Determination of the mass fraction of tantalum in Fe–Ni–Co–Ta alloys

Goundobin N.V., Titov V.I., Pilipenko L.V.
Goundobin N.V., Titov V.I., Pilipenko L.V. Determination of the mass fraction of tantalum in Fe–Ni–Co–Ta alloys // Proceedings of VIAM. 2015. No. 6. DOI: 10.18577/2307-6046-2015-0-6-7-7. URL: https://www.viam-works.ru/en/journal/2015/6/7
Abstract

The aim of this study was to conduct research on the development of methods for determination of tantalum mass fraction (within the range of 2–15% mass.) in Fe–Ni–Co–Ta alloys. In addition to the main alloying elements, the alloy may contain the following impurities: 2–3% mass. of titanium and microimpurities of chromium, aluminum and silicon. Studies on the selection of the conditions for translation of analytical sample of Fe–Ni–Co–Ta alloy into solution. For the subsequent deposition and separation of tantalum from the other alloy components, reagent tannin was selected. An effect of acidity on the completeness of the deposition of tantalum with tannin was studied. It was determined that for elimination of errors in the determination of tantalum due to co-precipitation of titanium a double re-precipitation of tantalum is required. The studies allowed to develop a method of gravimetric determination of the mass fraction of tantalum (within the range of 2–15% mass.) in Fe–Ni–Co–Ta a

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strate-gicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34) S. 3–33.
  2. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokolenija [Nickel foundry hot strength alloys of new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 36–52.
  3. Mubojadzhjan S.A., Aleksandrov D.A., Gorlov D.S., Egorova L.P., Bulavinceva E.E. Zashhitnye i uprochnjajushhie ionno-plazmennye pokrytija dlja lopatok i drugih otvetstvennyh detalej kompressora GTD [Protective and strengthening ion-plasma coverings for blades and other responsible details of the GTD compressor] //Aviacionnye materialy i tehnologii. 2012. №S. S. 71–81.
  4. Mubojadzhjan S.A., Lucenko A.N., Aleksandrov D.A., Gorlov D.S. Issledovanie vozmozhnosti povyshenija sluzhebnyh harakteristik lopatok kompressora GTD metodom ionnogo modificirovanija poverhnosti [Research of possibility of increase of office characteristics of compressor blades of GTD by method of ionic modifying of surface] //Trudy VIAM. 2013. №1. St. 02 (viam-works.ru).
  5. Kablov E.N. Materialy dlja izdelija «Buran» – innovacionnye reshenija formirovanija shestogo tehnologicheskogo uklada [Materials for the product «Buran» – innovative solutions of forming of the sixth technological way] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
  6. Markova E.S., Pokrovskaja N.G., Shal'kevich A.B., Gromov V.I. Martensitostarejushhie stali – novye perspektivnye materialy dlja valov GTD [Maraging became – new perspective materials for GTD shaft] //Aviacionnye materialy i tehnologii. 2012. №S. S. 81–84.
  7. Markova E.S., Revjakina O.K., Petrakov A.F. Novaja vysokoprochnaja martensitostarejushhaja stal' VKS-170 [New high-strength VKS-170 maraging steel] /V cb. Voprosy aviacionnoj nauki i tehniki. Ser. «Aviacionnye materialy». Vyp. Vysokoprochnye stali. M.: VIAM. 1986. S. 36–40.
  8. Gibalo I.M. Analiticheskaja himija niobija i tantala [Analytical chemistry of niobium and tantalum]. M.: Nauka. 1967. 352 s.
  9. Elinson S.V. Spektrofotometrija niobija i tantala [Niobium and tantalum spectrophotometry]. M.: Atomizdat. 1973. 288 s.
  10. Marchenko Z. Fotometricheskoe opredelenie jelementov [Photometric definition of elements]: Per. s pol'sk. M.: Mir. 1971. S. 276–287.
  11. OST1 90430–96. Otraslevoj standart. Splavy nikelevye zharoprochnye. Metod opredelenija tantala [Industry standard. Alloys the nickel heat resisting. Method of definition of tantalum].