Some features of high-temperature bend tests of Nb-based CM specimens

Basargin O.V., Kolyshev S.G., Schetanov B. V., Shcheglova T.M.
Basargin O.V., Kolyshev S.G., Schetanov B. V., Shcheglova T.M. Some features of high-temperature bend tests of Nb-based CM specimens // Proceedings of VIAM. 2015. No. 5. DOI: 10.18577/2307-6046-2015-0-5-11-11. URL: https://www.viam-works.ru/en/journal/2015/5/11
Abstract

The development of high-temperature structural materials means determination of their strength properties at operation temperatures. The decisions of the main problems of mechanical tests of specimens made from Nb-based matrix composite materials (CM) at 1300–1400°С are described in this work.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N., Shhetanov B.V., Ivahnenko Ju.A., Balinova Ju.A. Perspektivnye armirujushhie vysokotemperaturnye volokna dlja metallicheskih i keramicheskih kompozicionnyh materialov [Perspective reinforcing high-temperature fibers for metal and ceramic composite materials] //Trudy VIAM. 2013. №2. St. 05 (viam.works.ru).
  3. Kablov E.N., Grashhenkov D.V., Isaeva N.V., Solncev S.S. Perspektivnye vysokotemperaturnye keramicheskie kompozicionnye materialy [Perspective high-temperature ceramic composite materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 20–24.
  4. Kablov E.N., Kondrashov S.V., Jurkov G.Ju. Perspektivy ispol'zovanija uglerodsoderzhashhih nanochastic v svjazujushhih dlja polimernyh kompozicionnyh materialov [Perspectives of use of carbon-containing nanoparticles in binding for polymeric composite materials] //Rossijskie nanotehnologii. 2013. T. 8. №3–4. S. 24–42.
  5. Gunjaev G.M., Kablov E.N., Aleksashin V.M. Modificirovanie konstrukcionnyh ugleplastikov uglerodnymi nanochasticami [Modifying constructional ugleplastikov carbon nanoparticles] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 5–11.
  6. Kablov E.N., Shhetanov B.V., Grashhenkov D.V., Shavnev A.A., Njafkin A.N. Metallomatrichnye kompozicionnye materialy na osnove Al–SiC [Metalmatrix composite materials on the basis of Al–SiC] //Aviacionnye materialy i tehnologii. 2012. №S. S. 373–380.
  7. Varrik N.M., Ivahnenko Ju.A., Maksimov V.G. Oksid-oksidnye kompozicionnye materialy dlja gazoturbinnyh dvigatelej (obzor) [Oksid-oksidnye composite materials for gas turbine engines (review)] //Trudy VIAM. 2014. №8. St. 03 (viam.works.ru).
  8. Shhetanov B.V., Strjukov D.O., Kolyshev S.G., Murasheva V.V. Monokristallicheskie volokna oksida aljuminija: poluchenie, struktura, svojstva [Single-crystal fibers of aluminum oxide: receiving, structure, properties] //Vse materialy. Jenciklopedicheskij spravochnik. 2014. №4. S. 14–18.
  9. Kablov E.N., Svetlov I.L., Efimochkin I.Ju. Vysokotemperaturnye Nb–Si-kompozity [High-temperature Nb-Si-composites] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 164–173.
  10. Grashhenkov D.V., Shhetanov B.V., Efimochkin I.Ju. Razvitie poroshkovoj metallurgii zha-roprochnyh materialov [Development of powder metallurgy of heat resisting materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2011. №5. S. 13–26, №6. S. 10–22.
  11. Maksimov V.G., Basargin O.V., Shheglova T.M., Nikitina V.Ju. O projavlenii sverhplastich-nosti v polidispersnoj keramike mullit–oksid cirkonija s razmerom kristallov bolee 10 mkm [About superplasticity manifestation in unequigranular ceramics mullit-zirconium oxide with size of crystals more than 10 microns] //Trudy VIAM. 2013. №6. St. 04 (viam-works.ru).
  12. Basargin O.V., Shcheglova T.M., Kolyshev S.G., Nikitina V.Yu., Maksimov V.G., Babashov V.G. Determination of the high-temperature strength of ceramic oxide materials //Glass and Ceramics. 2013. V. 70. №1–2. P. 43–46.
  13. Maksimov V.G., Grashhenkov D.V., Lomovskoj V.A., Babashov V.G., Basargin O.V., Kolyshev S.G. Issledovanie vysokotemperaturnoj polzuchesti v polidispersnoj keramike mullit – oksid cirkonija [Research of high-temperature creep in unequigranular ceramics mullit – zirconium oxide] //Steklo i keramika. 2014. №5. S. 36–40.
  14. Ivahnenko Ju.A., Babashov V.G., Zimichev A.M., Tinjakova E.V. Vysokotemperaturnye teploizoljacionnye i teplozashhitnye materialy na osnove tugoplavkih soedinenij [High-temperature heatinsulating and heat-protective materials on the basis of high-melting connections] //Aviacionnye materialy i tehnologii. 2012. №S. S. 380–386.
  15. Tinjakova E.V., Grashhenkov D.V. Teploizoljacionnyj material na osnove mullito-korundovyh i kvarcevyh volokon [Heatinsulating material on the basis of mullito-korundovy and quartz fibers] //Aviacionnye materialy i tehnologii. 2012. №3. S. 43–46.
  16. Shhetanov B.V., Balinova Ju.A., Ljuljukina G.Ju., Solov'eva E.P. Struktura i svojstva nepre-ryvnyh polikristallicheskih volokon α-Al2O3 [Structure and properties of continuous polycrystalline fibers α-Al2O3] //Aviacionnye materialy i tehnologii. 2012. №1. S. 13–17.