Optimisation of structure of hybrid composition materials for aircraft

Lavrov A.V., Erasov V.S., Podzhivotov N.Y., Avtaev V.V.
Lavrov A.V., Erasov V.S., Podzhivotov N.Y., Avtaev V.V. Optimisation of structure of hybrid composition materials for aircraft // Proceedings of VIAM. 2016. No. 11. DOI: 10.18577/2307-6046-2016-0-11-7-7. URL: https://www.viam-works.ru/en/journal/2016/11/7
Keywords
composition laminate materials, hybrid composition materials.
Abstract

Layered hybrid metal-plastic composite materials are considered in the article from the point of view of optimisation of their composition for various conditions of functioning. Positioning and thickness influence of high-rigid layers on cylindrical rigidity of the composite is shown at a symmetric and asymmetric (unilateral) bend. Recommendations for choice of hybrid composites for various kinds of loads are given. The work is executed within the implementation of the complex scientific direction 6. «Layered metal-plastic, bimetallic and hybrid materials» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Materials of new generation are necessary to Russia] // Redkie zemli. 2014. №3. S. 813.
  3. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  4. Kablov E.N., Antipov V.V., Senatorova O.G. Sloistye alyumostekloplastiki SIAL-1441 i sotrudnichestvo s AIRBUS i TU DELFT [Layered aluminum fibreglasses SIAL-1441and cooperation with AIRBUS and TU DELFT] // Tsvetnye metally. 2013. №9 (849). S. 50–53.
  5. Oreshko E.I., Erasov V.S., Podjivotov N.Yu. Vybor shemy raspolozheniya vysokomodulnyh sloev v mnogoslojnoj gibridnoj plastine dlya ee naibolshego soprotivleniya potere ustojchivosti [Arrangement of high-modular layers in a multilayer hybrid plate for its greatest resistance to stability loss] // Aviacionnye materialy i tehnologii. 2014. №S4. S. 109–117.
  6. Arislanov A.A., Goncharova L.J., Nochovnaya N.А., Goncharov V.A. Perspektivy ispolzovaniya titanovyh splavov v sloistyh kompozicionnyh materialah [Prospects for the use of titanium alloys in laminated composite materials] //Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №10. St. 04. Available at: http://www.viam-works.ru (accessed: February 16, 2016). DOI: 10.18577/2307-6046-2015-0-10-4-4.
  7. Antipov V.V., Senatorova O.G., Sidelnikov V.V. Issledovanie pozharostojkosti sloistyh gibridnyh alyumostekloplastikov klassa SIAL [Research of fire firmness layered hybrid aluminum fibreglasses of SIAL’s class] // Aviacionnye materialy i tehnologii. 2011. №3. S. 36–41.
  8. Antipov V.V. Tehnologichnyj alyuminijlitievyj splav 1441 i sloistye gibridnye kompozity na ego osnove [Technological aluminum lithium alloy 1441 and layered hybrid composites on its basis] // Metallurg. №5. 2012. S. 36–39.
  9. Antipov V.V., Senatorova O.G., Lukina N.F. i dr. Sloistye metallopolimernye kompozicionnye materialy [Layered metalpolymeric composite materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 226–230.
  10. Gayamov A.M., Budinovskij S.A., Muboyadzhyan S.A., Kosmin A.A. Vybor zharostojkogo pokrytija dlya zharoprochnogo nikelevogo renij-rutenijsoderzhashhego splava marki VZhM4 [Selection of heat-resistant coating with metalloceramic barrier layer for protection of Re-Ru nickel-based superalloy] // Trudy VIAM : elektron. nauch.-tehnich. zhurn. 2014. №1. St. 01. Available at: http://viam-works.ru (accessed: February 14, 2016). DOI: 10.18577/2307-6046-2014-0-1-4-4.
  11. Belous V. Ya., Loshhinina A.O., Varlamova V.E., Nikitin Ya.Yu. Korrozionna ya stojkost i podgotovka poverhnosti holodnokatanoj lenty iz stali VNS-9-Sh dl ya izgotovleni ya MPKM [Corrosion resistance and preparation of a surface of a cold rolled tape from VNS9-Sh steel for production of metalpolymeric composite material] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №11. St. 10. Available at: http://www.viam-works.ru (accessed: Febru-ary 14, 2016). DOI: 10.18577/2307-6046-2015-0-11-10-10.
  12. Bulanov I.M., Vorobej V.V. Tehnologiya raketnyh i aerokosmicheskih konstrukcij iz kompozicionnyh materialov: ucheb. dlya vuzov [Technology of rocket and space designs from composite materials: textbook for higher education institutions]. M.: Izd-vo MGTU im. N.E. Baumana, 1998. 516 s.
  13. Propedevticheskaya stomatologiya: ucheb. dlya medicinskih vuzov / pod red. E.A. Bazikyana [Propaedeutic stomatology: textbook for medical higher education institutions / ed. by E.A. Bazikyan]. M.: GEOTAR-Media, 2008. 768 s.
  14. Zhelezina G.F. Treshhinostojkie metalloorganoplastiki dlya aviacionnyh konstrukcij: avtoref. dis. … kand. tehn. nauk [Crack resistant metalorganoplastics for aviation designs: thesis … Cand. Tech. Sci.]. M.: VIAM, 1996. 32 s.
  15. Trefilov B.F. Razrabotka i issledovanie uglealyuminievogo kompozicionnogo materiala VKU-1 [Development and research carbon aluminum VKU-1 composite material] // Aviacionnye materialy. M.: ONTI VIAM, 1981. Vyp. 1. S. 17–25.
  16. Prochnost, ustojchivost, kolebaniya: spravochnik v 3 t. / pod obshh. red. I.A. Birgera, Ya.G. Panovko [Durability, stability, fluctuations: the directory in 3 vol. / gen. ed. by. I.A.Birger, Ya.G.Panovko]. M.: Mashinostroenie, 1968.T. 2. 464 s.