Features of prepregs intended for automated laying by ATL and AFP technologies

Gusev Y.A., Borshchev A.V., Khrulkov A.V.
Gusev Y.A., Borshchev A.V., Khrulkov A.V. Features of prepregs intended for automated laying by ATL and AFP technologies // Proceedings of VIAM. 2015. No. 3. DOI: 10.18577/2307-6046-2015-0-3-6-6. URL: https://www.viam-works.ru/en/journal/2015/3/6
Keywords
ATL, AFP
Abstract

Automated laying made by ATL and AFP methods is used worldwide to increase productivity and accuracy of prepregs laying in the course of manufacture of large-sized PCM-based parts. However, conventional prepregs are not always suitable for processing by these methods – they have to meet special requirements in terms of delivery form, quality and processability. Some features of prepregs intended for automated laying, requirements to them and an influence of laying parameters on their technological properties are discussed in the article.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kablov E.N. Jepoksidnoe svjazujushhee, prepreg na ego osnove i izdelie, vypolnennoe iz nego [Epoxy binder prepreg on its base and a product made therefrom] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  3. Kablov E.N. Himija v aviacionnom materialovedenii [Chemistry aviation materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  4. Kablov E.N., Shhetanov B.V., Ivahnenko Ju.A., Balinova Ju.A. Perspektivnye armirujushhie vysokotemperaturnye volokna dlja metallicheskih i keramicheskih kompozicionnyh materialov [Prospective reinforcing fibers for high temperature ceramic composites and metal materials] //Trudy VIAM. 2013. №2. St. 05 (viam-works.ru)
  5. Kobets L.P., Deev I.S. Carbon fibres: structure and mechanical properties //Composites science and technology. 1998. V. 57. №12. P. 1571–1580.
  6. Sloan J. ATL and AFP: defining the megatrends in composite aerostructures //High performance composites. July 2008. P. 20–25.
  7. Grimshaw M.N., Grant C.G., Diaz J.M.L. Advanced technology tape laying for affordable manufacturing of large composite structures /In: 46-th International SAMPE Symposium. 2001. P. 2484–2494.
  8. Dirk H., Lukaszewicz J.A., Ward C., Potter K.D. The engineering aspects of automated prepreg layup: History, present and future //Composites: Part B. 2012. V. 43. P. 997–1009.
  9. Grimshaw M.N. Automated tape laying //Composites. 2001. V. 21. P. 480–500.
  10. Banks R. Development of a new structural prepreg: characterisation of handling, drape and tack properties //Composite Structures. 2004. V. 66(1–4). P. 169–174.
  11. Lukaszewicz DH-JA, Weaver P.M., Potter K. The impact of processing conditions on the final part quality in automated tape deposition technologies /In: Sampe Seico. Paris. 2009. P. 45–70.
  12. Lukaszewicz DH-JA, Weaver P.M., Potter K. An empirical model for the automated deposition of thermoset composite /In: ACS – 24-th technical conference. Newark-Delaware. 2009. P. 22–76.
  13. Hrul'kov A.V., Dushin M.I., Popov Ju.O., Kogan D.I. Issledovanija i razrabotka avtoklavnyh i bezavtoklavnyh tehnologij formovanija PKM [Research and development autoclave and non-autoclave molding technology PCM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 292–301.
  14. Dushin M.I., Hrul'kov A.V., Muhametov P.P. Vybor tehnologicheskih parametrov avtoklavnogo formovanija detalej iz polimernyh kompozicionnyh materialov [The choice of process parameters autoclave molding parts from polymeric composite materials] //Aviacionnye materialy i tehnologii. 2011. №3. S. 20–26.
  15. Ahn K.J., Seferis J.C., Pelton T., Wilhelm M. Analysis and characterization of prepreg tack //Polym Compos. 1992. V. 13(3). P. 197–206.
  16. Seferis J.C., Meissonnier J. Development of a tack and drape test for prepregs based on viscoelastic principles //Sampe Quarterly-Soc Adv Mater Process Eng. 1989. V. 20(3). P. 55–64.
  17. Muhametov R.R., Merkulova Ju.I., Chursova L.V. Termoreaktivnye polimernye svjazujushhie s prognoziruemym urovnem reologicheskih i deformativnyh svojstv [Thermosetting polymeric binders with the projected level of rheology and deformation properties] //Klei. Germetiki. Tehnologii. 2012. №5. S. 19–24.
  18. Jepoksidnaja kompozicija [Epoxy composition]: pat. 2447104 Ros. Federacija; opubl. 05.10.2010.
  19. Crossley R.J., Schubel P.J., Warrior N.A. The experimental determination of prepreg tack and dynamic stiffness //Composites. Part A. 2012. V. 43. P. 423–434.
  20. Crossley R.J., Schubel P.J., Warrior N.A. The experimental characterisation and investigate on of prepreg tack /In: Proceedings of ICCM-18. Edinburgh. 2009. P. 1–11.
  21. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svjazujushhie dlja perspektivnyh metodov izgotovlenija konstrukcionnyh voloknistyh PKM [New polymeric binders for advanced manufacturing methods of structural fiber PCM] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  22. Babin A.N. Svjazujushhie dlja polimernyh kompozicionnyh materialov novogo pokolenija [Binders for polymeric composite materials of new generation] //Trudy VIAM. 2013. №4 (viam-works.ru).
  23. Muhametov R.R., Ahmadieva K.R., Kim M.A., Babin A.N. Rasplavnye svjazujushhie dlja perspektivnyh metodov izgotovlenija PKM novogo pokolenija [Melt binders promising methods of manufacture of a new generation of PCM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 260–265.