Current state of investigations in the field of heat-resistant coatings for nickel and titanium alloys (review)

Denisova V.S., Solovyova G.A., Malinina G.A.
Denisova V.S., Solovyova G.A., Malinina G.A. Current state of investigations in the field of heat-resistant coatings for nickel and titanium alloys (review) // Proceedings of VIAM. 2015. No. 4. DOI: 10.18577/2307-6046-2015-0-4-2-2. URL: https://www.viam-works.ru/en/journal/2015/4/2
Abstract

Current development and research trends in the field of producing and investigating of long-life heat-resistant coatings for nickel and titanium alloys with working temperature up to 1000°C are considered. The results of investigations currently taken place and the ways of improving the properties of long-life enamel coatings are shown. The FSUE «VIAM» experience on the heat-resistant coatings development capable to provide long term effective operation of the nickel and titanium parts in high operational temperatures is considered.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period till 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N., Grashhenkov D.V., Isaeva N.V., Solncev S.S., Sevast'janov V.G. Perspektivnye vysokotemperaturnye keramicheskie kompozicionnye materialy [Perspective high-temperature ceramic composite materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 20–24.
  3. Ivahnenko Ju.A., Babashov V.G., Zimichev A.M., Tinjakova E.V. Vysokotemperaturnye teploizoljacionnye i teplozashhitnye materialy na osnove volokon tugoplavkih soedinenij [High-temperature heatinsulating and heat-protective materials on the basis of fibers of high-melting connections] //Aviacionnye materialy i tehnologii. 2012. №S. S. 380–385.
  4. Kablov E.N., Solncev S.S., Rozenenkova V.A., Mironova N.A. Sovremennye polifunkcional'nye vysokotemperaturnye pokrytija dlja nikelevyh splavov, uplotnitel'nyh metallicheskih voloknistyh materialov i berillievyh splavov [Modern multifunctional high temperature coatings for nickel alloys, sealing metal fibrous materials and beryllium alloys] //Novosti materialovedenija. Nauka i tehnika. 2013. №1 (materialsnews.ru).
  5. Solncev S.S. Vysokotemperaturnye steklokeramicheskie materialy i pokrytija – perspektivnoe napravlenie aviacionnogo materialovedenija [High-temperature steklokeramichesky materials and coverings – the perspective direction of aviation materials science] //Vse materialy. Jenciklopedicheskij spravochnik. 2009. №1. S. 26–37.
  6. Solncev S.S. Zashhitnye tehnologicheskie pokrytija i tugoplavkie jemali [Protective technological coverings and high-melting enamels]. M.: Mashino-stroenie. 1984. 256 s.
  7. Solncev S.S., Shvagireva V.V., Isaeva N.V., Solov'eva G.A. Armirovannye zharostojkie steklojemali dlja kamer sgoranija gazoturbinnyh dvigatelej [Reinforced heat resisting stekloemali for combustion tubes of gas turbine engines] //Aviacionnye materialy i tehnologii. 2010. №1. S. 26–29.
  8. Das S., Datta S., Basu D., Das G.C. Hot corrosion of glass coating on nickel base superalloy //Ceramics International. 2008. V. 34. P. 1215–1222.
  9. Minghui Chen, Mingli Shen, Shenglong Zhu, Fuhui Wang, Xiaolan Wang. Effect of sand blasting and glass matrix composite coating on oxidation resistance of a nickel-based superalloy at 1000°C //Corrosion Science. 2013. V. 73. P. 331–341.
  10. Das S., Mukhopadhyay A.K., Datta S., Basu D. Evaluation of microwave processed glass-ceramic coating on nimonic superalloy substrate //Ceramics International. 2010. V. 36. P. 1125–1130.
  11. Minghui Chen, Mingli Shen, Shenglong Zhu, Fuhui Wang. Comparative study of interfacial reaction between superalloy substrate and glass coating with and without alumina particles incorporation //Applied Surface Science. 2013. V. 271. P. 228–233.
  12. Xiaowei Niu, He Zhang, Xiaojun Hu, Wei Han. Synthesis of well-adhered SiO2–Al2O3 glass-ceramic coating on NiCrFe alloy supports //Applied Surface Science. 2013. V. 268. P. 265–269.
  13. Minghui Chen, Wenbo Li, Mingli Shen, Shenglong Zhu, Fuhui Wang. Glass-ceramic coating on titanium alloys for high temperature oxidation protection: Oxidation kinetics and microsctucture //Corrosion Science. 2013. V. 74. P. 178–186.
  14. Zinqi Xiao, Fatang Tan, Wei Wang, Fazhe Sun, Hongfei Lu, Xiaolin Qui, Jianguo Chen, Xueliang Qiao. Oxidation protection of Ti–6Al–4V alloy using a novel glass-amorphous silica composite coating //Ceramics International. 2014. V. 40. P. 3503–3509.
  15. Wenbo Li, Minghui Chen, Mingyu Wu, Shenglong Zhu, Cheng Wang, Fuhui Wang. Microstructure and oxidation behavior of a SiC–Al2O3–glass composite coating on Ti–47Al–2Cr–2Nb alloy //Corrosion Science. 2014. V. 87. P. 179–186.
  16. Wenbo Li, Minghui Chen, Cheng Wang, Shenglong Zhu, Fuhui Wang. Preparation and oxidation behavior of SiO2–Al2O3–glass composite coating on Ti–47Al–2Cr–2Nb alloy //Surface & Coatings Technology. 2013. V. 218. P. 30–38.
  17. Solncev S.St., Shvagireva V.V., Isaeva N.V., Solov'eva G.A. Zharostojkoe pokrytie dlja zashhity vysokoprochnyh slozhnolegirovannyh nikelevyh splavov ot vysokotemperatur-noj gazovoj korrozii [Heat resisting covering for protection of high-strength complex-alloyed nickel alloys against high-temperature gas corrosion] //Trudy VIAM. 2014. №6. St. 04 (viam-works.ru).
  18. Solncev St.S., Rozenenkova V.A., Mironova N.A., Solov'eva G.A. Vysokotemperaturnye pokrytija dlja voloknistyh substratov [High temperature coatings for fibrous substrates] //Trudy VIAM. 2013. №10. St. 03 (viam-works.ru).
  19. Solncev S.St., Shvagireva V.V., Isaeva N.V., Solov'eva G.A. Mnogocelevoe steklojemalevoe pokrytie dlja zashhity lityh fasonnyh detalej gazoturbinnyh dvigatelej [Multi-purpose stekloe-malevy covering for protection of cast shaped details of gas turbine engines] //Trudy VIAM. 2014. №3. St. 04 (viam-works.ru).
  20. Solncev St.S. Vysokotemperaturnye kompozicionnye materialy i pokrytija na osnove stekla i keramiki [High-temperature composite materials and coverings on the basis of glass and ceramics] /V sb. 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: Jubilejnyj nauch.-tehnich. sb. M.: VIAM. 2007. S. 90–99.
  21. Solncev St.S., Rozenenkova V.A., Mironova N.A. Vysokotemperaturnye steklokeramicheskie pokrytija i kompozicionnye materialy [High-temperature steklokeramichesky coverings and composite materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 359–368.