An influence of operational factors on the state of interfaces in high heat-resistant Ni-based alloys intended for GTE discs
UDC
669.018.44:669.245
DOI
10.18577/2307-6046-2015-0-8-2-2
Article PDF (Russian)
(616.8 KB)
How to cite
Chabina E.B. An influence of operational factors on the state of interfaces in high heat-resistant Ni-based alloys intended for GTE discs // Proceedings of VIAM. 2015. No. 8. DOI: 10.18577/2307-6046-2015-0-8-2-2. URL: https://www.viam-works.ru/en/journal/2015/8/2
Abstract
Changes in structure and chemical composition of grain boundaries in Ni–Co–Cr–Al–Ti–W–Mo–Nb wrought heat-resistant alloys after simulation of operation and operation in GTE disk structure were investigated. The researches have shown that there is a relationship between operational properties and the state of internal interfaces (grain boundaries). The determined regularities are general for Ni–Co–Cr–Al–Ti–W–Mo–Nb wrought Ni-based alloys with different content of alloying elements. It was stated that the mechanisms of a decreasing in cohesive strength of grain boundaries are different after holding within different temperature intervals.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period to 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
- Kablov E.N., Lomberg B.S., Ospennikova O.G. Sozdanie sovremennyh zharoprochnyh materialov i tehnologij ih proizvodstva dlja aviacionnogo dvigatelestroenija [Creation of modern heat resisting materials and technologies of their production for aviation engine building] //Kryl'ja Rodiny. 2012. №3–4. S. 34–38.
- Supersplavy [Superalloys]. T. II. Kn. 1. /Pod red. Ch.T. Simsa, N.S. Stoloffa, U.K. Hagelja. M.: Metallurgija. 1995. 384 s.
- Lomberg B.S., Moiseev S.A. Zharoprochnye deformiruemye splavy dlja diskov GTD i perspektivy ih razvitija [Heat resisting deformable alloys for disks GTD and perspective of their development] /V sb. Aviacionnye materialy: nauch.-tehnich. sb. M.: VIAM. 1982. S. 119–123.
- Lomberg B.S., Chabina E.B., Golubev A.A. Vlijanie vosstanovitel'noj termicheskoj obrabotki (VTO) na strukturu i svojstva diskov iz splava JeI698-VD [Influence of recovery thermal processing (WTO) on structure and property of disks from alloy EI698-VD] /V sb. Aviacionnye materialy i tehnologii. Vyp. «Remontnye tehnologii v aviastroenii». M.: VIAM. 2002. S. 14–20.
- Lomberg B.S. Zharoprochnye splavy i materialy dlja diskov GTD [Hot strength alloys and materials for disks GTD] /V sb. Aviacionnye materialy na rubezhe XX–XXI vekov: nauch.-tehnich. sb. M.: VIAM. 1994. S. 258–264.
- Lomberg B.S., Moiseev S.A. Zharoprochnye deformiruemye splavy dlja sovremennyh i perspektivnyh GTD [Heat resisting deformable alloys for modern and perspective GTD] /V sb. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2002: Jubilejnyj nauch.-tehnich. sb. M.: MISIS–VIAM. 2002. S. 82–93.
- Bokshtejn S.Z., Kishkin S.T., Shalin R.E. Strukturnaja stabil'nost' konstrukcionnyh materialov [Structural stability of constructional materials] /V sb. Aviacionnye materialy na rubezhe XX–XXI vekov. M.: VIAM. 1994. S. 547–553.
- Lomberg B.S., Bakradze M.M., Chabina E.B., Filonova E.V. Vzaimosvjaz' struktury i svojstv vysokozharoprochnyh nikelevyh splavov dlja diskov gazoturbinnyh dvigatelej [Interrelation of structure and properties of high-heat resisting nickel alloys for disks of gas turbine engines] //Aviacionnye materialy i tehnologii. 2011. №2. S. 25–30.
- Kablov E.N., Ospennikova O.G., Lomberg B.S. Kompleksnaja innovacionnaja tehnologija izotermicheskoj shtampovki na vozduhe v rezhime sverhplastichnosti diskov iz superzharoprochnyh splavov [Complex innovative technology of isothermal punching on air in mode of superplasticity of disks from superhot strength alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 129–141.
- Lomberg B.S., Ovsepjan S.V., Bakradze M.M., Mazalov I.S. Vysokotemperaturnye zharo-prochnye nikelevye splavy dlja detalej gazoturbinnyh dvigatelej [High-temperature heat resisting nickel alloys for details of gas turbine engines] //Aviacionnye materialy i tehnologii. 2012. №S. S. 52–57.
- Chabina E.B., Filonova E.V., Lomberg B.S., Morozova G.I. Jevoljucija struktury i fazovogo sostava deformiruemyh zharoprochnyh nikelevyh splavov dlja diskov GTD s uslozhneniem ih legirovanija [Evolution of structure and phase composition of deformable heat resisting nickel alloys for disks GTD with complication of their alloying] //MiTOM. 2015. №3 (717). S. 8–12.
- Chabina E.B., Filonova E.V., Lomberg B.S., Bakradze M.M. Struktura sovremennyh deformiruemyh nikelevyh splavov [Structure of modern deformable nickel alloys] //Vse materialy. Jenciklopedicheskij spravochnik. 2012. №6. S. 22–27.
- Kablov E.N., Bronfin M.B. Jeffekt S.T. Kishkina, ili pochemu struktura zharoprochnyh nikelevyh splavov dolzhna byt' geterofaznoj [Kishkin's effect or why the structure of heat resisting nickel alloys has to be heterophase] /V sb. Litejnye zharoprochnye splavy. Jeffekt S.T. Kishkina: Nauchn.-tehn. sb.; Pod. red. E.N. Kablova. M.: Nauka. 2006. S. 7–14.
- Lomberg B.S., Ovsepjan S.V., Bakradze M.M. Osobennosti legirovanija i termicheskoj obrabotki zharoprochnyh nikelevyh splavov dlja diskov gazoturbinnyh dvigatelej novogo pokolenija [Features of alloying and thermal processing of heat resisting nickel alloys for disks of gas turbine engines of new generation] //Aviacionnye materialy i tehnologii. 2010. №2. S. 3–8.
- Lomberg B.S., Bakradze M.M., Chabina E.B., Filonova E.V. Vlijanie mikrolegirujushhih jele-mentov na strukturno-fazovuju stabil'nost' i svojstva zharoprochnogo deformiruemogo splava (pri dlitel'nyh narabotkah) [Influence of microdoping elements on structural and phase stability and property of heat resisting deformable alloy (at long practices)] //Metallurg. 2013. №9. S. 93–97.
- Fizicheskoe metallovedenie. T. 1. Atomnoe stroenie metallov i splavov [Physical metallurgical science. T. 1. Nuclear structure of metals and alloys] /Pod red. R.U. Kana, P. Haazena. M.: Metallurgija. 1987. 639 s.
- Mak Lin D. Granicy zeren v metallah [Borders of grains in metals]. M.: Metallurgizdat. 1960. 322 s.
- Guttmann M. Grain boundary segregation, two dimensional compound formation and precipitation //Metal Transaction. 1977. V. A8. №9. P. 1383–1403.
- Meetham G.W. Trace elements in superalloys (overview) //Metals technology. 1984. V. 11. №10. P. 414–418.
- Ohrupchivanie konstrukcionnyh stalej i splavov [Okhrupchivaniye constructional staly and alloys] /Pod. red. K.L. Brajenta, S.K. Benerdzhi. M.: Metallurgija. 1988. 551 s.
- Guttmann M. Temper embrittlement and ternary equilibrium segregation //Material Science and Engineering. 1980. V. 42. P. 227–232.
- McLean M., Strang A. Effects of trace elements on mechanical properties of superalloys //Metals Technology. 1984. V. 11. №10. P. 454–465.
- Bragina T.K., Laricheva L.M. Osobennosti izmenenija harakteristik prochnosti diskov turbiny GTD posle dlitel'noj narabotki [Features of change of characteristics of durability of GTD turbine disks after long operating time] //Problemy prochnosti. 1976. №8. S. 78–87.
- Bragina T.K., Laricheva L.M. Osobennosti struktury materialov v svjazi s dlitel'noj narabotkoj diskov turbin GTD [Features of structure of materials in connection with long operating time of disks of turbines GTD] //Problemy prochnosti. 1978. №3. S. 34–43.
- Orehov N.G., Cherkasova E.R., Chabina E.B., Sidorenko V.I. Izuchenie poverhnostej razrushenija sovremennyh nikelevyh splavov metodom Ozhe-jelektronnoj spektroskopii [Studying of surfaces of destruction of modern nickel alloys by method Ozhe-elektronnoy of spectroscopy] /V sb. Voprosy aviacionnoj nauki i tehniki. Ser. «Aviacionnye materialy. Metody issledovanija konstrukcionnyh materialov». M.: VIAM. 1987. S. 150–156.
- Chabina E.B., Alekseev A.A., Filonova E.V., Lukina E.A. Primenenie metodov analiticheskoj mikroskopii i rentgenostrukturnogo analiza dlja issledovanija strukturno-fazovogo sostojanija materialov [Application of methods of analytical microscopy and the rentgenostrukturny analysis for research of structural and phase condition of materials] //Trudy VIAM. 2013. №5. St. 06 (viam-works.ru).
- Metody analiza poverhnosti [Methods of the analysis of surface] /Pod red. A.M. Zanderny. M.: Mir. 1979. 582 s.
- Edwards B.C., Byre B.L., Gage G. //Acta Metallurgica. 1980. V. 28. Р. 335–356.
- Was G.S., Martin J.R. The influence of grain boundary precipitation on the measurement of chromium redistribution and phosphorous segregation in Ni–16Cr–9Fe //Metallurgical Transaction. 1985. V. 16A. №3. P. 349–359.
- Guttmann M., Dumoulin P., Tan-Tai N., Fontaine P. An Auger Electron Spectroscopic study of phosphorus segregation in the grain boundaries of nickel base alloy 600 //Corrosion NACE. 1981. V. 37. №7. P. 416–425.
- Briant C.L. Grain boundary segregation in Ni-base alloy 182 //Metallurgical Transaction. 1988. V. 19A. №1. P. 137–143.
- Zhuanggi H., Hongwei S., Shouren G. Role of P, S and B on creep behavior of alloy 718 //Journal of Material Science and Technology. 2001. V. 17. №4. P. 399–402.