Study of the possibility of marking parts of polycarbonate

Petrova G.N., Starostina I.V., Rumyantseva T.V.
Petrova G.N., Starostina I.V., Rumyantseva T.V. Study of the possibility of marking parts of polycarbonate // Proceedings of VIAM. 2016. No. 10. DOI: 10.18577/2307-6046-2016-0-10-11-11. URL: https://www.viam-works.ru/en/journal/2016/10/11
Keywords
thermoplastic, polycarbonate, fluoropolymer, updating (modified), aging, silver-resistance, marking composition, paint, glue.
Abstract

Research results on the matter of thermoplastic polymer – polycarbonate parts marking are adduced. Influence of marking composition on the physical and mechanical characteristics of the pure (not modified) and modified by polycarbonate fluoropolymer 42 is studied. The polymers properties dependences on marking presence and kind of influence (thermal and heat – humidity aging) are adduced. It is found that applying the marking composition on polycarbonate practically does not make impact on mechanical properties of material and does not reduce «silver-resistance» of the pure and modified polycarbonate. It is shown that the marking paint of 7010 series and marking composition on the basis of VK-14 glue can be used for marking parts of polycarbonate as pure so modified by the fluoropolymer 42.

Reference list
  1. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Kablov E.N. Aviacionnoe materialovedenie: itogi i perspektivy [Aviation materials science: results and perspectives] // Vestnik Rossijskoj akademii nauk. 2002. T. 72. №1. S. 3–12.
  4. Yakovlev A.D. Himiya i tehnologiya lakokrasochnyh pokrytij [Chemistry and technology of paint coatings]. L.: Himiya, 1981. 352 s.
  5. Chebotarevskij V.V., Kondrashov E.K. Tehnologiya lakokrasochnyh pokrytij v mashinostroenii [Technology of paint coatings in mechanical engineering]. M.: Mashinostroenie, 1978. 294 s.
  6. OST1 90210–85. Specialnye markirovochnye kraski dlya priborov i elektroagregatov. Obshhie tehnicheskie trebovaniya. Vybor markirovochnyh krasok [OCT1 90210-85. Special marking paints for devices and electrounits. General technical requirements. Choice of marking paints]. M.: VIAM, 1986. 27 s.
  7. Karyakina M.I. Ispytanie lakokrasochnyh materialov i pokrytij [Testing of paint and varnish materials and coverings]. M.: Himiya, 1988. 272 s.
  8. Petrova G.N., Abakumova N.M., Rumyanceva T.V. i dr. Pozharobezopasnye litevye termoplasty [Fireproof molding thermoplastics] // Plasticheskie massy. 2005. №1. S. 45–46.
  9. Gryaznov V.I., Petrova G.N., Yurkov G.Yu., Buznik V.M. Smesevye termojelastoplasty so specialnymi svojstvami [Thermoplastic mixtures with special properties] // Aviacionnye materialy i tehnologii. 2014. №1. S. 25–29.
  10. Petrova G.N., Bejder E.Ya., Starostina I.V. Litevye termoplasty dlya izdelij aviacionnoj tehniki [Molding thermoplastics for products of aviation engineering] // Vse materialy. Enciklopedicheskij spravochnik. 2016. №7. S. 21–29.
  11. Sorokin A.E., Krasnov A.P., Zyuzina G.F. i dr. Stroenie i svojstva vysokomolekulyarnogo litevogo poliarilata [Structure and properties of high-molecular lityevy polyarylate] // Plasticheskie massy. 2012. №1. S. 8–12.
  12. Petrova G.N., Beyder E.Yа. Construction materials based on reinforced thermoplastics Chemistry and Materials Science // Russian Journal of General Chemistry. 2011. Vol. 81. No. 5. Р. 1001–1007.
  13. Brandshtetter F. Tendencii i perspektivy razvitiya polimernyh materialov [Tendencies and perspectives of development of polymeric materials] // Polimernye materialy: izdeliya, oborudovanie, tehnologii. 2005. №5. S. 2–4.
  14. Petrova G.N., Beyder E.Ya. Povyshenie ognestojkosti polibutilentereftalata (obzor) [Increasing of fire resistance of polybutylene terephthalate (review)] // Aviacionnye materialy i tehnologii. 2014. №4. S. 58–64. DOI: 10.18577/2071-9140-2014-0-4-58-64.
  15. Petrova G.N., Rumyanceva T.V., Beyder E.Ya. Vliyanie modificiruyushhih dobavok na pozharobezopasnye svojstva i tehnologichnost polikarbonata [Influence of modifying additives on fireproof properties and technological effectiveness of polycarbonate] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №6. St. 06. Available at: http://www.viam-works.ru (accessed: June 15, 2016).
  16. Orehov N.G., Starostina I.V. Analiz kachestva litoj prutkovoj (shihtovoj) zagotovki iz zharoprochnyh splavov proizvodstva FGUP «VIAM» [Quality analysis of the charge bar castings made from superalloys by FSUE «VIAM»] // Aviacionnye materialy i tehnologii. 2014. №S5. S. 23–30. DOI: 10.18577/2071-9140-2014-0-s5-23-30.
  17. Barbotko S.L. Pozharobezopasnost aviacionnyh materialov [Fire safety of aviation materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 431–439.
  18. Nesterova T.A., Zuev A.V., Platonov M.M. Teploizolyacionnyj material na osnove organicheskogo volokna dlya sistem kondicionirovaniya vozduha samoletov [Heat insulation material based on organic fiber for aircraft air conditioning systems] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 32–38. DOI: 10.18577/2071-9140-2015-0-2-32-38.
  19. Petrova G.N. Napravlennaya modifikaciya polisulfonov i sozdanie na ih osnove litevyh i kompozicionnyh materialov: avtoref. dis. … kand. tehn. nauk [The directed updating of polysulphones and creation on their basis of lityevy and composite materials: thesis of Cand. Tech. Sci.]. M.: VIAM, 2011. S. 10–27.
  20. Sytyj Yu.V., Sagomonova V.A., Kislyakova V.I., Bolshakov V.A. Vibropogloshhayushhie materialy na osnove termojelastoplastov [Vibro absorbing materials on the basis of thermoelastoplastics] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №3. St. 06. Available at: http://viam-works.ru (accessed: July 14, 2016).
  21. Mihajlin Yu.A. Termoustojchivye polimery i polimernye materialy na ih osnove [Thermosteady polymers and polymeric materials on their basis] // Polimernye materialy. 2005. №4. S. 29–32.
  22. Hazova T.N. Sostoyanie rynka v proizvodstve polikarbonata [Condition of the market in production of polycarbonate] // Mezhdunarodnye novosti mira plastmass. 2005. №1–2. S. 35–39.
  23. Nazarov V.G., Stolyarov V.P., Petrova G.N., Gryaznov V.I., Buznik V.M. Osobennosti poverhnostnogo ftorirovaniya termoelastoplastov na osnove poliuretana i ego vliyanie na svojstva polimera [Features of surface fluorine of thermoelastoplastics on the basis of polyurethane and its influence on properties of polymer] // Perspektivnye materialy. 2016. №2. S. 52–60.
  24. Semyonova L.V., Bejder E.Ya., Petrova G.N., Nefedov N.I. Elektroizolyacionnye svojstva polimernyh pokrytij [Electro-insulative properties of polymer coatings] // Trudy VIAM elektron. nauch.-tehnich. zhurn. 2014. №8. St. 07. Available at: http://www.viam-works.ru (accessed: March 16, 2016). DOI: 10.18577/2307-6046-2014-0-8-7-7.
  25. Mihajlin Yu.A. Pokazateli ognestojkosti PM i metody ih opredeleniya [Indicators of fire resistance of PM and methods of their definition] // Polimernye materialy. 2011. №8. S. 32–34.
  26. Petrova G.N., Zhuravleva P.L., Iskhodzhanova I.V., Beider E.Ya. Influence of Carbon Fillers on Properties and Structure of Polyethylene-Based Polymer Composites // Nanotechnologies in Russia. 2014. Vol. 9. No. 5–6. P. 305–310.
  27. Richardson M. Promyshlennye polimernye kompozicionnye materialy / pod red. P.G. Babaevskogo [Industrial polymeric composite materials / ed. by P.G. Babaevskiy]. M.: Himiya,1980. 472 s.
  28. Petrova G.N., Barbotko S.L., Bejder E.Ya. i dr. Pozharobezopasnye litevye termoplasty [Fireproof molding thermoplastics] // Plasticheskie massy. 2006. №1. S. 46–48.
  29. Polimernye kompozicionnye materialy. Svojstva. Struktura. Tehnologii / pod red. A.A. Berlina [Polymeric composite materials. Properties. Structure. Technologies / ed. by A.A.Berlin]. SPb.: Professiya, 2009. 560 s.
  30. Mihajlin Yu.A. Termoustojchivye polimery i polimernye materialy [Thermosteady polymers and polymeric materials]. SPb.: Professiya, 2006. S. 29–30.
  31. Lazareva T.K., Ermakin S.N., Kostyagina V.A. Problemy sozdaniya kompozicionnyh materialov na osnove konstrukcionnyh termoplastov [Problems of creation of composite materials on the basis of constructional thermoplastics] // Uspehi v himii i himicheskoj tehnologii 2010. T. 24. №4. S. 58–63.
  32. Petrova G.N., Platonov M.M., Bo'shakov V.A., Ponomarenko S.A. Issledovanie kompleksa harakteristik bazovyh materialov dlya FDM-tehnologii additivnogo sinteza. Fiziko-mehanicheskie i teplofizicheskie svojstva [Research of complex of characteristics of base materials for FDM technology of the additive synthesis. Physicomechanical and heatphysical properties] // Plasticheskie massy. 2016. №5–6 (v pechati).
  33. Platonov M.M., Petrova G.N., Larionov S.A., Barbotko S.L. Novyj termoplastichnyj material s ponizhennoj pozharoopasnostyu dlya FDM-tehnologii [New thermoflexible material with the lowered fire danger for FDM-technology] // Additivnye tehnologii: nastoyashhee i budushhee: mater. II Mezhdunar. konf. M.: VIAM, 2016. St. 05.
  34. Sudarushkin Yu.K., Gudimov M.M., Romanov D.S., Sokolov M.Yu. Primenenie litevyh polikarbonatov v aviapriborostroenii [Application of molding polycarbonates in avionics] // Aviacionnaya promyshlennost. 2003. №2. S. 48–52.