Liquation in castings made of Zr-bearing magnesium alloys

Mukhina I.Y., Uridiya Z.P.
Mukhina I.Y., Uridiya Z.P. Liquation in castings made of Zr-bearing magnesium alloys // Proceedings of VIAM. 2015. No. 8. DOI: 10.18577/2307-6046-2015-0-8-3-3. URL: https://www.viam-works.ru/en/journal/2015/8/3
Abstract

An uneven distribution of structural components caused by the segregation processes in the alloy during its melting and crystallization may occur on separate machined surfaces of castings in the course of production of Zr-bearing cast magnesium alloys: ML9, ML10, ML12 and VML20 intended for housing parts of hydraulic units, pumps, loaded wheel castings. The article describes the nature and formation mechanism of segregated inclusions. Their influence on the properties of castings is shown.

Reference list
  1. Kornysheva I.S., Volkova E.F., Goncharenko E.S., Muhina I.Ju. Perspektivy primenenija magnievyh i litejnyh aljuminievyh splavov [Perspectives of application of magnesium and cast aluminum alloys] //Aviacionnye materialy i tehnologii. 2012. №S. C. 212–222.
  2. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  3. Kablov E.N. VIAM: prodolzhenie puti [VIAM: way continuation] //Nauka v Rossii. 2012. №3. S. 36–44.
  4. Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] //Nauka i zhizn'. 2010. №4. S. 2–7.
  5. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] //Metally Evrazii. 2012. №3. S. 10–15.
  6. Muhina I.Ju., Uridija Z.P. Magnij – osnova sverhlegkih materialov [Magnesium – basis of extralight materials] //Metallurgija mashinostroenija. 2005. №6. S. 29–31.
  7. Antipov V.V., Vahromov R.O., Dujunova V.A., Nochovnaja N.A. Materialy s vysokoj udel'noj prochnost'ju na osnove aljuminija, magnija, titana i tehnologii ih pererabotki [Materials with high specific strength on the basis of aluminum, magnesium, titanium and technology of their processing] //Boepripasy i spechimija. 2013. №3. S. 51–55.
  8. Sadkov V.V., Laponov Ju.L., Ageev A.P. i dr. Perspektivy i uslovija primenenija magnievyh splavov v samoletah OAO «Tupolev» [Perspectives and conditions of application of magnesium alloys in JSC Tupolev airplanes] //Metallurgija mashinostroenija. 2007. №4. S. 19–23.
  9. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] //Vse materialy: Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  10. Muhina I.Ju., Dujunova V.A., Uridija Z.P. Perspektivnye litejnye magnievye splavy [Perspective cast magnesium alloys] //Litejnoe proizvodstvo. 2013. №5. S. 2–5.
  11. Dujunova V.A., Goncharenko N.S., Muhina I.Ju., Uridija Z.P., Volkova E.F. Nauchnoe naprav-lenie akademika I.N. Fridljandera. Sovremennye issledovanija magnievyh i litejnyh aljuminievyh splavov v VIAM [Scientific direction of academician I.N. Fridlyandera. Modern researches of magnesium and cast aluminum alloys in VIAM] //Cvetnye metally. 2013. №9. S. 71–78.
  12. Frolov A.V., Muhina I.Ju., Dujunova V.A., Uridija Z.P. Vlijanie tehnologicheskih parametrov plavki na strukturu i svojstva novyh magnievyh splavov [Influence of technological parameters of melting on structure and property of new magnesium alloys] //Metallurgija mashinostroenija. 2014. №2. S. 26–29.
  13. Goncharenko E.S., Trapeznikov A.V., Ogorodov D.V. Litejnye aljuminievye splavy (k 100-letiju so dnja rozhdenija M.B. Al'tmana) [Cast aluminum alloys (to the 100 anniversary since the birth of M.B. Altman)] //Trudy VIAM. 2014. №4. St. 02 (viam-works.ru).
  14. Dujunova V.A., Muhina I.Ju., Uridija Z.P. Novye protivoprigarnye prisadochnye materialy dlja litejnyh form magnievyh otlivok [New protivoprigarny prisadochny materials for casting molds of magnesian otlivka] //Litejnoe proizvodstvo. 2009. №9. S. 18–21.
  15. Leonov A.A., Dujunova V.A., Stupak E.V., Trofimov N.V. Lit'e magnievyh splavov v razovye formy, poluchennye novymi metodami [Molding of magnesium alloys in the one-time forms received by new methods] //Trudy VIAM. 2014. №12. St. 01 (viam-works.ru).
  16. Kablov E.N. Himija v aviacionnom materialovedenii [Chemistry in aviation materials science] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  17. Muhina I.Ju. Litejnye splavy i tehprocessy pri proizvodstve magnievyh otlivok [Cast alloys and technical processes by production of magnesian otlivka] //Litejnoe proizvodstvo. 2003. №4. S. 18–19.
  18. Uridija Z.P., Muhina I.Ju. Novye propityvajushhie materialy dlja germetizacii otlivok iz aljuminievyh i magnievyh splavov [New impregnating materials for sealing of otlivka from aluminum and magnesium alloys] //Vse materialy. Jenciklopedicheskij spravochnik. 2011. №8. S. 37–41.
  19. Uridija Z.P., Muhina I.Ju. O germetizacii otlivok iz aljuminievyh i magnievyh splavov [About sealing of otlivka from aluminum and magnesium alloys] //Litejnoe proizvodstvo. 2012. №2. S. 14–16.
  20. Postnov V.I., Burhan O.L., Rahmatullin A.Je., Kachura S.M. Nerazrushajushhie metody kontrolja soderzhanija svjazujushhih v prepregah i PKM (obzor) [Nondestructive control methods of the contents binding in prepregs and PKM (review)] //Trudy VIAM. 2013. №12. St. 06 (viam-works.ru).
  21. Murashov V.V. Nerazrushajushhij kontrol' zagotovok i detalej iz uglerod-uglerodnogo kompozicionnogo materiala dlja mnogorazovogo kosmicheskogo korablja «Buran» [Non-destructive testing of preparations and details from carbon - carbon composite material for the reusable Snow-storm spacecraft] //Trudy VIAM. 2013. №4. St. 06 (viam-works.ru).
  22. Muhina I.Ju. Struktura i svojstva novyh litejnyh magnievyh splavov [Structure and properties of new cast magnesium alloys] //Litejnoe proizvodstva. 2011. №12. S. 12–14.
  23. Muhina I.Ju., Uridija Z.P., Stepanov V.V. Issledovanie kachestva magnievo-cirkonievoj ligatury [Research of quality of magnesium-zirconium ligature] /V kn.: Magnievye splavy dlja sovremennoj tehniki. M.: Nauka. 1992. S. 135–142.
  24. Rohlin L.L. Magnievye splavy, soderzhashhie redkozemel'nye metally [The magnesium alloys containing rare earth metals]. M.: Nauka. 1980. S. 47–55.
  25. Uridija Z.P., Muhina I.Ju., Dujunova V.A., Kosarina E.I. Kontrol' kachestva lit'ja iz magnievyh splavov i sposoby vosstanovlenija germetichnosti otlivok [Molding quality control from magnesium alloys and ways of recovery of tightness of otlivka] //Trudy VIAM. 2014. №12. St. 04 (viam-works.ru).