Evaluation of porosity of chromecarbide coatings on different classes of structural materials using measurement of systems stationary potential

Semenychev V.V., Smirnova T.B.
Semenychev V.V., Smirnova T.B. Evaluation of porosity of chromecarbide coatings on different classes of structural materials using measurement of systems stationary potential // Proceedings of VIAM. 2016. No. 4. DOI: 10.18577/2307-6046-2016-0-4-7-7. URL: https://www.viam-works.ru/en/journal/2016/4/7
Abstract

Stationary potentials of pyrolytic chromecarbide coating (PCCC), deposited on samples of various structural materials, like steel 30HGSA, titanium alloy VT6 and aluminum alloy D16ch.-T have been measured in 3% aqueous NaCl solution. Thickness of chromecarbide coatings ranged from 6 to 30 μm. In order to eliminate the influence of substrate on formation of stationary potential the PCCC was deposited on glass samples. The potential steady-stated in 72 hours was taken as stationary. Additionally to coated samples the initial samples of selected structural alloys were studied. Research has shown that PCCC is a cathode coating and the value of its stationary potential is +285 mV. Stationary potentials of the used structural materials have negative values, which range from -110 to -730 mV. Analysis of experimental data showed that the decrease in thickness of coating leads to a shift of the value of stationary potential to negative range, i. e. at small coating thicknesses substrate through

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N. Aviacionnoe materialovedenie v XXI veke. Perspektivy i zadachi [Aviation materials science in the XXI century. Perspectives and tasks] / V kn. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2002: yubilejnyj nauch.-tehnich. sb. M.: MISIS–VIAM, 2002. S. 23–47.
  3. Kablov E.N., Startsev O.V., Medvedev I.M. Obzor zarubezhnogo opyta issledovanij korrozii i sredstv zashhity ot korrozii [Review of international experience on corrosion and corrosion protection] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 76–87.
  4. Kablov E.N. Himiya v aviacionnom materialovedenii [Chemistry in aviation materials science] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  5. Gribov B.G., Domrachev G.A., Zhuk B.V. Osazhdenie plenok i pokrytij razlozheniem metalloorganicheskih soedinenij [Sedimentation of films and coverings decomposition of organometallic compounds]. M.: Nauka, 1981. 324 c.
  6. Kostenkov V.A., Krasheninnikov V.N., Shhennikov V.I. i dr. Vliyanie mehanicheskih svojstv metalla podlozhki na formirovanie piroliticheskih hromovyh pokrytij [Influence of mechanical properties of metal of substrate on forming of pyrolitic chrome platings] // Fizika i himiya obrabotki materialov. 1979. Vyp. 2. S. 109–113.
  7. Panarin A.V. Piroliticheskie karbidohromovye pokrytiya. Tehnologiya polucheniya i svojstva [Pyrolitic carbide chrome platings. Technology of receiving and property] // Aviacionnye materialy i tehnologii. 2011. №4. S. 14–18.
  8. Koshelev V.N., Semenychev V.V., Panarin A.V. Ekologicheski bezopasnyj tehnologicheskij process naneseniya zashhitnyh piroliticheskih alyuminievyh pokrytij bez navodorozhivaniya stalnoj podlozhki [Ecologically safe technological process of drawing protective pyrolitic aluminum coverings without hydrogen saturation of steel substrate] // Izvestiya Samarskogo nauchnogo centra RAN. 2008. T. 1. Specialnyj vypusk. S. 18–23.
  9. Sokolov V.F., Yurchenko A.D., Arzhannikova E.V., Shipigina L.S. Zashhitnoe piroliticheskoe hromovoe pokrytie. Tehnologiya, svojstva, primenenie: Obzor [Protective pyrolitic chrome plating. Technology, properties, application: review]. M.: CNIIatominform, 1989. 72 c.
  10. Gafurov I.I., Panarin A.V. Piroliticheskoe hromirovanie kak sposob uprochnyayushhej obrabotki litejnyh alyuminievyh splavov s vysokim soderzhaniem kremniya [Pyrolitic chromizing as way of strengthening processing of cast aluminum alloys with the high silicon content] // Izvestiya Samarskogo nauchnogo centra RAN. 2015. T. 16. №6 (2). S. 412–415.
  11. Semenychev V.V., Salahova R.K., Smirnova T.B. Ocenka tokov korrozii razlichnyh par materialov metodom pryamogo izmereniya [Assessment of currents of corrosion of different couples of materials method of direct measurement] // Praktika protivokorrozionnoj zashhity. 2015. №2 (76). S. 44–50.
  12. Vulf B.K., Romadin K.P. Aviacionnoe materialovedenie [Aviation materials science]. M.: Mashinostroenie, 1967. 394 c.
  13. Tupicyn G.I., Mhitaryan L.S. Issledovanie zashhitnyh svojstv metallicheskih pokrytij [Research of protective properties of metallic coatings]. M.: Oborongiz, 1957. S. 145–183.
  14. Kostrzhickij A.I., Karpov V.F., Kabanchenko M.P. i dr. Spravochnik operatora ustanovok po naneseniyu pokrytij v vakuume [The directory of the operator of installations on drawing coverings in vacuum]. M.: Mashinostroenie, 1991. 176 c.
  15. Semenychev V.V., Smirnova T.B. O vozmozhnosti ocenki poristosti pokrytij potenciostaticheskimi metodami [About possibility of assessment of porosity of coverings potentsiostatichesky methods] // Aviacionnye materialy i tehnologii. 2009. №2. S. 7–10.