Abstract

Development and application of aluminum alloys of new generation is an important task because of the active development of aerospace engineering. Weldable aluminum alloys are promising structural materials due to good complex of service characteristics and processability. The addition of rare earth elements to aluminium alloys allows significant improving the mechanical properties and at the same time the structure of deformed semi-finished products could be greatly changed. Taking into account the peculiarities of metallurgical production it is necessary to understand the impact of various parameters on the characteristics of semi-finished products. The results of studies of 1913 alloy bearing scandium in the process of rolling and heat treatment are shown. Research is executed within implementation of the complex scientific direction 8.1. «High strength weldable aluminium and low density Al–Li alloys with high fracture toughness» («Strategic directions of development of materials an

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  3. Illarionov Je.I., Kolobnev N.I., Gorbunov P.Z., Kablov E.N. Alyuminievye splavy v aviakosmicheskoj tehnike [Aluminum alloys in aerospace equipment]. M.: Nauka, 2001. 192 s.
  4. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Materials of new generation are necessary to Russia] // Redkie zemli. 2014. №3. S. 8–13.
  5. Zou Liang, Pan Qing-lin, He Yun-bin, Wang Chang-zhen. Effect of minor Sc and Zr addition on microstructures and mechanical properties of Al–Zn–Mg–Cu alloys // Transactions of Nonferrous Metals Society of China. 2006. №10. P. 340–344.
  6. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of modern and future high technologies] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 01. Available at: http://www.viam-works.ru (accessed: March 01, 2016).
  7. Han G.M., Nikiforov A.O., Zaharov V.V., Novikov I.I. Vliyanie soderzhaniya skandiya na strukturu i pokazateli sverhplastichnosti alyuminievyh splavov sistemy Al–Zn–Mg–Sc–Zr [Influence of the content of scandium on structure and indicators of superplasticity of aluminum alloys of Al–Zn–Mg–Sc–Zr system] // Tsvetnye Metally. 1993. №11. S. 55–57.
  8. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  9. Ryabov D., Kolobnev N., Samohvalov S. Effect of scandium addition on mechanical properties and corrosion resistance of medium strength Al–Zn–Mg(–Cu) alloy // Materials Science Forum. 2014. V. 794–796. P. 241–246.
  10. Ryabov D.K., Kolobnev N.I., Mahsidov V.V., Fomina M.A. O stabilnosti peresyshhennogo tverdogo rastvora listov splava 1913 pri zakalke [About stability of super-saturated solid solution of sheets of alloy 1913 when tempering] // Metallurgiya mashinostroeniya. 2012. №3. S. 30–33.
  11. Ryabov D.K., Kolobnev N.I., Samohvalov S.V., Vahromov O.V. Izmenenie mehanicheskih i korrozionnyh svojstv splava 1913 pri iskusstvennom starenii [Change of mechanical and corrosion properties of alloy 1913 at artificial aging] // Voprosy materialovedeniya. 2013. №4 (76). C. 24–29.
  12. Engler O., Sachot E., Ehrstro J.C., Reeves A., Shahani R. Recrystallisation and texture in hot deformed aluminium alloy 7010 thick plates // Mater. Sci. Technol. 1996. V. 12. P. 717–729.
  13. Zeng X.H., Ahmad M., Engler O. Texture gradient, average texture and plastic anisotropy in various Al–Li sheet alloys // Mater. Sci. Technol. 1994. V. 10. P. 581–591.
  14. Shamraj V.F., Grushko O.E., Jegiz I.V., Borovskih S.N. Kristallograficheskaya tekstura i struktura katanyh listov iz splava Al–Cu–Li [Crystallographic structure and structure of sheets from Al–Cu–Li alloy] // Metally. 2006. №2. S. 94–98.
  15. Visser R.F., Wolff I.M., Harty B.D. The Effect of Hot-Rolling Parameters on Texture Development and Microstructure in Aluminium AA5182 // Mat. Sci. Forum. 1994. V. 157–162. P. 1095–1102.
  16. Ryabov D.K., Kolobnev N.I., Samohvalov S.V., Mahsidov V.V. Vliyanie predvaritelnogo estestvennogo stareniya na svojstva splava 1913 v iskusstvenno sostarennom sostoyanii [Influence of preliminary natural aging on properties of alloy 1913 in artificially made old condition] // Aviacionnye materialy i tehnologii. 2013. №2. S. 8–11.
  17. Ryabov D.K., Kolobnev N.I. Izmenenie mehanicheskih svojstv splava 1913 pri dvuhstupenchatom iskusstvennom starenii [Change of mechanical properties of alloy 1913 at two-level artificial aging] // Aviacionnye materialy i tehnologii. 2013. №4. S. 3–7.
  18. Rometsch P.A., Zhang Y., Knight S. Heat treatment of 7xxx series aluminum alloys – some recent developments // Trans. Nonferrous Met. Soc. China. 2014. V. 24. P. 2003−2017.
  19. Oliveira Jr. A.F., de Barros M.C., Cardoso K.R., Travessa D.N. The effect of RRA on the strength and SCC resistanceon AA7050 and AA7150 aluminum alloys // Mater. Sci. Eng. A. 2004. V. 379. P. 321–326.
  20. Socorro Valdez, Suarez M., Fregoso O.A., Ju´arez-Islas J.A. Microhardness, Microstructure and Electrochemical Efficiency of an Al (Zn/xMg) Alloy after Thermal Treatment // Journal of Materials Science & Technology. 2012. V. 28 (3). Р. 255–260.