Abstract

Magnesium alloys in a review article were examined. They are divided, depending on its application, as follows: high strength, heat resistant, corrosion resistant alloys. According to their purpose these alloys belong to different systems: Mg–Al–Zn, Mg–Zn–Zr, Mg–RE. The examples of alloys belonging to the above groups, their basic properties (tensile strength, yield strength, corrosion resistance, long-term strength, impact strength) and application fields were considered in the article. The work is executed within the implementation of the complex scientific direction 10.10. «Energy-efficient, resource-saving and additive technology of deformed semi-finished products and shaped castings from magnesium and aluminum alloys» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Reference list
  1. Kablov E.N. Aviacionnoe materialovedenie: itogi i perspektivy [Aviation materials science: results and perspectives] // Vestnik Rossijskoj akademii nauk. 2002. T. 72. №1. S. 3–12.
  2. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  3. Kablov E.N. VIAM: prodolzhenie puti [VIAM: way continuation] // Nauka v Rossii. 2012. №3. S. 36–44.
  4. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
  5. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of modern and future high technologies] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 01. Available at: http://www.viam-works.ru (accessed: January 25, 2016).
  6. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  7. Kornysheva I.S., Volkova E.F., Goncharenko E.S., Muhina I.Yu. Perspektivy primeneniya magnievyh i litejnyh alyuminievyh splavov [Perspectives of application of magnesium and cast aluminum alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 212–222.
  8. Goncharenko E.S., Alyabev I.P., Trapeznikov A.V., Ogorodov D.V. Tehnologiya polucheniya fasonnyh otlivok iz tehnologicheskogo germetichnogo splava AL4MS [Technology of receiving mold castings from technological tight alloy AL4MS] // Litejshhik Rossii. 2014. №7. S. 12–14.
  9. Basargin O.V., Shheglova T.M., Nikitina V.Yu., Svistunov V.I. Sposob opredeleniya prochnosti pri rastyazhenii monokristallicheskih volokon Al2O3 pri temperature 1400°S [High-temperature tensile strength determination of single crystal alumina fibers] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №4. St. 03. Available at: http://www.viam-works.ru (accessed: January 25, 2016). DOI: 10.18577/2307-6046-2014-0-4-3-3.
  10. Duyunova V.A., Goncharenko N.S., Muhina I.Yu., Uridiya Z.P., Volkova E.F. Nauchnoe nasledie akademika I.N. Fridlyandera. Sovremennye issledovaniya magnievyh i litejnyh alyuminievyh splavov v VIAM [Scientific heritage of academician I.N.Fridlyandera. Modern researches of magnesium and cast aluminum alloys in VIAM] // Tsvetnye metally. 2013. №9. S. 71–78.
  11. Korchagina V.A. Radi kachestva magnievyh otlivok [For the sake of quality of magnesian casting] // Inzhenernaya gazeta. 2006. №33–34. S. 5.
  12. Duyunova V.A. Magnievye splavy: nauchnye issledovaniya Centralnogo aerogidrodinamicheskogo instituta i Vsesoyuznogo instituta aviacionnyh materialov. 1930–1935 gg. [Magnesium alloys: scientific researches of the Central aero hydrodynamic institute and All-Union institute of aviation materials. 1930-1935.] // Istoriya nauki i tehniki. 2012. №10. S. 27–35.
  13. Karimova S.A., Pavlovskaya T.G. Razrabotka sposobov zashhity ot korrozii konstrukcij, rabotajushhih v usloviyah kosmosa [Development of ways of corrosion protection of the designs working in the conditions of space] // Trudy VIAM: electron. nauch.-tehnich. zhurn. 2013. №4. St. 02. Available at: http://www.viam-works.ru (accessed: January 25, 2016).
  14. Kozlov I.A., Karimova S.A. Korrozija magnievyh splavov i sovremennye metody ih zashhity [Corrosion of magnesium alloys and modern methods of their protection] // Aviacionnye materialy i tehnologii. 2014. №2. S. 15–20. DOI: 10.18577/2071-9140-2014-0-2-15-20.
  15. Duyunova V.A. Metody zashhity magnievyh splavov v otechestvennom litejnom proizvodstve s 1930-h gg. do nastoyashhego vremeni [Methods of protection of magnesium alloys in domestic foundry production since the 1930th so far] // Litejshhik Rossii. 2010. №10. S. 35–37.
  16. Duyunova V.A., Uridiya Z.P. Issledovanie vosplamenyaemosti litejnyh magnievyh splavov sistemy Mg–Zn–Zr [Research of inflammability of cast magnesium alloys of Mg-Zn-Zr system ] // Litejshhik Rossii. 2012. №11. S. 21–23.
  17. Kablov E.N. Himiya v aviacionnom materialovedenii [Chemistry in aviation materials science] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  18. Kablov E.N., Muhina I.Yu., Korchagina V.A. Prisadochnye materialy dlya formovochnyh smesej pri lite magnievyh splavov [Additives materials for forming mixes when molding magnesium alloys ] // Litejnoe proizvodstvo. 2007. №5. S. 15–18.
  19. Duyunova V.A., Muhina I.Yu., Uridiya Z.P. Novye protivoprigarnye prisadochnye materialy dlya litejnyh form magnievyh otlivok [New nonstick additives materials for casting molds of magnesian casting] // Litejnoe proizvodstvo. 2009. №9. S. 18–21.
  20. Duyunova V.A., Kozlov I.A. Holodnotverdeyushhie formovochnye smesi: perspektivy ispolzovaniya pri lite magnievyh splavov [Cold hardening forming mixes: use perspectives when molding magnesium alloys] // Vse materialy. Enciklopedicheskij spravochnik. 2011. №1. S. 41–43.
  21. Muhina I.Yu., Duyunova V.A., Uridiya Z.P. Perspektivnye litejnye magnievye splavy [Perspective cast magnesium alloys] // Litejnoe proizvodstvo. 2013. №5. S. 2–5.
  22. Frolov A.V., Muhina I.Yu., Duyunova V.A., Uridiya Z.P. Vliyanie tehnologicheskih parametrov plavki na strukturu i svojstva novyh magnievyh splavov [Influence of technological parameters of melting on structure and property of new magnesium alloys] // Metallurgiya mashinostroeniya. 2014. №2. S. 26–29.
  23. Uridiya Z.P., Mukhina I.Y., Frolov A.V., Leonov A.A. Issledovanie mikrostruktury magnievo-cirko-nievoj ligatury i zharoprochnogo litejnogo magnievogo splava ML10 [Study of microstructure of magnesium-zirconium master alloy and heat-resistant magnesium alloy ML10] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №10. St. 06. Available at: http://www.viam-works.ru (accessed: January 28, 2016). DOI: 10.18577/2307-6046-2015-0-10-1-1.
  24. Leonov A.A., Duyunova V.A., Stupak E.V., Trofimov N.V. Lite magnievyh splavov v razovye formy, poluchennye novymi metodami [Casting of magnesium alloys in disposable moulds produced by new methods] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №12. St. 01. Available at: http://www.viam-works.ru (accessed: January 28, 2016). DOI: 10.18577/2307-6046-2014-0-12-1-1.