Acoustic polymeric materials of new generation (review)

Platonov M.M., Nesterova T.A., Sagomonova V.A.
Platonov M.M., Nesterova T.A., Sagomonova V.A. Acoustic polymeric materials of new generation (review) // Proceedings of VIAM. 2016. No. 4. DOI: 10.18577/2307-6046-2016-0-4-9-9. URL: https://www.viam-works.ru/en/journal/2016/4/9
Abstract

Article is devoted to the questions of the application and description of characteristics of new polymeric materials with acoustic properties developed at «The All-Russian Scientific-Research Institute of Aviation Materials» in recent years. The sound-proof porous-fibrous polymeric materials VTI-7 and VTI-12 as well as cellular acoustic structure VZMK-1 on their basis are considered. Properties of sound-proof materials of VTP-1V-type intended for reduction of negative vibration impact and structural noise on passengers, pilots and microelectronics are described. Properties of the heat-sound-proof material VPP-1 on the basis of the polyimide being today material, exceeding at properties the earlier widely used material ATM-1 are considered. Work is executed within implementation of the complex scientific direction 15.3. «Materials and coatings for protection against EMЕ, impact, vibrating, acoustic and electric influences» («The strategic directions of development of materials and tech

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Sytyj Yu.V., Sagomonova V.A., Maksimov V.G., Babashov V.T. Zvukoteploizoliruyushhij material gradientnoj struktury VTI-22 [VTI-22 sound and thermal insulation material of gradient structure] // Aviacionnye materialy i tehnologii. 2013. №2. S. 47–49.
  3. Kablov E.N. Materialy dlya izdeliya «Buran» – innovacionnye resheniya formirovaniya shestogo tehnologicheskogo uklada [Materials for «Buran» spaceship – innovative solutions of formation of the sixth technological mode] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
  4. Kondrashov E.K., Kuzmin V.V., Minakov V.T., Ponomareva E.A. Netkanye materialy na osnove termostojkih polimernyh volokon i mezhplitochnye uplotneniya [Nonwoven materials based on heat-resistant polymer fibers and intertiled sealants] // Aviacionnye materialy i tehnologii. 2013. № S1. S. 51–55.
  5. Sytyj Yu.V., Kislyakova V.I., Sagomonova V.A., Antyufeeva N.V. Perspektivnyj vibropogloshhayushhij material VTP-3V [Perspective vibropogloshchayushchy material VTP-3B] // Aviacionnye materialy i tehnologii. 2012. №3. S. 47–49.
  6. Kablov E.N. Himiya v aviacionnom materialovedenii [Chemistry in aviation materials science ] // Rossijskij himicheskij zhurnal. 2010. T. LIV. № 1. S. 3–4.
  7. Farafonov D.P., Migunov V.P. Izgotovlenie poristovoloknistogo materiala sverhnizkoj plotnosti dlya zvukopogloshhajushhih konstrukcij aviacionnyh dvigatelej [Manufacturing of porous fibrous material of ultralow density for sound-proof designs of aircraft engines] // Aviacionnye materialy i tehnologii. 2013. №4. S. 26–30.
  8. Sun F.G., Chen H.L., Wu J.H., Feng K. Sound absorbing characteristics of fibrous metal materials at high temperatures // Appl. Acoust. 2010. V. 711. Р. 221–235.
  9. Migunov V.P., Farafonov D.P. Issledovanie osnovnyh ekspluatacionnyh svojstv novogo klassa uplotnitelnyh materialov dlya protochnogo trakta GTD [Research of the main operational properties of new class of sealing materials for flowing path of GTE] // Aviacionnye materialy i tehnologii. 2011. №3. S. 15–20.
  10. Migunov V.P., Lomberg B.S. Poristovoloknistye metallicheskie materialy dlya zvukopogloshhayushhih i uplotnitelnyh konstrukcij [Poristovoloknistye metal materials for sound-proof and sealing designs] / V sb.: 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: yubilejnyj nauch.-tehnich. sb. M.: VIAM, 2007. S. 270–275.
  11. Serov M.M., Borisov B.V. Poluchenie metallicheskih volokon i poristyh materialov iz nih metodom jekstrakcii visyashhej kapli rasplava [Receiving metal fibers and porous materials from them method of extraction of hanging drop melt] // Tehnologiya legkih splavov. 2007. №3.
  12. S. 62–65.
  13. Borisov B.V. Razrabotka tehnologii polucheniya volokon i poristyh materialov iz zharostojkih splavov metodom ekstrakcii visyashhej kapli rasplava: avtoref. dis. … kand. tehn. nauk [Development of technology of receiving fibers and porous materials from heat resisting alloys method of extraction of hanging drop melt: thesis … cand. of tech. sci.]. M.: MATI–RGTU im. K.E. Ciolkovskogo, 2011. 19 s.
  14. Migunov V.P., Farafonov D.P., Degovets M.L. Poristovoloknistyj material sverhnizkoj plotnosti na osnove metallicheskih volokon [Porous fibrous material of ultralow density on the basis of metal fibers] // Aviacionnye materialy i tehnologii. 2012. №4. S. 38–41.
  15. Zhengping X., Jilei Z., Huiping T., Qingbo A., Hao Z., Jianyong W., Cheng L. Progress of application researches of porous fiber metals // Materials. 2011. №4. Р. 816–824.
  16. Platonov M.M., Zhelezina G.F., Nesterova T.A. Poristovoloknistye polimernye materialy dlya izgotovleniya shirokodiapazonnyh ZPK i issledovanie ih akusticheskih svojstv [Porous fibrous polymer materials for wide range sound absorbing structures and investigation of their acoustical properties] // Trudy VIAM : elektron. nauch-tehnih. zhurn. 2014. №6. St. 09. Available at: http://viam-works.ru (accessed: July 07, 2015). DOI: 10.18577/2307-6046-2014-0-6-9-9.
  17. Bejder E.Ya., Gureeva E.V., Petrova G.N. Penopoliimidy [Foam polyimide] // Vse materialy. Enciklopedicheskij spravochnik. 2012. №6. S. 2–8.
  18. Beider E.Ya., Petrova G.N., Izotova T.F., Gureeva E.V. Kompozicionnye termoplastichnye materialy i penopoliimidy [Thermoplastic composite materials and foam polyimides] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №11. St. 01. Available at: http://viam-works.ru (accessed: July 07, 2015).
  19. Cherkasov V.D., Yurkin Yu.V., Nadkin E.A. Vibropogloshhayushhie materialy ekstra-klassa [Vibropogloshchayushchiye extra-class materials]. Saransk: Izd-vo Mordovskogo un-ta, 2007. S. 17–19.
  20. Myasnikova M.P., Pozamontir A.G., Gromov V.V. Metody regulirovaniya vibropogloshhayushhih svojstv polimernyh materialov [Methods of regulation of vibropogloshchayushchy properties of polymeric materials] / V sb. materialov seminara «Vibropogloshhayushhie materialy i pokrytiya i ih primenenie». 1974. S. 41–45.
  21. Smotrova S.A. Analiz vibropogloshhayushhih svojstv polimernyh materialov s celyu ocenki vozmozhnogo ih primeneniya v konstrukciyah dempferov i dinamicheski podobnyh modelej [The analysis of vibropogloshchayushchy properties of polymeric materials for the purpose of assessment of their possible application in designs of dampers and dynamically similar models] // Plasticheskie massy. 2002. №3. S. 39–45.
  22. Ionov A.V. Sredstva snizheniya vibracii i shuma na sudah [Means of decrease in vibration and noise on vessels]. S-Pb.: GNC RF CNII im. A.N. Krylova, 2000. 123 s.
  23. Sytyj Yu.V., Sagomonova V.A., Kislyakova V.I., Bolshakov V.A. Vibropogloshhayushhie materialy na osnove termojelastoplastov [Vibro absorbing materials on the basis of thermoelastoplastics] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №3. St. 06. Available at: http://viam-works.ru (accessed: July 07, 2015).