Рrognostication of surface temperature of epoxy coatings on aluminum alloy subjected to long exposure in natural climate conditions

Startsev V.O., Medvedev I.M., Startsev O.V.
Startsev V.O., Medvedev I.M., Startsev O.V. Рrognostication of surface temperature of epoxy coatings on aluminum alloy subjected to long exposure in natural climate conditions // Proceedings of VIAM. 2016. No. 10. DOI: 10.18577/2307-6046-2016-0-10-12-12. URL: https://www.viam-works.ru/en/journal/2016/10/12
Keywords
aluminum alloy, surface temperature, climatic parameters, prognostication, multilinear model.
Abstract

The variations in surface temperature of D16-AT aluminum samples with white, grey and black epoxy coatings subjected to 9 years of natural weathering in Gelendzhik Climatic Testing Center are studied. The multilinear predication model of temperature variations including 12 meteorological indexes is proposed to predict the sample surface temperature. High reliability of model is shown. The rigorous 12-month intervals in the value of mean square error of monthly models surface temperature prediction are shown.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Startsev O.V., Medvedev I.M. Obzor zarubezhnogo opyta issledovanij korrozii i sredstv zashhity ot korrozii [Review of international experience on corrosion and corrosion protection] //Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 76–87.
  3. Kablov E.N. i dr. Korrozionnaya agressivnost' primorskoj atmosfery. Ch. 1. Faktory vliyaniya (obzor) [Corrosion aggression of the seaside atmosphere. P.1. Factors of influence (review)] // Korroziya: materialy, zashhita. 2013. №12. S. 6–18.
  4. Kablov E.N., Startsev O.V., Medvedev I.M. Korrozionnaya agressivnost primorskoj atmosfery. Ch. 2. Novye podhody k ocenke korrozivnosti primorskih atmosfer [Corrosion aggression of the seaside atmosphere. H. 2. New approaches to assessment of korrozivnost of the seaside atmospheres] // Korroziya: materialy, zashhita. 2016. №1. S. 1–15.
  5. Berdahl P., Akbari H., Levinson R. Weathering of Roofing Materials-An Overview // Constr. Build. Mater. 2006. P. 23.
  6. Dan Z., Muto I., Hara N. Constant Dew Point Corrosion Tests for Metals, Developments in Corrosion Protection // Developments in Corrosion Protection / ed. by M. Aliofkhazraei. 2014. P. 81–101.
  7. Dursun T., Soutis C. Recent developments in advanced aircraft aluminum alloys // Mater. Des. 2014. Vol. 56. P. 862–871.
  8. Pickett J.E., Sargent J.R. Sample temperatures during outdoor and laboratory weathering exposures // Polym. Degrad. Stab. 2009. Vol. 94. P. 189–195.
  9. Bijl P. и др. Modelling of sample surface temperature in an outdoor weathering test // Polym. Test. 2011. Vol. 30. P. 485–492.
  10. Myers D. Predicting temperatures of exposure panels: models and empirical data // ACS Symposium Series, D. / ed. by R. Bauer, J. W. Martin. 1999. Vol. 722. P. 71–84.
  11. Haillant O., Dumbleton D., Zielnik A. An Arrhenius approach to estimating organic photovoltaic module weathering acceleration factors // Sol. Energy Mater. Sol. Cells. 2011. Vol. 95. P. 1889–1895.
  12. Tocháček J., Vrátníčková Z. Polymer life-time prediction: The role of temperature in UV accelerated ageing of polypropylene and its copolymers // Polym. Test. 2014. Vol. 36. P. 82–87.
  13. Boxhammer J. Surface temperatures and temperature measurement techniques on the level of exposed samples during irradiational weathering in equipment // Weather. Plast. Test. to Mirror Real Life Perform. 1999. P. 105–119.
  14. Schönlein A., Haillant O., Senff S. Surface temperatures of color painted samples in natural and artificial weathering with different laboratory light sources for optimized testing and investigations // Weathering Symposium: Natural and Artificial. 2009.
  15. Burch D., Martin J. Predicting the temperature and relative humidity of polymer coatings in the field // ACS Symp. Ser. Am. Chem. Soc. 1999. P. 85–107.
  16. Pickett J.E.E., Gibson D.A.A., Gardner M.M.M. Effects of irradiation conditions on the weathering of engineering thermoplastics // Polym. Degrad. Stab. 2008. Vol. 93. No. 8. P. 1597–1606.
  17. Draper N.R., Smith H. Applied regression analysis. John Wiley & Sons, 1998. 736 p.
  18. Kondratev K.Ya. Aktinometriya [Actinometry]. L.: Gidrometeorologicheskoe izdatelstvo, 1965. 693 s.
  19. Startsev O.V. i dr. Zavisimost temperatury poverhnosti obrazcov ot harakteristik klimata pri ekspozicii v naturnyh usloviyah [Dependence of surface temperature of samples on climate characteristics on exposure in natural conditions] // Korroziya: materialy, zashhita. 2013. №7. S. 43–47.
  20. Hromov S.P., Petrosyanc M.A. Meteorologiya i klimatologiya [Meteorology and climatology]. M.: Nauka, 2006. 582 s.
  21. Kalitkin N.N. Chislennye metody [Numerical methods]. M.: Nauka, 1978. 512 s.
  22. Tejlor Dzh. Vvedenie v teoriyu oshibok; per. s angl. [Introduction in the theory of mistakes; trans. form English]. M.: Mir, 1985. 272 s.
  23. Moore D.S., McCabe G.P., Craig B.A. Introduction to the Practice of Statistics. Sixth Edit. New York, 2009. 766 p.
  24. Stenli R. Perechislitelnaya kombinatorika [Enumerative combinatory]. M.: Mir, 1990. 440 s.
  25. Handbook of Linear Algebra. Edited by Leslie Hogben. Chapman&Hall/CRC, Taylor&Francis Group, 2007. 1402 р.
  26. Startsev O.V., Krotov A.S., Golub P. Effect of climatic and radiation ageing on properties of glass fibre reinforced epoxy laminates // Polym. Polym. Compos. 1998. Vol. 6. No. 7. P. 481–488.
  27. Startsev O.V., Krotov A.S., Mashinskaya G.P. Climatic ageing of organic fiber reinforced plastics: water effect // Int. J. Polym. Mater. 1997. Vol. 37. No. 3–4. P. 161–171.
  28. Afshar A. и др. Effect of long-term exposure to marine environments on the flexural properties of carbon fiber vinylester composites // Compos. Struct. 2015. Vol. 126. P. 72–77.
  29. Starcev V.O., Frolov A.S. Vliyanie klimaticheskogo vozdejstviya na cvetovye harakteristiki lakokrasochnyh pokrytij [Influence of climatic influence on color characteristics of paint coatings] // Lakokrasochnye materialy i ih primenenie. 2015. №3. S. 16–18.
  30. Startsev V.O., Nizina T.A. Prognozirovanie klimaticheskogo stareniya epoksidnyh polimerov po izmeneniyu cvetovyh pokazatelej [The modeling of epoxy polymers weathering by the color characteristics measurements] // Trudy VIAM elektron. nauch.-tehnich. zhurn. 2015. №12. St. 10 Available at: http://www.viam-works.ru (accessed: July 04, 2016). DOI: 10.18577/2307-6046-2015-0-12-10-10.
  31. Dan Z. et al. Applicability of Constant Dew Point Corrosion Tests for Evaluating Atmospheric Corrosion of Aluminium Alloys // Corros. Sci. 2011. Vol. 53. P. 2006–2014.
  32. Titareva A.S., Kirillov V.N., Startsev O.V. Povedenie materialov v elementah konstrukcij aviacionnoj tehniki, izgotovlennyh s primeneniem PKM i sistem LKP v usloviyah umerenno teplogo klimata [Behavior of materials in structural components of aeronautical engineering, manufactured using PCM and PC systems under conditions of temperate thermal climate] // Aviacionnye materialy i tehnologii. 2013. №S2. S. 81–85.
  33. Panin S.V., Startsev O.V., Krotov A.S., Medvedev I.M., Frolov A.S. Korroziya i starenie poverhnosti konstrukcionnyh materialov po dannym 3D mikroskopii [Corrosion and aging of structural materials surface studied by 3D microscopy] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №12. St. 12. Available at: http://www.viam-works.ru (accessed: July 04, 2016). DOI: 10.18577/2307-6046-2014-0-12-12-12.
  34. 34 Panin S.V., Startsev O.V., Krotov A.S. Diagnostika nachalnoj stadii klimaticheskogo stareniya PKM po izmeneniyu koefficienta diffuzii vlagi [Initial stage environmental degradation of the polymer matrix composites evaluated by Water diffusion coefficient] // Trudy VIAM: electron. nauch.-tehnich. zhurn. 2014. №7. St. 09. Available at: http://viam-works.ru (accessed: July 04, 2016). DOI: 10.18577/2307-6046-2014-0-7-9-9.
  35. Startsev V.O., Mahonkov A.Yu., Kotova E.A. Mehanicheskie svojstva i vlagostojkost' PKM s povrezhdeniyami [Mechanical properties and moisture resistance of PCM with damages] // Aviacionnye materialy i tehnologii. 2015. №S1 (38). S. 49–55. DOI: 10.18577/2071-9140-2015-0-S1-49-55.