Study of tribological properties of organoplastics on the basis of reinforcing fabric filler

Kulagina G.S., Korobova A.V., Zuev S.V., Zhelezina G.F.
Kulagina G.S., Korobova A.V., Zuev S.V., Zhelezina G.F. Study of tribological properties of organoplastics on the basis of reinforcing fabric filler // Proceedings of VIAM. 2016. No. 11. DOI: 10.18577/2307-6046-2016-0-11-6-6. URL: https://www.viam-works.ru/en/journal/2016/11/6
Keywords
friction coefficient, tribological properties, antifriction organoplastics, antifriction coatings, a reinforcing fabric filler, polytetrafluoroethylene, ultrahigh molecular weight polyethylene.
Abstract

Antifriction organoplastics reinforced with fabrics with polytetrafluoroethylene (PTFE) fibers or ultrahigh molecular weight polyethylene (UHMWPE) fibers are investigated. It is shown that friction coefficients in pairs «organoplastic–steel» and «organoplastic–carbon-filled plastic» change in the range of 0,07 to 0,20 depending on load and sliding speed (0,8–3,2 MPa; 0,1–0,45 m/s) with extremely low weight wear. Organoplastics are recommended as antifriction coatings for heavy-loaded sliding bearings in condition of dry friction. The work is executed within the implementation of the complex scientific direction 13. «Polymer composite materials» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Sovremennye mashinostroitelnye materialy. Nemetallicheskie materialy: spravochnik / pod obshh. red. I.V. Gorynina i A.S. Oryshhenko [Modern machine-building materials. Non-metallic materials: the directory / gen. ed. by. I.V.Gorynin and A.S.Oryshchenko]. SPb.: Professional, 2012. 916 s.
  3. Voronkov B.D. Podshipniki suhogo treniya [Bearings of dry friction]. L.: Mashinostroenie, 1979. 224 s.
  4. Buhin V.E., Evseev V.N., Postnikov Yu.A., Fedoseeva A.Yu. Polimernye materialy dlya uzlov treniya [Polymeric materials for friction nodes] // Tehnologiya, organizaciya proizvodstva i upravleniya, obzornaya informaciya. NIIEinformenergomash. 1987. Vyp. 15. S. 1–33.
  5. Adamenko N.A., Agafonova G.V. Tribotehnicheskie polimernye materialy. Volgograd: VolgGTU, 2013. 107 s.
  6. Sirenko G.A., Sviderskij V.P., Gerasimov V.D., Nikonov V.Z. Antifrikcionnye termostojkie polimery [Antifriction heat-resistant polymers]. Kiev: Tehnika, 1978. 246 s.
  7. Davydova I.F., Kavun N.S. Teplostojkie antifrikcionnye tekstolity [Heat-resistant anti-friction textolites] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №11. St. 04. Available at: http://www.viam-works.ru (accessed: February 29, 2016). DOI: 10.18577/2307-6046-2014-0-11-4-4.
  8. Donetskij K.I., Khrulkov A.V. Primenenie naturalnyh volokon pri izgotovlenii polimernyh kompozicionnyh materialov [Application of naturals fibers for manufacturing of polymer composite materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №2. St. 10. Available at: http://www.viam-works.ru (accessed: March 04, 2016). DOI: 10.18577/2307-6046-2015-0-2-10-10.
  9. Anisimov A.V., Bahareva V.E., Balyshko I.V., Ginzburg B.M., Kirik E.V., Tochilnikov D.G. Harakteristiki organoplastikov na osnove fenolnoj matricy i oksolanovogo volokna [Characteristics organic plastics on the basis of phenolic matrix and oxolan fiber] // Voprosy materialovedeniya. 2006. №2. S. 113–118.
  10. Yudin A.S. Razrabotka iznosostojkih, antifrikcionnyh organotekstolitov na osnove polioksadiazol'nyh tkanej i polimer-mineralnyh modifikatorov: avtoref. dis. ... kand. tehn. nauk [Development wearproof, antifriction organocloth-based laminate on the basis of polyoxadiazole fabrics and polymer-mineral modifiers: thesis of Cand. Tech. Sci.]. M., 2013. 20 s.
  11. Kablov E.N., Kondrashov S.V., Yurkov G.Y. Prospects of using carbonaceous nanoparticles in binders for polymer composites // Nanotechnologies in Russia. 2013. Т. 8. №3–4. С. 163–185.
  12. Bejder E.Ya., Donskoj A.A., Zhelezina G.F., Kondrashov E.K., Sytyj Yu.V., Surnin E.G. Opyt primeneniya ftorpolimernyh materialov v aviacionnoj tehnike [Experience of application of ftorpolimerny materials in aviation engineering] // Rossijskij himicheskij zhurnal. 2008. T. LII. №3. S. 30–44.
  13. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  14. Timoshkov P.N., Hrulkov A.V. Sovremennye tehnologii pererabotki polimernyh kompozitsionnyh materialov, poluchaemyh metodom propitki rasplavnym svyazuyushchim [Modern technologies of hotmelt polymer composite materials processing] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №8. St. 04. Available at: http://www.viam-works.ru (accessed: February 19, 2016). DOI: 10.18577/2307-6046-2014-0-8-4-4.
  15. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svyazujushhie dlya perspektivnyh metodov izgotovleniya konstrukcionnyh voloknistyh PKM [New polymeric binding for perspective methods of manufacturing of constructional fibrous PCM] // Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.