Threads of refractory oxides for sealing thermal insulation

Zimichev A.M., Varrik N.M., Sumin А.V.
Zimichev A.M., Varrik N.M., Sumin А.V. Threads of refractory oxides for sealing thermal insulation // Proceedings of VIAM. 2015. No. 6. DOI: 10.18577/2307-6046-2015-0-6-5-5. URL: https://www.viam-works.ru/en/journal/2015/6/5
Abstract

An influence of sizing agents and auxiliary threads on ability to weaving of threads from alumina continuous fibers on the braiding equipment is studied. Tests were carried out to define breaking loading and flexibility of threads. The experiments allowed to establish that the usage of auxiliary threads and sizing agent facilitates application of heat-resistant ceramic threads for production of flexible sealing thermal insulation.

Reference list
  1. Kablov E.N., Shhetanov B.V., Ivahnenko Ju.A., Balinova Ju.A. Perspektivnye armirujushhie vysokotemperaturnye volokna dlja metallicheskih i keramicheskih kompozicionnyh materialov [Perspective reinforcing high-temperature fibers for metal and ceramic compo-site materials] //Trudy VIAM. 2013. №2. St. 05 (viam-works.ru).
  2. Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] //Nauka i zhizn'. 2010. №4. S. 2–7.
  3. Kablov E.N., Shhetanov B.V., Ivahnenko Ju.A. Poluchenie, struktura i prochnost' volokon Al2O3 [Receiving, structure and durability of Al2O3 fibers] /V sb. trudov Mezhdunarodnoj konf. «Teorija i praktika tehnologij proizvodstva izdelij iz kompozicionnyh materialov i novyh metallicheskih splavov». M. 2003. S. 194–196.
  4. Oxide Fibers for High-Temperature Reinforcement and Insulation, Bunsell Ecole Nationale Superieure des Mines de Paris //J. Miner., Metalls and Mater. Sci. 2005. V. 57. №2. С. 48–51.
  5. Varrik N.M. Termostojkie volokna i teplozvukoizoljacionnye ognezashhitnye materialy [Heat-resistant fibers and heatsound-proof fireproof materials] //Trudy VIAM. 2014. №6. St. 07 (viam-works.ru).
  6. Composite sewing thread of ceramic fibers: pat. №4375779 US; pabl. 08.03.1983.
  7. Aluminum borate and aluminum borosilicate articles: pat. №3795524 US; pabl. 05.03.1974.
  8. Twisted ceramic fiber sewing thread: pat. №4430851 US; pabl. 14.02.1984.
  9. Razdel kataloga produkcii kompanii 3M (SShA) www.3m.com Ceramic Textiles and Composites Nextel 440 Braided Sleeving.
  10. Sposob poluchenija vysokotemperaturnogo volokna na osnove oksida aljuminija [Way of receiving high-temperature fiber on the basis of aluminum oxide]: pat. №2212388 Ros. Federacija; opubl. 20.09.2003.
  11. Zimichev A.M., Varrik N.M., Dalin M.A. Izmerenie modulja uprugosti volokon iz tugoplavkih oksidov [Measurement of elastic modulus of fibers from high-melting oxides] //Trudy VIAM. 2014. №6. St. 05 (viam-works.ru).
  12. Shheglova T.M., Zimichev A.M., Varrik N.M. Issledovanie obrazcov shnura iz volokon Fiber-frax [Research of samples of cord from Fiberfrax fibers] //Trudy VIAM. 2014. №9. St. 05 (viam-works.ru).
  13. Zimichev A.M., Varrik N.M. Termogravimetricheskie issledovanija nitej na osnove oksida aljuminija [Thermogravimetric researches of threads on the basis of aluminum oxide] //Trudy VIAM. 2014. №6. St. 06 (viam-works.ru).
  14. Shhetanov B.V., Ivahnenko Ju.A., Babashov V.G. Teplozashhitnye materialy [Heat-protective materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 12–20.
  15. Ivahnenko Ju.A., Babashov V.G., Zimichev A.M., Tinjakova E.V. Vysokotemperaturnye teploizoljacionnye i teplozashhitnye materialy na osnove volokon tugoplavkih soedinenij [High-temperature heatinsulating and heat-protective materials on the basis of fibers of high-melting connections] //Aviacionnye materialy i tehnologii. 2012. №S. S. 380–386.
  16. Lugovoj A.A., Babashov V.G., Karpov Ju.V. Temperaturoprovodnost' gradientnogo tep-loizoljacionnogo materiala [Temperaturoprovodnost of gradient heatinsulating material] //Trudy VIAM. 2014. №2. St. 02 (viam-works.ru).