Adhesive binders for polymer composite materials based on carbon- and glass fillers

Petrova A.P., Dement’eva L.A., Lukina N.F., Chursova L.V.
Petrova A.P., Dement’eva L.A., Lukina N.F., Chursova L.V. Adhesive binders for polymer composite materials based on carbon- and glass fillers // Proceedings of VIAM. 2015. No. 9. DOI: 10.18577/2307-6046-2015-0-9-11-11. URL: https://www.viam-works.ru/en/journal/2015/9/11
Abstract

Some basic physical, mechanical and rheological properties of the developed adhesive epoxy melt-based binders are presented. Distinctive features of adhesive prepregs based on adhesive binders and fiberglass or carbon fillers are listed and results of their application are given. The fields of application, advantage and efficiency of composite materials based on adhesive prepregs are shown. Possible applications of these materials in structures of aerospace equipment are described as well.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Anihovskaja L.I., Minakov V.T. Klei i kleevye prepregi dlja perspektivnyh izdelij aviakosmicheskoj tehniki [Glues and glue prepregs for perspective products of aerospace equipment] /V kn.: Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2002: Jubilejnyj nauch.-tehnich. sb. M.: MISiS–VIAM. 2002. S. 315–326.
  3. Kablov E.N., Minakov V.T., Anihovskaja L.I. Klei i materialy na ih osnove dlja remonta konstrukcij aviacionnoj tehniki [Glues and materials on their basis for repair of designs of aviation engineering] /V sb. Aviacionnye materialy i tehnologii. Vyp. «Remontnye tehnologii v aviastroenii». M.: VIAM. 2002. №1. S. 61–65.
  4. Lukina N.F., Dement'eva L.A., Petrova A.P., Serezhenkov A.A. Konstrukcionnye i termostojkie klei [Constructional and heat-resistant glues] //Aviacionnye materialy i tehnologii. 2012. №S. S. 328–335.
  5. Dement'eva L.A., Serezhenkov A.A., Bocharova L.I., Anihovskaja L.I., Lukina N.F. Kompozicionnye materialy kleevye na osnove stekljannyh i uglerodnyh napolnitelej [Composite materials glue on the basis of glass and carbon fillers] //Klei. Germetiki. Tehnologii. 2009. №1. S. 24–27.
  6. Dement'eva L.A., Lukina N.F., Serezhenkov A.A., Kucevich K.E. Osnovnye svojstva i naznachenie PKM na osnove kleevyh prepregov [The main properties and PKM assignment on the basis of glue prepregs] /V sb. tezisov dokladov XIX Mezhduna-rodnoj nauch.-tehnich. konf. «Konstrukcii i tehnologija poluchenija izdelij iz neme-tallicheskih materialov». Obninsk. 2010. S. 11–12.
  7. Dement'eva L.A., Serezhenkov A.A., Bocharova L.I., Lukina N.F., Kucevich K.E., Petrova A.P. Svojstva kompozicionnyh materialov na osnove kleevyh prepregov [Properties of composite materials on the basis of glue prepregs] //Klei. Germetiki. Tehnologii. 2012. №6. S. 19–24.
  8. Kirienko T.A., Lukina N.F., Kucevich K.E., Petrova A.P. Issledovanie reologicheskih svojstv kleevyh svjazujushhih [Research of rheological properties of the glue binding] //Klei. Germetiki. Tehnologii. 2015. №12 (v pechati).
  9. Lukina N.F., Dement’eva L.A., Serezhenkov A.A., Kotova E.V., Senatorova O.G., Sidel’nikov V.V., Kutsevich K.E. Adhesive prepregs and composite materials on their basis //Russian Journal of General Chemistry. 2011. V. 81. №5. P. 1022–1024.
  10. Dement'eva L.A., Serezhenkov A.A., Lukina N.F., Kucevich K.E. Kleevye prepregi – perspektivnye materialy dlja detalej i agregatov iz PKM [Glue prepregs – perspective materials for details and units from PKM] //Kompozity 21 vek. 2014. №2. S. 12–14.
  11. Petrova A.P., Donskoj A.A., Chalyh A.E., Shherbina A.A. Klejashhie materialy. Germetiki [Gluing materials. Hermetics]. SPb.: Professional. 2008. 592 s.
  12. Dement'eva L.A., Serezhenkov A.A., Lukina N.F., Kucevich K.E. Svojstva i naznachenie kompozicionnyh materialov na osnove kleevyh prepregov [Properties and assignment of composite materials on the basis of glue prepregs] //Trudy VIAM. 2014. №8. St. 06 (viam-works.ru).
  13. Kablov E.N., Antipov V.V., Senatorova O.G., Lukina N.F. Novyj klass sloistyh aljumostekloplastikov na osnove aljuminij-litievogo splava 1441 s ponizhennoj plotnost'ju [New class layered alyumostekloplastikov on basis aluminum-lithium alloy 1441 with lowered density] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 174–183.
  14. Dement'eva L.A., Serezhenkov A.A., Lukina N.F., Kucevich K.E. Kleevye prepregi i sloistye materialy na ih osnove [Glue prepregs and layered materials on their basis] //Aviacionnye materialy i tehnologii. 2013. №2. S. 19–21.
  15. Kablov E.N., Antipov V.V., Senatorova O.G. Sloistye aljumostekloplastiki SIAL-1441 i sotrudnichestvo s Airbus i Tu Delft [Layered alyumostekloplastiki SIAL-1441 and cooperation with Airbus and Tu Delft] //Cvetnye metally. 2013. №9 (849). S. 50–53.
  16. Lukina N.F., Dement'eva L.A., Serezhenkov A.A., Kotova E.V., Senatorova O.G., Sidel'nikov V.V., Kucevich K.E. Kleevye prepregi i kompozicionnye materialy na ih osnove [Glue prepregs and composite materials on their basis] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 53–56.
  17. Hrychev Ju.I., Shkodina E.P., Magin N.A., Dement'eva L.A., Hajretdinov R.H., Kucevich K.E. Razrabotka tehnologicheskogo processa izgotovlenija radioprozrachnogo obtekatelja iz kleevyh prepregov tipa KMKS-2m.120 [Development of technological process of manufacturing of radio transparent fairing from glue prepregs of the KMKS-2M.120 type] //Klei. Germetiki. Tehnologii. 2013. №2. S. 27–30.