Paint-and-lacquer materials with lowered content of volatile organic compounds (review)

Eskov A.A., Lebedeva T.A., Belova M.V.
Eskov A.A., Lebedeva T.A., Belova M.V. Paint-and-lacquer materials with lowered content of volatile organic compounds (review) // Proceedings of VIAM. 2015. No. 6. DOI: 10.18577/2307-6046-2015-0-6-8-8. URL: https://www.viam-works.ru/en/journal/2015/6/8
Abstract

The development trends of paint-and-lacquer materials, whose production and application are connected with the lowered content of volatile, toxic and flammable or-ganic sub-stances are considered. Various paint-and-lacquer materials are used for painting of a-chitectural objects, metal structures, products from polymeric composite materials. For this purpose, they have to possess good adhesion to surface, good protective and anticorrosive properties, stability to atmospheric and mechanical impacts.

Reference list
  1. Chebotarevskij V.V., Kondrashov Je.K. Tehnologija lakokrasochnyh pokrytij v mashi-nostroenii [Technology of paint coatings in mechanical engineering]. M.: Mashinostroenie. 1978. 295 s.
  2. Kondrashov Je.K., Kuznecova V.A., Semenova L.V., Lebedeva T.A., Malova N.E. Razvi-tie aviacionnyh lakokrasochnyh materialov [Development of aviation paint and varnish materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2012. №5. S. 49–54.
  3. Kuznecova V.A., Kuznecov G.V. Tendencii razvitija v oblasti toplivostojkih lakokraso-chnyh pokrytij dlja zashhity toplivnyh kesson-bakov letatel'nyh apparatov (obzor) [Devel-opment tendencies in the field of toplivostoyky paint coatings for protection fuel caisson tanks of flight vehicles (review)] //Trudy VIAM. 2014. №11. St. 08 (viam-works.ru).
  4. Kablov E.N. Himija v aviacionnom materialovedenii [Chemistry in aviation materials sci-ence] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  5. Kablov E.N. Materialy i himicheskie tehnologii dlja aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] //Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  6. Istorija aviacionnogo materialovedenija: VIAM – 75 let poiska, tvorchestva, otkrytij [His-tory of aviation materials science: VIAM – 75 years of search, creativity, opening] /Pod obshh. red. E.N. Kablova. M.: Nauka. 2007. S. 152–158.
  7. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strate-gicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 go-da» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  8. Semenova L.V., Malova N.E., Kuznecova V.A., Pozhoga A.A. Lakokrasochnye materialy i po-krytija [Paint and varnish materials and coverings] //Aviacionnye materialy i tehnologii. 2012. №S. S. 315–327.
  9. Kondrashov Je.K., Kuznecova V.A., Semenova L.V., Lebedeva T.A. Osnovnye napravleni-ja po-vyshenija jekspluatacionnyh, tehnologicheskih i jekologicheskih harakteristik lakokrasochnyh pokrytij dlja aviacionnoj tehniki [The main directions of increase of utili-zation, technical and ecological properties of paint coatings for aviation engineering] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 96–102.
  10. Kuznecova V.A., Semenova L.V., Kondrashov Je.K., Lebedeva T.A. Lakokrasochnye ma-terialy s ponizhennym soderzhaniem vrednyh i toksichnyh komponentov dlja okraski agre-gatov i konstrukcij iz PKM [Paint and varnish materials with the lowered content of harm-ful and toxic components for coloring of units and designs from PKM] //Trudy VIAM. 2013. №8. St. 05 (viam-works.ru).
  11. Hennesi T. Novye dostizhenija v reologii sudovyh i zashhitnyh lakokrasochnyh materialov s vysokim suhim ostatkom [New achievements in rheology of ship and protection paint and varnish materials with the high dry rest] //Lakokrasochnye materialy i ih primenenie. 2014. №9. S. 28–31.
  12. Konga X., Liua G., Qib H., Curtisa J.M. Preparation and characterization of high-solid polyurethane coating systems based on vegetable oil derived polyols //Progress in Organic Coatings. 2013. №76. Р. 1151–1160.
  13. Mannari V.M., Massingill J.L. Two-component high-solid polyurethane coating systems based on soy polyols //JCT Research. 2006. №3. P. 151–157.
  14. Naik R.B., Ratna D., Singh S.K. Synthesis and characterization of novel hyperbranched alkyd and isocyanate trimer based high solid polyurethane coatings //Progress in Organic Coatings. 2014. №77. P. 369–379.
  15. Diaz I., Chico B., Fuente D., Simancas J., Vega J.M., Morcillo M. Corrosion resistance of new epoxy-siloxane hybrid coatings. A laboratory study //Progress in Organic Coatings. 2010. №69. P. 278–286.
  16. Brusciotti F., Snihirova D.V., Xue H., Montemor M.F., Lamaka S.V., Ferreira M.G.S. Hybrid epoxy-silane coatings for improved corrosion protection of Mg alloy //Corrosion Science. 2013. №67. P. 82–90.
  17. Ahmad S., Gupta A.P., Sharmin E., Alam M., Pandey S.K. Synthesis, characterization and development of high performance siloxane-modified epoxy paints //Progress in Organic Coatings. 2005. №54. P. 248–255.
  18. Qian M., Soutar A.M., Tan X.H., Zeng X.T., Wijesinghe S.L. Two-part epoxy-siloxane hybrid corrosion protection coatings for carbon steel //Thin Solid Films. 2009. №517. P. 5237–5242.
  19. Pathak S.S., Khanna A.S. Investigation of anti-corrosion behavior of waterborne orga-nosilane–polyester coatings for AA6011 aluminum alloy //Progress in Organic Coatings. 2009. №65. P. 288–294.
  20. Xue D., Ooij W.J.V. Corrosion performance improvement of hot-dipped galvanized (HDG) steels by electro-deposition of epoxy-resin-ester modified bis-[tri-ethoxy-silyl] ethane (BTSE) coatings //Progress in Organic Coatings. 2013. №76. P. 1095–1102.
  21. Kunst S.R., Cardoso H.R.P., Oliveira C.T., Santana J.A., Sarmento V.H.V., Muller I.L., Malfatti C.F. Corrosion resistance of siloxane-poly(methyl methacrylate) hybrid films modified with acetic acid on tin plate substrates: Influence of tetraethoxysilane addition //Applied Surface Science. 2014. №298. P. 1–11.
  22. Seo J.Y., Han M. Multi-functional hybrid coatings containing silica nanoparticles and anti-corrosive acrylate monomer for scratch and corrosion resistance //Nanotechnology. 2011. №22. P. 1–9.
  23. Ozcam А.Е., Spontak R.J., Genzer J. Towards the Development of a Versatile Functional-ized Silicone Coating //ACS Applied Materials Interfaces. 2014. P. 22544–22552.
  24. Babkin O.Je., Myskina E.D. Plenki na osnove butadienstirol'nogo i stirolakrilovogo late-ksov, modificirovannyh metilfenil-polisiloksanovoj smoloj [Films on the basis of the buta-diene-styrene and stirolakrilovy latex modified by metilfenil-polysiloxane pitch] //Lakokrasochnye materialy i ih primenenie. 2013. №9. S. 39–41.
  25. Pathak S.S., Sharma A., Khanna A.S. Value addition to waterborne polyurethane resin by silicone modification for developing high performance coating on aluminum alloy //Progress in Organic Coatings. 2009. №65. P. 206–216.
  26. Zhoua H., Wanga H., Tiana X., Zhenga K., Cheng Q. Effect of 3-Aminopropyltriethoxysilane on polycarbonate based waterborne polyurethane transparent coatings //Progress in Organic Coatings. 2014. №77. P. 1073–1078.
  27. Lambourne R., Strivens T.A. Paint and surface soatings – theory and practice //Second edition Woodhead Publishing Limited. 1999. Reprinted 2004.
  28. Weiss K.D. Paint and coatings: A mature industry in transition //Progress in Polymer Sci-ence. 1997. №22. P. 203–245.
  29. Bestetti M., Cavallotti P.L., Da Forno A., Pozzi S. Anodic oxidation and powder coating for corrosion protection of AM60B magnesium alloys //Transactions of the Institute of Metal Finishing. 2007. №85. P. 316–319.
  30. Barletta M., Tagliaferri V. Electrostatic fluidized bed deposition of a high performance-polymeric powder on metallic substrates //Surface and Coatings Technology. 2006. №200. P. 4282–4290.
  31. Pathak S.S., Khanna A.S., Sinha T.J.M. Sol-gel derived organic–inorganic hybrid coating: A new era in corrosion protection of material //Corrosion Reviews. 2006. №24. P. 281–306.
  32. Boccaccini A.R., Zhitomirsky I. Application of electrophoretic and electrolytic deposition techniques in ceramics processing //Current Opinion in Solid State & Materials Science. 2002. №6. P. 251–260.
  33. Besra L., Liu M. A review on fundamentals and applications of electrophoretic deposition (EPD) //Progress in Materials Science. 2007. №52. P. 1–61.
  34. Zhang J., Wu C.Y. Corrosion protection behavior of AZ31 magnesium alloy with cathodic electrophoretic coating pretreated by silane //Progress in Organic Coatings. 2009. №66. P. 387–392.
  35. Bakkar A., Neubert V. Electrodeposition onto magnesium in air and water stable ionic liquids: from corrosion to successful plating //Electrochemistry Communications. 2007. №9. P. 2428–2435.
  36. Zhang J., Yang S., Wu C.Y., Zeng R.C. Galvanic corrosion of AM50 magnesium alloy with cathodic electrophoretic coating and Q235 steel //Rare Metal Materials and Engineer-ing. 2009. №38. P. 1158–1163.
  37. Zucchi F., Grassi V., Frignani A., Monticelli C., Trabanelli G. Influence of a silane treat-ment on the corrosion resistance of a WE43 magnesium alloy //Surface and Coatings Technology. 2006. №200. P. 4136–4143.
  38. Montemor M., Ferreira M. Electrochemical study of modified bis-[triethoxysilylpropyl] tetrasulfide silane films applied on the AZ31 Mg alloy //Electrochimica Acta. 2007. №52. P. 7486–7495.
  39. Li G.Y., Lian J.S., Niu L.Y., Jiang Z.H., Dong H. Effect of zinc–phosphate–molybdate conversion precoating on performance of cathode epoxy electrocoat on AZ91D alloy //Surface Engineering. 2007. №23. P. 56–61.
  40. Song G.-L. Electroless deposition of a pre-film of electrophoresis coating and its corrosion resistance on a Mg alloy. // Electrochimica Acta. 2010. №55. P. 2258–2268.
  41. Wang D., Bierwagen G.P. Sol-gel coatings on metals for corrosion protection //Progress in Organic Coatings. 2009. №64. P. 327–338.
  42. Khramov A., Balbyshev V., Kasten L., Mantz R. Sol-gel coatings with phosphonate func-tionalities for surface modification of magnesium alloys //Thin Solid Films. 2006. №514. P. 174–181.
  43. Lamaka S., Montemor M., Galio A., Zheludkevich M., Trindade C., Dick L., Ferreira M. Novel hybrid sol-gel coatings for corrosion protection of AZ31B magnesium alloy //Electrochimica Acta. 2008. №53. P. 4773–4783.
  44. Oichi M., Takamiy K., Kiyohara O., Nakanishi T. Effect of the addition of aramid-silicone block copolymer on phase structure and toughness of cured epoxy resins modified with silicone //Polymer. 1998. №39. P. 725–731.
  45. Rouw A.C. Model epoxy powder coatings and their adhesion to steel //Progress in Organ-ic Coatings. 1998. №34. P. 181–192.
  46. Wegmann А. Novel waterborne epoxy resin emulsion //Journal of coating technology. 1993. №65. P. 27–34.
  47. Miskovic-Stankovic V.B., Drazic D.M., Teodorovic M.J. Electrolyte penetration through epoxy coatings electrodeposited on steel //Corrosion Science. 1995. №37. P. 241–151.
  48. Miskovic-Stankovic V.B., Zotovic J.B., Kacarevic-Popovic Z., Maksimovic M.D. Corro-sion behaviour of epoxy coatings electrodeposited on steel electrochemically modified by Zn–Ni alloy //Electrochimica Acta. 1999. №44. P. 4269–4277.
  49. Patel C.J., Dighe А. Novel isocyanate-free self-curable cathodically depositable epoxy coatings: Influence of epoxy groups on coating properties //Progress in Organic Coatings. 2007. №60. P. 219–223.
  50. Liu B., Wang Y. A novel design for water-based modified epoxy coating with anti-corrosive application properties //Progress in Organic Coatings. 2014. №77. P. 219–224.
  51. Shah M.Y., Ahmad S. Waterborne vegetable oil epoxy coatings: Preparation and charac-terization. //Progress in Organic Coatings. 2012. №75. P. 248–252.
  52. Konwar U., Karak N., Jana T. Vegetable oil-based highly branched polyester modified epoxy based low VOC high solid industrial paint //Journal of Applied Polymer Science. 2012. №125 (S2). P. E2–E9.
  53. Almeida E., Santos D., Fragata F., Fuente D., Morcillo M. Anticorrosive painting for a wide spectrum of marine atmospheres: environmental-friendly versus traditional paint sys-tems //Progress in Organic Coatings. 2006. №57. P. 11–22.
  54. Gaschke M., Dreher B. Review of solvent-free liquid epoxy coating technology //Journal Coating Technology. 1976. №48. P. 46–51.
  55. Samuelsson J., Sundell P.E., Johansson M. Synthesis and polymerization of a radiation curable hyperbranched resin based on epoxy functional fatty acids //Progress in Organic Coatings. 2004. №50. P. 193–198.
  56. Ou J., Yang Y., Gan J., Ha C., Zhang M. Preparation, properties, and applications of acrylic–polyurethane hybrid emulsions in extinction electrophoresis //Journal of Applied Polymer Science. 2014. №131 (7). P. 1–9.
  57. Kjellqvist K. Reactive acid curing waterborne microparticles //Progress in Organic Coat-ings. 1994. №24. P. 209–223.
  58. Ben H.-J., Ji C.-Q., Cheng F., Cui W.-Z., Chen Y. Water-borne core–shell latexes of acry-late-vinylidene chloride copolymers: preparation, characterization, and their anticorrosive properties. //Industrial & engineering chemistry research. 2014. №53. P. 17362−17369.
  59. Barbosa J.V., Veludo E., Moniz J., Mendes A., Magalhaes F.D., Margarida М.S.M. Bastos. Low VOC self-crosslinking waterborne acrylic coatings incorporatingfatty acid de-rivatives //Progress in Organic Coatings. 2013. №76. P. 1691–1696.
  60. Dhoke S.K., Sinha T.J.M., Dutta P., Khanna A.S. Formulation and performance study of low molecular weight, alkyd-based waterborne anticorrosive coating on mild steel //Progress in Organic Coatings. 2008. №62. P. 183–192.
  61. Pathan S., Ahmad S. s‑Triazine ring-modified waterborne alkyd: synthesis, characteriza-tion, antibacterial, and electrochemical corrosion studies //ACS Sustainable Chemistry En-gineering. 2014. P. 1246–1257.
  62. Rao M., Samarnayake G., Marlow J., Tomko R. Novel waterborne soy hybrid dispersions and soy latex emulsion for coatings applications /In Soy-Based Chemicals and Materials; Brentin; ACS Symposium Series; American Chemical Society: Washington. DC. 2014. Сh. 9. P. 193–196.
  63. Coogan R.G. Post-Crosslinking of Water-Borne Urethanes //Progress in Organic Coatings. 1997. №32. P. 51–63.
  64. Geurink P., Veer T., Buter R., Rood I., Schlief J., Ven L., Leijzer R. Binder systems for waterborne two-pack products for car refinishes application //Progress in Organic Coatings. 2003. №48. P. 153–160.
  65. Brinkman E., Vandevoorde P. Waterborne two-pack isocyanate-free systems for industrial coatings //Progress in Organic Coatings. 1998. №34. P. 21–25.
  66. Clamena G., Ferrari T., Fu Z., Hejl A., Larson G., Procopio L., Rosano W., Sheppard A., Swartz A. Protection of metal with a novel waterborne acrylic/urethane hybrid technology //Progress in Organic Coatings. 2011. №72. P. 144–151.
  67. Wua G., Konga Z., Chena J., Huoa S., Liua G. Preparation and properties of waterborne polyurethane/epoxy resin composite coating from anionic terpene-based polyol dispersion //Progress in Organic Coatings. 2014. №77. P. 315–321.
  68. Berg K.J., Ven L.G.J., Haak H.J.W. Development of waterborne UV-A curable clear coat for car refinishes //Progress in Organic Coatings. 2008. №61. P. 110–118.
  69. Li K., Shen Y., Fei G., Wang H., Li J. Preparation and properties of castor oil/pentaerythritoltriacrylate-based UV curable waterborne polyurethane acrylate //Progress in Organic Coatings. 2015. №78. P. 146–154.
  70. Babkin O.Je., Babkina L.A., Letunovich O.A., Jacenko I.A. Vinilirovannye alkidy v pokrytijah UF-otverzhdenija [Vinilirovannye alkidy in coverings UF-otverzhdeniya] //Lakokrasochnye materialy i ih primenenie. 2014. №5. S. 61–63.
  71. Babkin O.Je., Babkina L.A., Kazachenko N.N., Arabej A.V. Zashhitnye pokrytija dvojnogo UF-otverzhdenija [Protecting covers of the double UF-otverzhdeniya] //Lakokrasochnye materialy i ih primenenie. 2014. №6. S. 47–50.
  72. Fataliev R.Ju., Homko E.V., Mashljakovskij L.N. Issledovanie svojstv plenok i pokrytij iz UF-otverzhdaemoj poliuretanakrilatnoj dispersii, modificirovannoj vodnoj jemul'siej silana [Research of properties of films and coverings from UF-otverzhdayema of the poliuretana-krilatny dispersion modified by water emulsion of silane] //Lakokrasochnye materialy i ih primenenie. 2013. №12. S. 51–54.
  73. Kowalczyk K., Spychaj T. Epoxy coatings with modified montmorillonites //Progress in Organic Coatings. 2008. №62. P. 425–429.
  74. Gordeeva N.V., Tolmachev I.A., Mashljakovskij L.N., Vasil'ev V.K. Modifikacija akrilo-vyh dispersij nanorazmernymi chasticami sloistyh silikatov dlja poluchenija pokrytij s povyshennymi jekspluatacionnymi svojstvami [Updating of acrylic dispersions by nanodimensional particles of layered silicates for receiving coverings with the increased operational properties] //Lakokrasochnye materialy i ih primenenie. 2013. №8. S. 23–26.
  75. H'juer M., Ajhenberger F., Herrvert S. Nanochasticy dioksida kremnija v organo-rastvorimyh vysokogljancevyh 2K poliuretanovyh lakah dlja plastikov [Silicon dioxide na-noparticles in organorastvorimy high-glossy 2К polyurethane varnishes for plastics] //Lakokrasochnye materialy i ih primenenie. 2013. №9. S. 16–20.
  76. Zhang S., Yu A., Song X., Liu X. Synthesis and characterization of waterborne UV-curable polyurethane nanocomposites based on the macromonomer surface modification of colloidal silica //Progress in Organic Coatings. 2013. №76. P. 1032–1039.
  77. Lewis O.D., Critchlow G.W., Wilcox G.D., Zeeuw A., Sander J. A study of the corrosion resistance of a waterborne acrylic coating modified with nano-sized titanium dioxide //Progress in Organic Coatings. 2012. №73. P. 88–94.
  78. Rahman O., Kashif M., Ahmad S. Nanoferrite dispersed waterborne epoxy-acrylate: Anti-corrosive nanocomposite coatings //Progress in Organic Coatings. 2015. №80. P. 77–86.
  79. Ruiz M.M., Cavaille J.Y., Dufresne A., Graillat C., Gereard J.-F. New waterborne epoxy coatings based on cellulose nanofillers //Macromolecular Symposia. 2001. №169. P. 211–222.