Refractory alloys for innovative equipment

Ospennikova O.G., Podjyachev V.N., Stolyankov Yu.V.
Ospennikova O.G., Podjyachev V.N., Stolyankov Yu.V. Refractory alloys for innovative equipment // Proceedings of VIAM. 2016. No. 10. DOI: 10.18577/2307-6046-2016-0-10-5-5. URL: https://www.viam-works.ru/en/journal/2016/10/5
Keywords
heat resistant nickel alloys, refractory metals and alloys, tungsten, tantalum, molybdenum, niobium.
Abstract

Modern development of innovative equipment (primarily aviation and aerospace) makes demands to materials capable to work at high temperatures in which traditional nickel alloys cannot work. The problem of creating new heat resistant including refractory alloys acquires nowadays particular significance not only in the aircraft industry in connection with development of high-economic gas turbine engines of new generation, but also in other industries. One of the promising scientific and research directions in this field is the refractory metals and alloys development which keep considerable durability up to temperatures of 1300–2500°C. Among the metals of the kind the «big four» – tungsten, tantalum, molybdenum, niobium are outstanding that both in pure or as alloys widely used in various industrial fields.

Reference list
  1. Litye lopatki gazoturbinnyh dvigatelej: splavy, tehnologii, pokrytiya. 2-e izd. / pod obshh. red. E.N. Kablova [Cast blades of gas turbine engines: alloys, technologies, coverings. 2nd prod. / ed. by E.N. Kablov]. M.: Nauka, 2006. 632 s.
  2. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  3. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of modern and future high technologies] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 01. Available at: http://www.viam-works.ru (accessed: February 11, 2015).
  4. Kolobov Yu.R., Kablov E.N., Kozlov E.V. i dr. Struktura i svojstva intermetallidnyh materialov s nanofaznym uprochneniem [Structure and properties of intermetallidny materials with nanophase hardening]. M.: MISiS, 2008. 328 s.
  5. Stolyankov Yu.V. Zharoprochnye metallicheskie kompozicionnye materialy konstrukcionnogo naznacheniya na osnove intermetallidov nikelya (obzor) [Heat resisting metal composite materials of constructional assignment on the basis of nickel intermetallic compound (review)] // Kompozity i nanostruktury. 2016. №4 (v pechati).
  6. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Materials of new generation are necessary to Russia] // Redkie zemli. 2014. №3. S. 8–13.
  7. Kablov E.N. Tendencii i orientiry innovacionnogo razvitiya Rossii: sb. nauch.-inform. mater.; 3-e izd. [Tendencies and reference points of innovative development of Russia: collection of scientific information materials; 3rd ed.]. M.: VIAM, 2015. 720 s.
  8. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  9. Grashhenkov D.V., Shhetanov B.V., Efimochkin I.Yu. Razvitie poroshkovoj metallurgii zharoprochnyh materialov [Development of powder metallurgy of heat resisting materials] // Vse materialy. Enciklopedicheskij spravochnik. 2011. №5. S. 13–26.
  10. Grashhenkov D.V., Shhetanov B.V., Efimochkin I.Yu. Razvitie poroshkovoj metallurgii zharoprochnyh materialov [Development of powder metallurgy of heat resisting materials] // Vse materialy. Enciklopedicheskij spravochnik. 2011. №6. S. 10–20.
  11. Savickij E.M., Povarova K.B., Makarov P.V. Metallovedenie volframa [Tungsten metallurgical science]. M.: Metallurgiya, 1978. 223 s.
  12. Savickij E.M., Burhanov G.S. Metallovedenie splavov tugoplavkih i redkih metallov [Metallurgical science of alloys of refractory and rare metals]. M.: Nauka, 1971. 352 s.
  13. Gavrilyuk M.I., Podyachev V.N. Issledovanie svojstv splavov volframa, legirovannyh uglerodom, tantalom, niobiem i cirkoniem [Research of properties of alloys of the tungsten alloyed by carbon, tantalum, niobium and zirconium] // MiTOM. 1975. №4. S. 24–27.
  14. Zaharova G.V., Popov A.I., Zhorova A.P., Fedin B.V. Niobij i ego splavy [Niobium and its alloys]. M.: Metallurgizdat, 1961. 380 s.
  15. Kablov E.N., Svetlov I.L., Efimochkin I.Yu. Vysokotemperaturnye Nb–Si-kompozity [High-temperature Nb–Si-composites] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroenie. 2011. №SP2. S. 164–173.
  16. Svetlov I.L. Vysokotemperaturnye niobij-kremnievye kompozity – zamena monokristallicheskim nikelevym zharoprochnym splavam [High-temperature niobium - silicon composites – replacement to single-crystal nickel hot strength alloys] // Dvigatel. 2010. №5. S. 36–37.
  17. Svetlov I.L. Vysokotemperaturnye niobij-kremnievye kompozity [High-temperature niobium-silicon composites] // Materialovedenie. 2010. №9. S. 29–38.
  18. Svetlov I.L. Vysokotemperaturnye niobij-kremnievye kompozity [High-temperature niobium-silicon composites] // Materialovedenie. 2010. №10. S. 18–27.
  19. Karpov M.I., Vnukov V.I., Korzhov T.S. i dr. Struktura i mehanicheskie svojstva zharoprochnogo splava sistemy Nb–Si evtekticheskogo sostava, poluchennogo metodom napravlennoj kristallizacii [Structure and mechanical properties of hot strength alloy of Nb–Si-system of the eutectic structure received by method of directed crystallization] // Deformaciya i razrushenie materialov. 2012. №12. S. 2–8.
  20. Kuzmina N.A., Bondarenko Yu.A. Issledovanie fazovogo sostava i struktury niobij-kremnievogo kompozita, poluchennogo metodom napravlennoj kristallizacii v zhidkometallicheskom ohladitele [The phase composition and structure of the niobium-silicon composite manufactured by directional solidification in the liquid metal cooler] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №5. St. 03. Available at: http://www.viam-works.ru (accessed: June 20, 2016). DOI: 10.18577/2307-6046-2016-0-5-3-3.
  21. Voronin G.M., Kishkin S.T., Panasyuk I.O., Podyachev V.N., Sivakova E.V. Tugoplavkie splavy v izdeliyah aviacionnoj i kosmicheskoj tehniki [] // Aviacionnye materialy na rubezhe XX–XXI vekov: nauch.-tehnich. sb. M.: VIAM, 1994. S. 264–273.
  22. Podyachev V.N., Demonis I.M., Baranova O.A. Laboratoriya tugoplavkih splavov VIAM i ee pervyj rukovoditel A.S. Stroev. K 55-letiyu so dnya organizacii [Refractory alloys in products of aviation and space engineering] // Istoriya nauki i tehniki. 2013. №4. S. 19–25.
  23. Kashin D.S., Stehov P.A. Zashhitnye pokrytiya dlya zharoprochnyh splavov na osnove niobiya [Protective coatings for high-temperature niobium-based alloys] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №6. St. 01. Available at: http://www.viam-works.ru (accessed: September 16, 2015). DOI: 10.18577/2307-6046-2015-0-6-1-1.