An influence of loading rate on mechanical properties of heat-resistant titanium alloys

Savushkin A.N., Kashapov O.S., Golinets S.A
Savushkin A.N., Kashapov O.S., Golinets S.A An influence of loading rate on mechanical properties of heat-resistant titanium alloys // Proceedings of VIAM. 2015. No. 3. DOI: 10.18577/2307-6046-2015-0-3-4-4. URL: https://www.viam-works.ru/en/journal/2015/3/4
Abstract

Mechanical properties of heat-resistant (α+β) titanium alloys and pseudo-α-titanium alloys VT18U, VT41, VT8, VT8M-1 were investigated depending on loading conditions. The tension test of specimens with different loading rates at 20°С and maximal working temperatures were made for each alloy with the use of TIRA-test 2300/1 testing machine. It was found out that sensibility of heat-resistant titanium alloys to the loading rate varies depending on the alloying level.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Tarasov Ju.M., Antipov V.V. Novye materialy VIAM – dlja perspektivnoj aviacionnoj tehniki proizvodstva OAO «OAK» [New materials VIAM - for promising aviation equipment produced by JSC «UAC»] //Aviacionnye materialy i tehnologii. 2012. №2. S. 5–6.
  3. Shmotin Ju.N., Starkov R.Ju., Danilov D.V., Ospennikova O.G., Lomberg B.S. Novye materialy dlja perspektivnogo dvigatelja OAO «NPO “Saturn”» [New materials for advanced engine JSC «NPO „Saturn”»] //Aviacionnye materialy i tehnologii. 2012. №2. S. 6–8.
  4. Kashapov O.S., Pavlova T.V., Nochovnaja N.A. Vlijanie rezhimov termicheskoj obrabotki na strukturu i svojstva zharoprochnogo titanovogo splava dlja lopatok KVD [Effect of heat treatment on the structure and properties of heat-resistant titanium alloy blades for HPC] //Aviacionnye materialy i tehnologii. 2010. №2. S. 8–14.
  5. Nochovnaja N.A., Panin P.V. Analiz ostatochnyh makronaprjazhenij v svarnyh soedinenijah titanovyh splavov raznyh klassov [Analysis of residual macroscopic stresses in welded joints of titanium alloys of different classes] //Trudy VIAM. 2014. №5. St. 02 (viam-works.ru).
  6. Erasov V.S., Jakovlev N.O., Nuzhnyj G.A. Kvalifikacionnye ispytanija i issledovanija prochnosti aviacionnyh materialov [Qualification testing and research strength of aircraft materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 440–448.
  7. Moiseev V.N. Vysokoprochnye titanovye splavy dlja aviakosmicheskoj tehniki [High-strength titanium alloys for aerospace engineering] /V sb. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2002. Jubilejnyj nauch.-tehnich. sb. /Pod obshh. red. E.N. Kablova. 2002. S. 115–121.
  8. Kablov E.N. Materialy dlja izdelija «Buran» – innovacionnye reshenija formirovanija shestogo tehnologicheskogo uklada [Materials for the product «Buran» – innovative solutions forming the sixth technological order] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
  9. Kashapov O.S., Novak A.V., Nochovnaja N.A., Pavlova T.V. Sostojanie, problemy i per-spektivy sozdanija zharoprochnyh titanovyh splavov dlja detalej GTD [Status, problems and prospects of creating heat-resistant titanium alloys for GTE parts] //Trudy VIAM. 2013. №3. St. 02 (viam-works.ru).
  10. Horev A.I., Belov S.P., Glazunov S.G. Metallovedenie titana i ego splavov [Physical metallurgy of titanium and its alloys]. M.: Metallurgija. 1992. 352 s.
  11. Sposob termicheskoj obrabotki vysokoprochnyh (α+β)-titanovyh splavov [A method of heat treatment of high (α+β) alloy titanic]: pat. 2465366 Ros. Federacija; opubl. 15.09.2011.
  12. Sposob termomehanicheskoj obrabotki izdelij iz titanovyh splavov [Method of thermome-chanical processing of titanium alloys]: pat. 2457273 Ros. Federacija; opubl. 05.04.2011.
  13. Gorynin I.V., Kudrjavcev A.S., Ushkov S.S. i dr. Opyt izgotovlenija slitkov massoj do 17 tonn iz psevdo-al'fa splavov [Experience of producing ingots weighing up to 17 tons of pseudo-alpha alloys] //Titan. 2013. №2. S. 23–28.
  14. Gorynin I.V., Ushkov S.S., Baranov A.V., Mihajlov V.I., Ushakov B.G. Titanovye splavy dlja konstrukcij morskogo primenenija [Titanium alloys for marine applications designs] //Morskie intellektual'nye tehnologii. 2009. №4. S. 61–66.
  15. Ilyin A., Kolachev B., Volodin V., Ryndenkov D. About the purposefulness of comprasion of titanium alloys in terms of aluminium and Molybdenium equivalents /In: Titanium–99. Science and technology. 1999. P. 53–60.