Comprehensive research of the influence of climatic and operational factors on new generation epoxy binding and polymeric composite materials on its basis

Part 2. Substantiation of the choice of modes and conducting heat aging of polymeric composite materials based on epoxy matrix
Nikolaev E.V., Barbotko S.L., Andreeva N.P., Pavlov M.R.
Nikolaev E.V., Barbotko S.L., Andreeva N.P., Pavlov M.R. Comprehensive research of the influence of climatic and operational factors on new generation epoxy binding and polymeric composite materials on its basis. Part 2. Substantiation of the choice of modes and conducting heat aging of polymeric composite materials based on epoxy matrix // Proceedings of VIAM. 2016. No. 1. DOI: 10.18577/2307-6046-2016-0-1-80-89. URL: https://www.viam-works.ru/en/journal/2016/1/10
Abstract

The effect of higher temperature and moisture content on basic mechanical and thermal characteristics of carbon fiber and glass fiber plastic based on epoxy binder has been studied. The most sensitive response has been chosen to calculate the activation energies of the aging process and make predictions of retentive properties of polymeric composite materials.

Reference list
  1. Firefighting and emergency responsestudy of advanced composites aircraft. 88ABW-2012-0190 / In: Objective 2: Firefighting Effectiveness of Technologies and Agents on Composite Aircraft Fires: distribution A. Approved for public release 10.01.2012. P. 3.
  2. Sugita Y., Winkelmann C., La Saponara V. Environmental and chemical degradation of carbon/epoxy lap joints for aerospace applications, and effects on their mechanical performance // Compos. Sci. and Technol. 2010. V. 70. №5. P. 829–839.
  3. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  4. Kablov E.N., Gunyaev G.M. Tumanov A.T. – initsiator sozdaniya kompozitov [Tumanov A.T. – initiator of creation of composites] / V sb. tez. dokl. mezhotrasl. nauch.-tehnich. konf. «Kompozi- cionnye materialy v aviakosmicheskom materialovedenii». М.: VIAM, 2009. S. 6–9.
  5. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozitsionnyh materialov aviacionnogo naznacheniya. III. Znachimye faktory stareniya [Climatic aging of composite materials of aviation assignment. III. Significant factors of aging] // Deformaciya i razrushenie materialov. 2011. №1. S. 34–40.
  6. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimemye svyazuyushhie dlya perspektivnyh metodov izgotovleniya konstrukcionnyh voloknistyh PKM [New polymeric binding for perspective methods of manufacturing of constructional fibrous PCM] // Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  7. Kirillov V.N., Vapirov Yu.М., Drozd E.A. Issledovanie atmosfemoj stojkosti polimernyh kompozi- cionnyh materialov v usloviyah atmosfery teplogo vlazhnogo i umerenno teplogo klimata [Re¬search of atmospheric firmness of polymeric composite materials in the conditions of the atmos¬phere of warm wet and moderately warm climate] // Aviacionnye materialy i tehnologii. 2012. №4. S. 31–38.
  8. Mishra G., Mohapatra S.R., Behera P.R., Dash B., Mohanty U.K., Ray B.C. Environmental stability of GFRP laminated composites: an emphasis on mechanical behavior // Aircraft Eng. and Aerosp. technol. 2010. V. 82. №4. P. 258–266.
  9. Nikolaev E.V., Korenkova T.G., Shvedkova A.K., Valevin E.O. Issledovanie vliyaniya tempera- tumyh faktorov na process stareniya novyh polimernyh kompozicionnyh materialov dlya moto- gondoly aviacionnogo dvigatelya [Research of an influence of temperature factors on aging of new polymer composite materials for aviation engine nacelle] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №3. St. 12. Available at: http://www.viam-works.ru (accessed: January 01, 2015). DOI: 10.18577/2307-6046-2015-0-3-12-12.
  10. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznacheniya. I. Mehanizmy stareniya [Climatic aging of composite ma¬terials of aviation assignment. I. Aging mechanisms] // Deformaciya i razrushenie materialov. 2010. №11. S. 19–27.
  11. Kirillov V.N., Startsev O.V., Efimov V.A. Klimaticheskaya stojkost i povrezhdaemost polimernyh kompozicionnyh materialov, problemy i puti resheniya [Climatic firmness and damageability of polymeric composite materials, problems and solutions] // Aviacionnye materialy i tehnologii. 2012. №S. S. 412–423.
  12. Kirillov V.N., Efimov V.A. Problemy issledovanija klimaticheskoj stojkosti aviacionnyh nemetal- licheskih materialov [Problems of research of climatic firmness of aviation non-metallic materials] / V sb.: 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: yubilejnyj nauch.-tehnich. sb. М.: VIAM, 2007. S. 379–388.
  13. Kuleznev V.N., Ushakova O.B. Struktura i mehanicheskie svojstva polimerov (Konspekt kursa lekcij. Chast 1) [Structure and mechanical properties of polymers (Abstract of course of lectures. Part 1)]. М.: MITHT, 2006. S. 36–38.
  14. Gul V.E., Kuleznev V.N. Struktura i mehanicheskie svojstva polimerov [Structure and mechanical properties of polymers]. М.: Labirint, 1994. 367 s.
  15. Madorsky S.L. Thermal degradation of organic polymers. New York: Interscience Publishers, 1964. P. 26.
  16. Van Krevelen D.V. Svojstva i himicheskoe stroenie polimerov [Properties and chemical structure of polymers]. М.: Himiya, 1976. 416 s.
  17. Entsiklopediya polimerov [Encyclopedia of polymers]. М.: Sovetskaya enciklopediya. 1977. T. 3. 575 s.
  18. Arhireev V.P. Starenie i stabilizatsiya polimerov: ucheb. posobie [Aging and stabilization of polymers: education guidance], Kazan: KGTU, 2002. 88 s.
  19. Mikols W.J., Seferis J.C., Apicella A., Nicolais L. Evaluation of structural changes in epoxy systems by moisture sorption-desorption and dynamic mechanical studies // Polym. Compos. 1982. V. 3. №3. P. 118–124.
  20. Nikolaev E.V., Kirillov V.N., Skirta A.A., Grashhenkov D.V. Issledovanie zakonomernostej vlagoperenosa i razrabotka standarta po opredeleniyu koefficienta diffuzii i predelnogo vlagosoderzhaniya dlya ocenki mehanicheskih svojstv ugleplastikov [Study of moisture transport rules and development of a standard on measurement of the diffusion coefficient and moisture con¬tent limit to evaluate mechanical properties of carbon fiber reinforced plastics] // Aviacionnye materialy i tehnologii. 2013. №3. S. 44-48.
  21. Efimov V.A., Shvedkova A.K., Korenkova T.G., Kirillov V.N. Issledovanie polimernyh kon- strukcionnyh materialov pri vozdejstvii klimaticheskih faktorov i nagruzok v laboratornyh i natumyh usloviyah [Research of polymeric constructional materials at influence of climatic factors and loadings in laboratory and natural conditions] // Trudy VIAM: elektron. nauch.-tehnich. zhum. 2013. №1. St. 05. Available at: http://www.viam-works.ru (accessed: January 01, 2015).
  22. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznachenija. II. Relaksatsiya ishodnoj strukturnoj neravnovesnosti i gra¬dient svojstv po tolshhine [Climatic aging of composite materials of aviation assignment. II. Relax¬ation of initial structural non-equilibrium and gradient of properties on thickness] // Deformaciya i razrushenie materialov. 2012. №6. S. 17–19.