Application of the confocal laser imaging microscopy method for corrosive damages study
Iskhodzhanova I.V., Orlov M.R., Grigorenko V.B., Lapteva M.A. Application of the confocal laser imaging microscopy method for corrosive damages study // Proceedings of VIAM. 2015. No. 4. DOI: 10.18577/2307-6046-2015-0-4-11-11. URL: https://www.viam-works.ru/en/journal/2015/4/11
Abstract
On the investigations examples of aircraft gas turbine engines corrosive damages after 5 years exposure on the open experimental ground of the FSUE «VIAM» G.V. Akimov Gelendzhik climatic test center (VIAM GCTC) the possibilities of confocal laser imaging microscopy are represented. The 3D-models were built and quantitative assessment of surface topography by statistical data processing of the roughness using standard software was undertaken.
Reference list
- Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
- Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period till 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Kablov E.N. Korrozija ili zhizn' [Corrosion or life] //Nauka i zhizn'. 2012. №11. S. 16–21.
- Orlov M.R. Strategicheskie napravlenija razvitija Ispytatel'nogo centra FGUP «VIAM» [Strategic directions of development of the Test center VIAM Federal State Unitary Enterprise] //Aviacionnye materialy i tehnologii. 2012. №S. S. 387–393.
- Morozova L.V., Ishodzhanova I.V. Issledovanie zakonomernostej izmenenija rel'efa pover-hnosti obrazcov iz aljuminijlitievyh splavov metodom lazernoj mikroskopii [Research of patterns of change of relief of surface of samples from alyuminiylitiyevy alloys method of laser microscopy] //Trudy VIAM. 2014. №10. St. 08 (viam-works.ru).
- Fridljander I.N., Chuistov K.V., Berezina A.L., Kolobnev N.I., Koval' Ju.N. Aljuminij-litievye splavy. Struktura i svojstva [Aluminum - lithium alloys. Structure and properties]. K.: Naukova dumka. 1992.
- Antipov V.V., Kolobnev N.I., Hohlatova L.B. Razvitie aljuminijlitievyh splavov i mnogostupenchatyh rezhimov termicheskoj obrabotki [Development of alyuminiylitiyevy alloys and multistage modes of thermal processing] //Aviacionnye materialy i tehnologii. 2012. №S. S. 183–195.
- Orlov M.R. High-Temperature Corrosive Damage to Superalloys during Operation of Blades of Gas-Turbines and Power Plans //Polymer science. D. 2013. V. 6. №3. P. 250–255.
- Abraimov N.V., Orlov M.R., Shkretov Ju.P. Nekotorye aspekty vysokotemperaturnogo okis-lenija splava na osnove γʹ-Ni3Al [Some aspects of high-temperature oxidation of alloy on basis γʹ-Ni3Al] //Korrozija: materialy, zashhita. 2010. №8. S. 1–11.
- Orlov M.R., Ospennikova O.G., Gromov V.I. Zamedlennoe razrushenie stali 38HN3MA v processe dlitel'noj jekspluatacii [Steel 38ХН3МА delayed fracture in the course of long operation] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 5–12.
- Orlov M.R., Jakimova M.S. Zamedlennoe razrushenie monokristallicheskih lopatok iz zharo-prochnogo splava ZhS26-VI v processe jekspluatacii GTU [Delayed fracture of single-crystal blades from ZhS26-VI hot strength alloy in use GTU] //Gazoturbinnye tehnologii. 2011. №8. S. 10–15.
- Ishodzhanova I.V. Primenenie konfokal'noj lazernoj skanirujushhej mikroskopii dlja reshenija materialovedcheskih zadach [Application of konfokalny laser scanning microscopy for the solution of materialovedchesky tasks] /V sb. materialov VII Evrazijskoj nauch.-praktich. konf. «Prochnost' neodnorodnyh struktur». M.: MISiS. 2014. S. 138.
- Chabina E.B., Alekseev A.A., Filonova E.V., Lukina E.A. Primenenie metodov analiticheskoj mikroskopii i rentgenostrukturnogo analiza dlja issledovanija strukturno-fazovogo sostojanija materialov [Application of methods of analytical microscopy and the rentgenostrukturny analysis for research of structural and phase condition of materials] //Trudy VIAM. 2013. №5. St. 06 (viam-works.ru).
- Klevcov G.V., Merson E.D. O vozmozhnosti ispol'zovanija konfokal'nogo lazernogo skanirujushhego mikroskopa dlja issledovanija mikrorel'efa poverhnosti razrushenija metallicheskih materialov [About possibility of use of konfokalny laser scanning microscope for research of microrelief of surface of destruction of metal materials] //Fundamental'nye issledovanija. 2012. №11. S. 1185–1189.
- Hovis D.B., Heuer A.H. The use of laser scanning confocal microscopy (LSCM) in materials science //Journal of Microscopy. 2010. V. 240. №3. P. 173–180.
- Klark Je.R., Jeberhardt K.N. Mikroskopicheskie metody issledovanija materialov [Microscopic methods of research of materials]. M.: Tehnosfera. 2007. 376 s.
- Orlov M.R., Ospennikova O.G., Naprienko S.A., Morozova L.V. Issledovanie ustalostnogo razrushenija konicheskih shesteren reduktora central'nogo privoda gazoturbinnogo dvigatelja, izgotovlennyh iz stali 20H3MVF [Research of fatigue failure of conic gear wheels of reducer of the central drive of the gas turbine engine, made of steel 20Х3МВФ] //Deformacija i razrushenie materialov. 2014. №7. S. 18–26.
- Jevans Ju.R. Korrozija, passivnost' i zashhita metallov [Corrosion, passivity and protection of metals]. M.: Gosudarstvennoe nauch.-tehnich. izd-vo lit. po chernoj i cvetnoj metallurgii. 1941. 886 s.
- Orlov M.R., Ospennikova O.G., Karachevcev F.N. Obespechenie kachestva poverhnosti rabochih lopatok turbiny pri nanesenii zashhitnyh diffuzionnyh pokrytij [Providing surface quality of working turbine blades when drawing protective diffusion coatings] //Metallurg. 2013. №2. S. 77–84.
- Orlov M.R., Ospennikova O.G., Rassohina L.I. Podgotovka poverhnosti lopatok turbiny dlja nerazrushajushhego kontrolja metodom kapilljarnoj defektoskopii [Surface preparation of turbine blades for non-destructive testing by method of capillary defektoskopiya] //Zavodskaja laboratorija. Diagnostika materialov. 2013. №8. S. 52–60.
- Zhuk N.P. Kurs teorii korrozii i zashhity metallov [Course of the theory of corrosion and protection of metals]. M.: Metallurgija. 1976. 472 s.
- Shluger M.A., Azhogin F.F., Efimov E.A. Korrozija i zashhita metallov [Corrosion and protection of metals]. M.: Metallurgija. 1981. 216 s.
- Sokol I.Ja., Ul'janin E.A., Fel'dgandler Je.G. i dr. Struktura i korrozija metallov i splavov. Atlas [Structure and corrosion of metals and alloys. Atlas]: Sprav. izd. M.: Metallurgija. 1989. 400 s.
- Semenova I.V., Florianovich G.M., Horoshilov A.V. Korrozija i zashhita ot korrozii [Corrosion and corrosion protection]. M.: Fizmatlit. 2002. 336 s.
- Environmental and Industrial Corrosion – Practical and Theoretical Aspects /Ed. B.V. Salas, M. Schorr. In Tech. 2012. 168 p.
- Reformatskaja I.I., Rodionova I.G., Bejlin Ju.A. i dr. Rol' nemetallicheskih vkljuchenij i mikrostruktury v processe lokal'noj korrozii uglerodistyh i nizkolegirovannyh stalej [Role of non-metallic inclusions and microstructure in the course of local corrosion carbonaceous and low-alloy steels] //Zashhita metallov. 2004. T. 40. №5. S. 498–503.
- Filippov G.A., Rodionova I.G., Baklanova O.N. Korrozionnaja stojkost' stal'nyh trubo-provodov [Corrosion resistance of steel pipelines] //Tehnologija metallov. 2004. №2. S. 24–27.
- Rodionova I.G., Baklanova O.N., Filippov G.A. i dr. Rol' nemetallicheskih vkljuchenij v uskorenii processov lokal'noj korrozii neftepromyslovyh truboprovodov i drugih vidov metalloprodukcii i oborudovanija iz uglerodistyh i nizkolegirovannyh stalej [Role of non-metallic inclusions in acceleration of processes of local corrosion of oil-field pipelines and other types of steel products and the equipment from carbonaceous and low-alloy steels]. M.: Metallurgizdat. 2005. S. 7–14.
- Semenychev V.V. Korrozionnaja stojkost' listov splava D16ch.-T v morskih subtropikah [Corrosion resistance of sheets of alloy Д16ч.-T in sea subtropics] //Trudy VIAM. 2014. №7. St. 11 (viam-works.ru).