On rheological characteristics of alumina-based slip suspensions
UDC
532.584:666.37
DOI
10.18577/2307-6046-2015-0-8-6-6
Article PDF (Russian)
(647.83 KB)
How to cite
Buchilin N.V., Prager E.P. On rheological characteristics of alumina-based slip suspensions // Proceedings of VIAM. 2015. No. 8. DOI: 10.18577/2307-6046-2015-0-8-6-6. URL: https://www.viam-works.ru/en/journal/2015/8/6
Abstract
The results of rheology investigations of alumina-based slip suspensions intended for production of ceramic filters are presented. It was shown that the replacement of water used as a technological binder with the water solution of carbamide and aluminum oxychloride leads to an increase of suspensions fluidity that, in turn, facilitates formability of green bod-ies and improves mechanical characteristics of ceramic materials. The ranges of ratios between solid phase (sintered powders) and liquid phase (technological binder) providing coagulation and direct contacts between solid phase particles in slips were determined.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
- Buntushkin V.P., Kablov E.N., Bazyleva O.A., Morozova G.I. Splavy na osnove aljuminidov nikelja [Alloys on the basis of nickel aluminides] //MiTOM. 1999. №1. S. 32–34.
- Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokolenija [Nickel foundry hot strength alloys of new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 36–52.
- Aminzare M., Mazaheri M., Golestanifard F., Rezaie H.R., Ajeian R. Sintering behavior of nano alumina powder shaped by pressure filtration //Ceramics International. 2011. №37. P. 9–14.
- Keramicheskij fil'tr, soderzhashhij uglerodnoe pokrytie, i sposob ego izgotovlenija [The ceramic filter containing carbon covering, and way of its manufacturing]: pat. 2456056 Ros. Federacija; zajavl. 28.01.2008; opubl. 20.07.2012 Bjul. №20. 15 s.
- Yang W., Jiang B., Wang A., Shi H. Effect of Negatively Charged Ions on the Formation of Microarc Oxidation Coating on 2024 Aluminium Alloy //Journal of Material Science and Technology. 2012. №28 (8). P. 707–712.
- Vogt U.F., Gorbar M., Dimopoulos-Eggenschwiler P., Broenstrup A., Wagner G., Colombod P. Improving the properties of ceramic foams by a vacuum infiltration process //Journal of the European Ceramic Society. 2010. №30. P. 3005–3011.
- Himicheskaja tehnologija keramiki [Chemical technology of ceramics]: Uch. posobie dlja vuzov /Pod red. I.Ja. Guzmana. M.: OOO RIF Strojmaterialy. 2003. 496 s.
- Anciferov V.N. Problemy poroshkovogo materialovedenija [Problems of powder materials science]. Chast' II. Ekaterinburg: UrO RAN. 2002. 263 s.
- Kablov E.N. Korrozija ili zhizn' [Corrosion or life] //Nauka i zhizn'. 2012. №11. S. 16–21.
- Kablov E.N., Shhetanov B.V., Ivahnenko Ju.A., Balinova Ju.A. Perspektivnye armirujushhie vysokotemperaturnye volokna dlja metallicheskih i keramicheskih kompozicionnyh materialov [Perspective reinforcing high-temperature fibers for metal and ceramic composite materials] //Trudy VIAM. 2013. №2. St. 05 (viam-works.ru).
- Buchilin N.V., Prager E.P. Reologicheskie harakteristiki shlikernyh suspenzij na osnove oksida aljuminija [Rheological characteristics of slip suspensions on the basis of aluminum oxide] //Trudy VIAM. 2015. №5. St. 06 (viam-works.ru).
- Sandoval M.L., Camerucci M.A. Foaming performance of aqueous albumin and mullite-albumin systems used in cellular ceramic processing //Ceramics International. 2014. №40. P. 1675–1686.
- Magnani G., Brentari A., Burresi E., Raiteri G. Pressureless sintered silicon carbide with enhanced mechanical properties obtained by the two-step sintering method //Ceramics International. 2014. №40. P. 1759–1763.
- Shhukin E.D., Percov A.V., Amelina E.A. Kolloidnaja himija [Colloid chemistry]. 3-e izd., pererab. i dop. M.: Vysshaja shkola. 2004. 445 s.
- Praktikum i zadachnik po kolloidnoj himii [Workshop and the book of problems on colloid chemistry] /Pod red. V.V. Nazarova, A.S. Grodskogo. M.: Akademkniga. 2007. 374 s.
- Otto M. Sovremennye metody analiticheskoj himii [Modern methods of analytical chemistry]. 2-e izd. M.: Tehnosfera. 2006. 416 s.
- Frolov Ju.G. Kurs kolloidnoj himii. Poverhnostnye javlenija i dispersnye sistemy [Course of colloid chemistry. Surface phenomena and disperse systems]. 2-e izd. M.: Himija. 1989. 464 s.
- Kirienko T.A., Balinova Ju.A. Vlijanie atmosfernoj vlazhnosti na reologiju tonkih sloev koncentrirovannyh vodnyh rastvorov sistemy «neorganicheskie soli–organicheskij polimer» [Influence of atmospheric humidity on rheology of thin coats of the concentrated aqueous solutions of system «inorganic salts-organic polymers»] //Aviacionnye materialy i tehnologii. 2014. №2. S. 56–58.
- Shhetanov B.V., Balinova Ju.A., Ljuljukina G.Ju., Solov'eva E.P. Struktura i svojstva nepreryvnyh polikristallicheskih volokon α-Al2O3 [Structure and properties of continuous polycrystalline fibers α-Al2O3] //Aviacionnye materialy i tehnologii. 2012. №1. S. 13–17.
- Kirienko T.A., Balinova Ju.A. Fiziko-himicheskie svojstva mnogokomponentnyh rastvorov dlja keramicheskih materialov, soderzhashhih polivinilovyj spirt [Physical and chemical properties of multicomponent solutions for the ceramic materials containing polyvinyl alcohol] //Aviacionnye materialy i tehnologii. 2014. №1. S. 34–38.
- Uvarova N.E., Grashhenkov D.V., Isaeva N.V., Orlova L.A., Sarkisov P.D. Vysokotemperaturnye radioprozrachnye materialy: segodnja i zavtra [High-temperature radio transparent materials: today and tomorrow] //Aviacionnye materialy i tehnologii. 2010. №1. S. 16–21.
- Tehnologija stekla [The technology has flown down] /Pod red. I.I. Kitajgorodskogo. 3-e izd. M.: Gosudarstvennoe izdatel'stvo literatury po stroitel'stvu, arhitekture i stroitel'nym materialam. 1961. S. 517.
- Malkin A.Ja., Isaev A.I. Reologija: koncepcii, metody, prilozhenija [Rheology: concepts, methods, appendices]. SPb: Professija. 2007. 560 s.