Abstract
The choice of optimum flame retardant and its content in rubber mix is made for creation of self-extinguishing rubber on basis of ethylenepropylene-diene rubber (EPDM). The structure and complex of physical-mechanical and operational properties of rubber on the basis of EPDM with lowered combustibility of optimum composition are studied. Results of research of the influence of particle size of flame retardants – aluminum and magnesium hydroxides on curing processes, combustibility, physical-mechanical characteristics and rubber microstructure on the basis of EPDM are provided.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
- Kablov E.N. Himiya v aviacionnom materialovedenii [Chemistry in aviation materials science] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
- Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] // Nauka i zhizn. 2010. №4. S. 2–7.
- Istoriya aviacionnogo materialovedeniya. VIAM–80 let: gody i lyudi / pod. obshh. red. E.N. Kablova [History of aviation materials science. VIAM-80 years: years and people / general editorship by E.N.Kablov]. M.: VIAM, 2012. S. 346–348.
- Bolshoj spravochnik rezinshhika: spravochnik v 2 ch. [Big directory of rezinshchik: the directory in 2 parts]. M.: OOO «Tehinform», 2012. 1385 s.
- Tehnologiya reziny: recepturostroenie i ispytaniya. Per. s angl. / pod red. Dzh.S. Dika [Technology of rubber: compounding structure and tests. Trans. from English / editorship by J. S. Dick]. SPb.: Nauchnye osnovy i tehnologii, 2010. 617 s.
- Alifanov E.V., Chaykun A.М., Venediktova M.A., Naumov I.S. Osobennosti receptur rezin na osnove etilenpropilenovyh kauchukov i ih primenenie v izdeliyah specialnogo naznacheniya (obzor) [Specialties of rubber compounds recipes based on ethylene-propylene rubbers and their application in the articles for special purpose (review)] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 51–55.
- Gorenie, destrukciya i stabilizaciya polimerov / pod red. G.E. Zaikova [Burning, destruction and stabilization of polymers / editorship by G.E. Zaikov]. SPb.: Nauchnye osnovy i tehnologii, 2008. 422 s.
- Goryuchest i dymoobrazujushhaya sposobnost polimernyh materialov aviacionnogo naznacheniya / pod red. R.E. Shalina, B.I. Panshina [Combustibility and smoke-generating ability of polymeric materials of aviation assignment / editorship by R.E. Shalin, B.I.Panshina]. M.: VIAM, 1986. 104 s.
- Kodolov V.I. Zamedliteli goreniya polimernyh materialov [Decelerators of burning of polymeric materials]. M.: Himiya, 1980. 269 s.
- Barbotko S.L., Shurkova E.N., Volny O.S., Skrylyov N.S. Ocenka pozharnoj bezopasnosti polimernyh kompozicionnyh materialov dlya vneshnego kontura aviacionnoj tehniki [Evolution of polymer composite fire-safety for the outer contour of aeronautical engineering] // Aviacionnye materialy i tehnologii. 2013. №1. S. 56–59.
- Barbotko S.L., Shurkova E.N. O pozharnoj bezopasnosti materialov, ispolzuemyh dlya izgotovleniya vneshnego kontura samoletov [About fire safety of the materials used for manufacturing of external circuit of airplanes] // Pozharovzryvobezopasnost'. 2011. T. 20. №10. S. 19–24.
- Petrova G.N., Beider E.Ya., Perfilova D.N., Rumyantseva T.V. Pozharobezopasnye litevye termoplasty i termojelastoplastyv [Fire safety of injection molding thermoplastics and TPE materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №11. St. 02. Available at: http://www.viam-works.ru (accessed: December 01, 2015).
- Petrova G.N., Rumyantseva T.V., Beider E.Ya. Vliyanie modificirujushhih dobavok na pozharobezopasnye svojstva i tehnologichnost polikarbonata [Influence of modifying additives on fireproof properties and technological effectiveness of polycarbonate] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №6. St. 06. Available at: http://www.viam-works.ru (accessed: December 01, 2015).
- Clough R.L. Aging Effects on Fire-Retardant Additives in Polymers // Journal of Polymer Science: Polymer Chemistry Edition. 1983. V. 21. P. 767–780.
- Shurkova E.N., Volny O.S., Izotova T.F., Barbotko S.L. Issledovanie vozmozhnosti snizheniya teplovydeleniya pri gorenii kompozicionnogo materiala putem izmeneniya ego struktury [Research of possibility of decrease in heat release when burning composite material by change of its structure] // Aviacionnye materialy i tehnologii. 2012. №1. S. 27–30.
- Barbotko S.L. Pozharobezopasnost aviacionnyh materialov [Fire safety of aviation materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 431–439.
- Barbotko S.L. Puti obespechenija pozharnoj bezopasnosti aviacionnyh materialov [Ways of ensuring fire safety of aviation materials] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 121–126.
- Naumov I.S., Petrova A.P., Chaikun A.M. Reziny uplotnitelnogo naznacheniya i snizhenie ih goryuchesti [Rubbers of sealing assignment and decrease in their combustibility] // Vse materialy. Enciklopedicheskij spravochnik. 2013. №5. S. 28–35.
- Mitina E.L., Naumov I.S. Samozatuhayushhij material na osnove kombinacii hloroprenovogo i butadienovogo kauchukov [Self-fading material on the basis of combination of chloroprene and butadiyene rubbers] // Klei. Germetiki. Tehnologii. 2012. №6. S. 9–12.
- Mitina E.L., Barbotko S.L. Vliyanie antipirenov na gorjuchest dekorativnyh rezin na osnove kombinacii butadien-stirolnogo i butadienovogo kauchukov [Influence of antipyrines on combustibility of decorative rubbers on the basis of combination of styrenr-butadiene and butadiyene rubbers] // Klei. Germetiki. Tehnologii. 2012. №3. S. 17–21.
- Naumov I.S., Chajkun A.M., Eliseev O.A. Rossijskie i mezhdunarodnye standarty na metody ispytanij rezin, syryh rezinovyh smesej i vysokomolekuljarnyh kauchukov [The Russian and international standards on test methods of rubbers, crude rubber mixes and high-molecular rubbers] // Vse materialy. Enciklopedicheskij spravochnik. 2014. № 11. S. 4–13.
- Aviacionnye pravila. Chast 25 Normy letnoj godnosti samoletov transportnoj kategorii. 3-e izd.: utv. Sovetom po aviacii i ispolzovaniyu vozdushnogo prostranstva 11.12.2008 [Aviation rules. Part 25 of Standard of the flight validity of airplanes of transport category. 3rd ed.: approved by Council for aircraft and use of air space. November 12, 2008.]. M.: OAO «Aviaizdat». 2009. 274 s.
- OST1 90094–79. Polimernye materialy. Metod opredeleniya goryuchesti dekorativno-otdelochnyh i konstrukcionnyh polimernyh materialov [OST1 90094-79. Polymeric materials. Method of determination of combustibility of decorative and finishing and constructional polymeric materials]. M.: Tipografiya CAGI, 1980. 8 s.
- Eliseev O.A., Krasnov L.L., Zajceva E.I., Savenkova A.V. Razrabotka i modificirovanie elastomernyh materialov dlya primeneniya vo vseklimaticheskih usloviyah [Development and modifying of elastomeric materials for application in all weather conditions] // Aviacionnye materialy i tehnologii. 2012. №S. S. 309–314.
- Chaikun A.M., Eliseev O.A., Naumov I.S., Venediktova M.A. Osobennosti morozostojkih rezin na osnove razlichnyh kauchukov [Features of old-resistant rubbers on the basis on different unvulcanized rubbers] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №12. St. 04. Available at: http://www.viam-works.ru (accessed: December 01, 2015).
- Naumov I.S., Barbotko S.L., Petrova A.P., Malysheva G.V. Vliyanie antipirenov na svojstva uplotnitelnoj reziny na osnove etilenpropilen-dienovogo kauchuka (EPDK) [Influence of antipyrines on properties of sealing rubber on the basis of etilenpropilen-diene rubber (EPDK)] //Vse materialy. Jenciklopedicheskij spravochnik. 2014. №5. S. 31–34.
- Naumov I.S., Petrova A.P., Eliseev O.A., Barbotko S.L. Eksperimentalnye issledovaniya v oblasti sozdaniya kremnijorganicheskih rezin s ponizhennoj goryuchestyu [Experimental research in the field of development of organic silicon rubbers with low flammability] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №10. St. 09. Available at: http://www.viam-works.ru (accessed: December 01, 2015).DOI: 10.18577/2307-6046-2015-0-10-9-9.