From single-crystal uncooled blades to turbines blades with penetration (transpiration) cooling made by additive technologies (review on technology of single-crystal GTE bladescasting)

Gerasimov V. V.
Gerasimov V. V. From single-crystal uncooled blades to turbines blades with penetration (transpiration) cooling made by additive technologies (review on technology of single-crystal GTE bladescasting) // Proceedings of VIAM. 2016. No. 10. DOI: 10.18577/2307-6046-2016-0-10-1-1. URL: https://www.viam-works.ru/en/journal/2016/10/1
Keywords
the directed crystallization of heat resisting alloys, GTD blades with directed and single-crystal structure, compound ceramic core.
Abstract

Stages of formation and development of single-crystal blade casting of heat resistant intermetallic alloys, composite alloys like VKLS, the creation of experimental industrial and industrial equipment for directed crystallization process and also development of blades cooling systems through creation of complex internal cavities are adduced. The problems connected with blades manufacture with the penetrating cooling system are considered. The forecast of getting blades with the penetrating cooling system without application of ceramic forms and cores, i.e. by additive technology is discussed.

Reference list
  1. Litye lopatki gazoturbinnyh dvigatelej: splavy, tehnologii, pokrytiya / pod obshh. red. E.N. Kablova. 2-e izd. [Cast blades of gas turbine engines: alloys, technologies, coverings / gen. ed. by E.N. Kablov. 2nd ed.]. M.: Nauka, 2006. 632 s.
  2. Kablov E.N., Golubovskij E.R. Zharoprochnost nikelevyh splavov: ucheb. posobie [Thermal stability of nickel alloys: manual]. M.: Mashinostroenie, 1998. 464 s.
  3. Kurc V., Zam P.R. Napravlennaya kristallizaciya evtekticheskih materialov [The directed crystallization of eutectic materials]. M.: Metallurgiya, 1980. S. 91–96.
  4. Evtekticheskij splav na osnove nikelya: a. s. 1111500 [Eutectic alloy on the basis of nickel: copyright certificate 1111500]; opubl. 09.06.83.
  5. Splav na osnove nikelya: a. s. 1358425 [Alloy on the basis of nickel: copyright certificate 1358425]; opubl. 08.08.87.
  6. Kishkin S.T., Petrushin N.V., Svetlov I.L. Evtekticheskie zharoprochnye splavy [Eutectic hot strength alloys] // Aviacionnye materialy na rubezhe XX–XXI vekov: nauch.-tehnich. sb. M.: VIAM, 1994. S. 252–258.
  7. Bibring H. Conception et etude d' eutectiques orientes fortement solicites en temperature et en contraite // Ann. Chim. 1980. V. 5. №2–3. P. 111–138.
  8. Khan T. Further Assessment and Improvement of High Strength y/y`-NbC. Composites for Advanced Turbine Blades // Proc. Conf. On in Situ Composites III. 1979. P. 378–389.
  9. SR. 1.2.010–84. Sertifikat na splav VKLS20 [SR. 1.2.010-84. The certificate on alloy VKLS20]. M.: VIAM, 1984.
  10. Gerasimov V.V., Demonis I.M. Formirovanie kompozicionnoj struktury v evtekticheskih splavah pri poluchenii lopatok GTD [Forming of composition structure in eutectic alloys when receiving blades of GTE] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №6. St. 01. Available at: http://www.viam-works.ru (accessed: February 20, 2014).
  11. Vestbruk D. Issledovaniya i perspektivy primeneniya intermetallicheskih soedinenij [Researches and perspectives of application of intermetallic compounds] // Metallovedenie i termicheskaya obrabotka. 1971. №4. S. 74–80.
  12. Kornilov I.I. Metallidy – materialy s unikal'nymi svojstvami [Metallides – materials with unique properties] // Vestnik AN SSSR. 1970. №12. S. 30–33.
  13. Himicheskij enciklopedicheskij slovar / pod red. I.L. Knunyanc [The chemical encyclopedic dictionary / ed. by I.L. Knunyants]. M.: Sovetskaya enciklopediya, 1983. 792s.
  14. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  15. Kablov E.N., Buntushkin V.P., Bazyleva O.A. Litye lopatki iz intermetallidov nikelya (Ni3Al) dlya vysokotemperaturnyh gazovyh turbin [Cast blades from intermetallic compound of nickel (Ni3Al) for high-temperature gas turbines] // Konversiya v mashinostroenii. 2004. №4. S. 57–59.
  16. Ospennikova O.G. Strategiya razvitiya zharoprochnyh splavov i stalej specialnogo naznacheniya, zashhitnyh i teplozashhitnyh pokrytij [Strategy of development of hot strength alloys and steels special purpose, protective and heat-protective coverings] // Aviacionnye materialy i tehnologii. 2012. №S. S. 19–36.
  17. Gerasimov V.V., Petrushin N.V., Visik E.M. Usovershenstvovanie sostava i tehnologiya lit'ya monokristallicheskih lopatok iz zharoprochnogo intermetallidnogo splava [Improvement of casting technology and composition of single crystal blades made of heat-resistant intermetallic alloy] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №3. St. 01. Available at: http://www.viam-works.ru (accessed: April 21, 2015). DOI: 10.18577/2307-6046-2015-0-3-1-1.
  18. Kablov E.N., Lomberg B.S., Ospennikova O.G. Sozdanie sovremennyh zharoprochnyh materialov i tehnologij ih proizvodstva dlya aviacionnogo dvigatelestroeniya [Creation of modern heat resisting materials and technologies of their production for aviation engine building] // Krylya Rodiny. 2012. №3–4. S. 34–38.
  19. Kablov E.N., Petrushin N.V. Kompyuternyj metod konstruirovaniya litejnyh zharoprochnyh nikelevyh splavov [Computer method of designing of cast heat resisting nickel alloys] // Litejnye zharoprochnye splavy. Effekt S.T. Kishkina. M.: Nauka, 2006. S. 56–78.
  20. Polaya lopatka «Vihrepor»: pat. 2078946 Ros. Federaciya [Hollow blade «Vihrepor»: pat. 2078946 Rus. Federation]; opubl. 13.05.96.
  21. Single-cast high-temperature, thin wall structure and method of making the same: pat. 5295530 US; publ. 22.03.94.
  22. Kablov E.N., Svetlov I.L., Demonis I.M., Folomejkin Yu.I. Monokristallicheskie lopatki s transpiracionnym ohlazhdeniem dlya vysokotemperaturnyh gazoturbinnyh dvigatelej [Single-crystal blades with transpiration cooling for high-temperature gas turbine engines] // Aviacionnye materialy i tehnologii: nauch.-tehnich. sb. M.: VIAM, 2003. Vyp. Vysokozharoprochnye materialy dlya sovremennyh i perspektivnyh gazoturbinnyh dvigatelej i progressivnye tehnologii ih proizvodstva. S. 24–33.
  23. Skibin V.A., Solonin V.I., Dulnev A.A. Perspektivy razvitiya gazoturbinnyh dvigatelej [Perspectives of development of gas turbine engines] // Gazoturbinnye tehnologii. 2000. №2. S. 4–14.
  24. Gerasimov V.V., Visik E.M., Kolyadov E.V. O neispolzovannyh rezervah napravlennoj kristallizacii v povyshenii ekspluatacionnyh harakteristik detalej GTD i GTU [About unused reserves of the directed crystallization in increase of utilization properties of details of GTE and GTU] // Litejnoe proizvodstvo. 2013. №9. S. 30–32.
  25. Sostavnoj keramicheskij sterzhen: pat. 2094163 Ros. Federaciya [Compound ceramic rod: pat. 2094163 Rus. Federation]; opubl. 27.10.97.
  26. Bouse G.K. and Sikkenga B. Characterization of Double Walled Single Crystal Turbine Blades From Russian VIAM Institute // Technical Report №1058/A. Howmet Corporation. 1997. 11 p.
  27. Kablov E.N. Chtoby sobrat samolet po atomam [To collect airplane on atoms] // Industriya. Inzhenernaya gazeta. 2015. №12. S. 1–2.
  28. Moldless/coreless single crystal castings of nickel-aluminide: pat. 5312584 US; publ. 17.05.94.
  29. Veys J.M., Mevrel R. Influence of Protective Coatings on the Mechanical Properties of CMSX-2 and Cotac 784 // Materials Science and Engineering. 1987. №88. P. 253–260.