 1998. S. 208–211.
  18. Kirillov V.N., Efimov V.A., Kislyakova V.I., Baritko N.V., Savenkova A.V., Sytyj Yu.V., Kosteltsev V.V., Vapirov Yu.M. Vliyanie vozdejstviya vlazhnogo subtropicheskogo klimata na svojstva nemetallicheskih materialov [Influence of influence of humid subtropical climate on properties of non-metallic materials] // Sb. dokl. ІV nauch. konf. po gidroaviacii «Gidroaviasalon-2002». M.: VIAM, 2002. S. 214–221.
  19. Vapirov Yu.M., Kirillov V.N., Krivonos V.V. Zakonomernosti izmeneniya svojstv polimernyh kompozitov konstrukcionnogo naznacheniya pri dlitel'nom klimaticheskom starenii v svobodnom i nagruzhennom sostoyaniyah [Influence of influence of humid subtropical climate on properties of non-metallic materials] // V sb. dokl. VІ nauch. konf. po gidroaviacii «Gidroaviasalon-2006». M.: VIAM, 2006. Ch. ІІ. S.103–108.
  20. Kirillov V.N., Efimov V.A., Mazaev P.Yu. Metodika obrabotki rezul'tatov naturnyh ispytanij materialov [Technique of processing of results of natural tests of materials] // Sb. dokl. VІ nauch. konf. po gidroaviacii «Gidroaviasalon-2006». M.: VIAM, 2006. Ch. ІІ. S. 117–123.
  21. Nikolaev E.V., Barbotko S.L., Andreeva N.P., Pavlov M.R. Kompleksnoe issledovanie vozdejstviya klimaticheskih i ekspluatacionnyh faktorov na novoe pokolenie epoksidnogo svyazuyushhego i polimernyh kompozicionnyh materialov na ego osnove. Chast 3. Raschet energii aktivacii i teplovogo resursa polimernyh kompozicionnyh materialov na osnove epoksidnoj matricy [Comprehensive research of the influence of climatic and operational factors on new generation epoxy binding and polymeric composite materials on its basis. Part 3. Calculation of activation energy and thermal resource of polymeric composite materials on the basis of epoxy matrix] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №5. St. 11 Available at: http://www.viam-works.ru (accessed: May 16, 2016). DOI: 10.18577/2307-6046-2016-0-5-11-11.
  22. Nikolaev E.V., Barbotko S.L., Andreeva N.P., Pavlov M.R. Kompleksnoe issledovanie vozdejstviya klimaticheskih i ekspluatacionnyh faktorov na novoe pokolenie epoksidnogo svyazuyushhego i polimernyh kompozicionnyh materialov na ego osnove. Chast 2. Obosnovanie vybora rezhimov i provedenie teplovogo stareniya polimernyh kompozicionnyh materialov na osnove epoksidnoj matricy [Comprehensive research of the influence of climatic and operational factors on new generation epoxy binding and polymeric composite materials on its basis. Part 2. Substantiation of the choice of modes and conducting heat aging of polymeric composite materials based on epoxy matrix] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №1. St. 10. Available at: http://www.viam-works.ru (accessed: February 01, 2016). DOI: 10.18577/2307-6046-2016-0-1-10-10.
  23. Nikolaev E.V., Barbotko S.L., Andreeva N.P., Pavlov M.R. Kompleksnoe issledovanie vozdejstviya klimaticheskih i ekspluatacionnyh faktorov na novoe pokolenie epoksidnogo svyazuyushhego i polimernyh kompozicionnyh materialov na ego osnove. Chast 1. Issledovanie vliyaniya sorbirovannoj vlagi na epoksidnuyu matricu i ugleplastik na ee osnove [Comprehensive research of the influence of climatic and operational factors on new generation epoxy binding and polymeric composite materials on its basis. Part 1. Research of the influence of sorbate moisture on epoxy matrix and layered carbon fiber on its basis] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №12. St. 11. Available at: http://www.viam-works.ru (accessed: February 01, 2016). DOI: 10.18577/2307-6046-2015-0-12-11-11.
  24. Plastiki konstrukcionnogo naznacheniya (reaktoplasty) / pod. red. E.B. Trostyanskoj [Plastics of constructional assignment (thermosets) / ed. by E.B.Trostyanskaya]. M.: Himiya, 1974. 304 s.