Hydrophobic structures for additional protection of aluminum alloys in fuel systems of products of aviation equipment

Mikov D.A., Kutyrev A.E., Petrova V.A.
Mikov D.A., Kutyrev A.E., Petrova V.A. Hydrophobic structures for additional protection of aluminum alloys in fuel systems of products of aviation equipment // Proceedings of VIAM. 2015. No. 9. DOI: 10.18577/2307-6046-2015-0-9-8-8. URL: https://www.viam-works.ru/en/journal/2015/9/8
Abstract

In this work functional polymer coatings which can be used as hydrophobic pro-cessing for increase of protective properties the aluminum alloys working in fuels at in-fluence of condensate are investigated. Data on resistance in the salt spray chamber and fuel of functional polymer coatings on aluminum alloy are obtained. The most effective hydrophobic agents for receiving polymer coatings are functional fluorinated oligomers. As express method the measurement method to regional corners of wetting was used by water. On the basis of the carried-out researches structures of functional polymer coatings which can be used in fuel systems of products of aviation equipment for additional pro-tection of aluminum alloys are developed.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  3. Kablov E.N. Korrozija ili zhizn' [Corrosion or life] //Nauka i zhizn'. 2012. №11. S. 16–21.
  4. Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] //Nauka i zhizn'. 2010. №4. S. 2–7.
  5. Karimova S.A., Pavlovskaja T.G. Razrabotka sposobov zashhity ot korrozii konstrukcij, rabotajushhih v uslovijah kosmosa [Development of ways of corrosion protection of the designs working in the conditions of space] //Trudy VIAM. 2013. №4. St. 02 (viam-works.ru).
  6. Antipov V.V., Senatorova O.G., Tkachenko E.A., Vahromov R.O. Aljuminievye deformirue-mye splavy [Aluminum deformable alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 167–182.
  7. Antipov V.V., Kolobnev N.I., Hohlatova L.B. Razvitie aljuminijlitievyh splavov i mnogo-stupenchatyh rezhimov termicheskoj obrabotki [Development of alyuminiylitiyevy alloys and multistage modes of thermal processing] //Aviacionnye materialy i tehnologii. 2012. №S. S. 183–195.
  8. Karimova S.A., Kutyrev A.E., Pavlovskaja T.G., Zaharov K.E. Nizkotemperaturnoe uplotne-nie anodno-oksidnyh pokrytij na detaljah iz aljuminievyh splavov [Low-temperature consolidation of anode oxide coatings on details from aluminum alloys] //Aviacionnye materialy i tehnologii. 2014. №4. S. 9–17.
  9. Aver'janov E.E. Spravochnik po anodirovaniju [Directory on anodizing]. M.: Mashinostroenie. 1988. 132 s.
  10. Bojnovich L.B., Emel'janenko A.M. Gidrofobnye materialy i pokrytija: principy sozda-nija, svojstva i primenenie [Waterproof materials and coverings: principles of creation, property and application] //Uspehi himii. 2008. T. 77. №7. S. 619–638.
  11. Sostav dlja poluchenija supergidrofobnogo pokrytija [Structure for receiving superhydrophobic coating]: pat. 2400510 Ros. Federacija; opubl. 27.09.2010. Bjul. №27.
  12. Shhukin E.D., Percov A.V., Amelina E.A. Kolloidnaja himija [Colloid chemistry]. M.: Izd-vo MGU. 1982. 82 s.
  13. Emel'janenko A.M., Bojnovich L.B. Analiz smachivanija, kak jeffektivnyj metod izuchenija harakteristik pokrytij, poverhnostej i proishodjashhih na nih processov [The wetting analysis, as effective method of studying of characteristics of coverings, surfaces and processes occurring on them] //Zavodskaja laboratorija. 2010. №9. S. 27–36.
  14. Zhilikov V.P., Karimova S.A., Leshko S.S., Chesnokov D.V. Issledovanie dinamiki korro-zii aljuminievyh splavov pri ispytanii v kamere solevogo tumana (KST) [Research of dynamics of corrosion of aluminum alloys when testing in the salt spray chamber (KST)] //Aviacionnye materialy i tehnologii. 2012. №4. S. 18–22.
  15. Karimova S.A., Pavlovskaja T.G., Petrova A.P. Podgotovka poverhnosti aljuminievyh splavov s primeneniem anodnogo oksidirovanija [Surface preparation of aluminum alloys using anodic oxidation] //Klei. Germetiki. Tehnologii. 2014. №4. S. 34–38.
  16. Vernik S. Himicheskaja i jelektrohimicheskaja obrabotka aljuminija i ego splavov [Chemical and electrochemical treatment of aluminum and its alloys]: Per. s angl. M.: Sudpromizdat. 1960. 218 s.
  17. Emel'janenko A.M., Bojnovich L.B. Primenenie dinamicheskoj porogovoj obrabotki videoizobrazhenij dlja opredelenija poverhnostnogo natjazhenija zhidkostej i kraevyh uglov smachivanija [Application of dynamic threshold processing of video images for determination of surface tension of liquids and regional corners of wetting] //Pribory i tehnika jeksperimenta. 2002. №1. S. 52–57.
  18. Topliva. Smazochnye materialy. Tehnicheskie zhidkosti. Assortiment i primenenie [Fuels. Lubricants. Technical liquids. Range and application] /Pod red. V.M. Shkol'nikova. M.: «Tehinform». 1999. 62 s.
  19. Mansfild F. Use of electrochemical impedance spectroscopy for the study of corrosion protection by polymer coating //Journal of Applied Electrochemistry. 1995. V. 25. P. 187–202.