On the question of glass-forming ability tendency evaluation (review)

Stolyankov Yu.V., Aleksashin V.M., Antyufeeva N.V.
Stolyankov Yu.V., Aleksashin V.M., Antyufeeva N.V. On the question of glass-forming ability tendency evaluation (review) // Proceedings of VIAM. 2015. No. 7. DOI: 10.18577/2307-6046-2015-0-7-8-8. URL: https://www.viam-works.ru/en/journal/2015/7/8
Abstract

Amorphous metal materials are well known for unique complex of properties inherent in them. There have been developed a lot of production means of amorphous metals in different conditions – from thin and up to bulk amorphous metal materials. The question of the most importance here is some practical approaches to glass-forming ability tendency evaluation the materials of the kind. It defines not only possibility of production the alloy in amorphous state, but also characterizes productivity of the production means and quality of the product

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] //Metally Evrazii. 2012. №3. S. 10–15.
  3. Kablov E.N., Lomberg B.S., Ospennikova O.G. Sozdanie sovremennyh zharoprochnyh materia-lov i tehnologij ih proizvodstva dlja aviacionnogo dvigatelestroenija [Creation of modern heat resisting materials and technologies of their production for aviation engine building] //Kryl'ja Rodiny. 2012. №3–4. S. 34–38.
  4. Ryl'nikov V.S., Lukin V.I. Pripoi, primenjaemye dlja pajki materialov aviacionnogo naznachenija [The solders applied to the soldering of materials of aviation assignment] //Trudy VIAM. 2013. №8. St. 02 (viam-works.ru).
  5. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemel'nye jelementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of modern and future high technologies] //Trudy VIAM. 2013. №2. St. 01 (viam-works.ru).
  6. Evgenov A.G., Nerush S.V., Vasilenko S.A. Poluchenie i oprobovanie melkodispersnogo metallicheskogo poroshka vysokohromistogo splava na nikelevoj osnove primenitel'no k lazernoj LMD-naplavke [Receiving and approbation of finely divided metal powder of high-chromic nickel-based alloy with reference to laser LMD welding] //Trudy VIAM. 2014. №5. St. 04 (viam-works.ru).
  7. Afanas'ev-Hodykin A.N., Lukin V.I., Ryl'nikov V.S. Vysokotehnologichnye polufabrikaty zharoprochnyh pripoev (lenty i paty na organicheskom svjazujushhem) [Hi-tech semi-finished products of heat resisting solders (tapes and stalemates on organic binding)] //Trudy VIAM. 2013. №9. St. 02 (viam-works.ru).
  8. Chabina E.B., Alekseev A.A., Filonova E.V., Lukina E.A. Primenenie metodov analiticheskoj mikroskopii i rentgenostrukturnogo analiza dlja issledovanija strukturno-fazovogo sostojanija materialov [Application of methods of analytical microscopy and the rentgenostrukturny analysis for research of structural and phase condition of materials] //Trudy VIAM. 2013. №5. St. 06 (viam-works.ru).
  9. Farafonov D.P., Degovec M.L., Serov M.M. Issledovanie svojstv i tehnologicheskih para-metrov poluchenija metallicheskih volokon dlja istiraemyh uplotnitel'nyh materialov aviacionnyh GTD [Research of properties and technological parameters of receiving metal fibers for abraded sealing materials of aviation GTD] //Trudy VIAM. 2014. №7. St. 02 (viam-works.ru).
  10. Fizikohimija amorfnyh (stekloobraznyh) metallicheskih materialov [Fizikokhimiya of amorphous (stekloobrazny) metal materials] /Pod red. Ju.K. Kovneristogo. M.: Metallurgija. 1987. 328 s.
  11. Kovneristyj Ju.K., Osipov Je.K., Trofimova E.A. Fiziko-himicheskie osnovy sozdanija amorfnyh metallicheskih splavov [Physical and chemical bases of creation of amorphous metal alloys]. M.: Nauka. 1983. 145 s.
  12. Amorfnye metallicheskie materialy [Amorphous metal materials]. M.: Nauka. 1984. 158 s.
  13. Amorfnye metallicheskie splavy [Amorphous metal alloys]: Per. s angl. /Pod red. F.E. Ljuborskogo. M.: Metallurgija. 1987. 584 s.
  14. Shhereckij A.A., Shumihin V.S., Sergienko R.A. Fiziko-himicheskie aspekty poluchenija amorfnyh metallicheskih splavov pri nizkih skorostjah ohlazhdenija [Physical and chemical aspects of receiving amorphous metal alloys at low cooling rates] //Processy lit'ja. 2003. №4. S. 62–70.
  15. Klementjun W., Willens R.H., Duwez P. Non-crystalline Structure in Solidified Gold-Silicon Alloys //Nature. 1960. V. 187. P. 869–870.
  16. Sudzuki K., Fudzimori H., Hasimoto K. Amorfnye metally [Amorphous metals]. M.: Metallurgija. 1987. 328 s.
  17. Inoue A. Stabilization and high strain-rate super plasticity of metallic super cooled liquid //Materials Science and Engineering. A. 1999. V. 267. №2. P. 171–183.
  18. Zrnik J. Materials development trends connected with materials science and technology research //Metalurgija. 2000. V. 39. №3. P. 147–155.
  19. Vereshagin M.N., Stasenko D.L., Celuev M.Ju. Analiz processa amorfizacii slozhnolegirovannyh splavov na zheleznoj osnove pri zakalke iz rasplava [The analysis of process of amorfizatsiya of complex-alloyed alloys on iron basis when tempering from rasplava] //Materialy tehnologii, instrumenty. 2003. T. 8. №1. S. 51–56.
  20. Davies H.A., Aucote J., Hull J.B. Amorphous Nickel produced by Splat Quenching //Nature. 1973. V. 246. P. 13–14.
  21. Alehin V.P., Honik V.A. Struktura i fizicheskie zakonomernosti deformacii amorfnyh splavov [Structure and physical patterns of deformation of amorphous alloys]. M.: Metallurgija. 1992. 248 s.
  22. Turnbull D. Under what conditions can a glass be formed? //Contemporary Physics. 1969. V. 10. №5. P. 473–488.
  23. Donald I.W., Davies H.A., Kenemy T. The effect of Pt-group metal additions on the thermal stability of Fe- and Ni-based glass alloys //Journal non-crystalline solids. 1982. V. 50. P. 351–358.
  24. Polk D.E., Gissen B.K. Metallicheskie stekla: Per. s angl [Metal glasses]. M.: Metallurgija. 1984. S. 12–39.
  25. Anosov V.Ja., Ozerova M.I., Fialkov Ju.Ja. Osnovy fiziko-himicheskogo analiza [Bases of the physical and chemical analysis]. M.: Nauka. 1976. 503 s.
  26. Novikov I.I. Teorija termicheskoj obrabotki metallov [Theory of thermal processing of metals]. M.: Metallurgija. 1978. 392 s.
  27. Zhukova L.A. Atomnoe stroenie metallov i splavov v zhidkom i amorfnom sostojanii [Nuclear structure of metals and alloys in liquid and amorphous state]: Ucheb. posob. Ekaterinburg: UGTU–UPI. 2009. 192 s.
  28. Krasnov V.Ju. Issledovanie atomnoj struktury amorfnogo nikelja i strukturnyh prevra-shhenij, soprovozhdajushhih ego kristallizaciju [Research of nuclear structure of amorphous nickel and the structural transformations accompanying its crystallization]. Avtoref. k.f.-m.n. Barnaul. 2009. 19 s.
  29. Levchenko E.V., Evteev A.V., Vahmin S.Ju., Kosilov A.T., Prjadil'shhikov A.Ju. Klasternaja model' strukturnoj organizacii amorfnogo zheleza [Pryadilshchikov A.Yu. Klasterny model of the structural organization of amorphous iron] //Fizika metallov i materialovedenie. 2010. T. 109. №6. S. 603–607.