An effect of iron content on mechanical properties of bars made of heat-resistant titanium alloy VT41

Kashapov O.S., Pavlova T.V., Istrakova A.R., Kalashnikov V.S.
Kashapov O.S., Pavlova T.V., Istrakova A.R., Kalashnikov V.S. An effect of iron content on mechanical properties of bars made of heat-resistant titanium alloy VT41 // Proceedings of VIAM. 2015. No. 3. DOI: 10.18577/2307-6046-2015-0-3-2-2. URL: https://www.viam-works.ru/en/journal/2015/3/2
Abstract

The paper describes the studies focused on structure and mechanical properties of bars made from heat-resistant near-α-titanium alloy VТ41 with different iron contents. It was established that an increase in Fe content leads to modification of microstructure, an increase in strength and fatigue characteristics of the material and to a decrease in ductility characteristics, fracture toughness and heat resistance. In addition, rising of Fe content is accompanied by an increase of sensitivity to stress concentrators at different types of tests.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N. Materialy dlja izdelija «Buran» – innovacionnye reshenija formirovanija shestogo tehnologicheskogo uklada [Materials for the product «Buran» – innovative solutions forming the sixth technological order] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
  3. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemel'nye jelementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements - materials of current and future high-tech] //Trudy VIAM. 2013. №2. St. 01 (viam-works.ru).
  4. Kashapov O.S., Novak A.V., Nochovnaja N.A., Pavlova T.V. Sostojanie, problemy i perspektivy sozdanija zharoprochnyh titanovyh splavov dlja detalej GTD [Status, problems and prospects of creating heat-resistant titanium alloys for GTE parts] //Trudy VIAM. 2013. №3. St. 02 (viam-works.ru).
  5. Erasov V.S., Jakovlev N.O., Nuzhnyj G.A. Kvalifikacionnye ispytanija i issledovanija prochnosti aviacionnyh materialov [Qualification testing and research strength of aircraft materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 440–448.
  6. Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] //Nauka i zhizn'. 2010. №4. S. 2–7.
  7. Titanium-base alloy: патент EP 87 30 5197, опубл. 01.06.1988. Applicant Inventor Bania Paul J. – Timet, Europe, USA.
  8. Russo P.A., Yu K.O. Effect of Ni, Fe and primary alpha on the creep of alpha-beta processed and annealed Ti–6Al–2Sn–4Zr–2Mo–0,09Si /In: Titanium-99. Science and technology. 1999. P. 596–603.
  9. Russo P.A., Yu K.O. Effect of Ni, Fe and Si on the creep of Ti–6Al–2Sn–4Zr–6Mo /In: Titanium-99. Science and technology. 1999. P. 713–720.
  10. Ivanova L.A., Kudrjavcev A.S., Chudakov E.V., Lysenko L.V., Travin V.V. Optimizacija kompleksa sluzhebnyh svojstv titanovyh splavov marok 5V i 37 dlja uzlov i detalej jenergeticheskogo oborudovanija [Optimization of complex service properties of titanium alloys brands 5V and 37 units and parts of the power equipment] //Titan. 2010. №4. S. 23–30.
  11. Travin V.V., Ivanova L.A., Kudrjavcev A.S., Kozlova I.R. Polzuchest' psevdo-al'fa-titanovyh splavov i ee vlijanie na naprjazhenno-deformirovannoe sostojanie detalej parovyh turbin [Creep pseudo-alpha titanium alloys and its influence on the stress-strain state of parts of steam turbines] //Titan. 2013. №2. S. 4–12.
  12. Kashapov O.S., Pavlova T.V., Nochovnaja N.A. Vlijanie rezhimov termicheskoj obrabotki na strukturu i svojstva zharoprochnogo titanovogo splava dlja lopatok KVD [Effect of heat treatment on the structure and properties of heat-resistant titanium alloy blades for HPC] //Aviacionnye materialy i tehnologii. 2010. №2. S. 8–14.
  13. Sposob termicheskoj obrabotki vysokoprochnyh (α+β)-titanovyh splavov [A method of heat treatment of high (α + β) alloy titanic]: pat. 2465366 Ros. Federacija; opubl. 15.09.2011.
  14. Sposob termomehanicheskoj obrabotki izdelij iz titanovyh splavov [Method of thermomechanical processing of titanium alloys]: pat. 2457273 Ros. Federacija; opubl. 05.04.2011.
  15. Horev A.I., Belov S.P., Glazunov S.G. Metallovedenie titana i ego splavov [Physical metallurgy of titanium and its alloys]. M.: Metallurgija. 1992. 352 s.
  16. Horev A.I. Perspektivnye napravlenija povyshenija konstrukcionnoj prochnosti titanovyh splavov [Promising ways to improve the structural strength of titanium alloys] //Tehnologija legkih splavov. 2007. №2. S. 144–153.
  17. Horev A.I. Razrabotka konstrukcionnyh titanovyh splavov dlja izgotovlenija detalej i uzlov aviakosmicheskoj tehniki [Development of structural titanium alloys for the manufacture of parts and components of aerospace engineering] //Svarochnoe proizvodstvo. 2009. №3. S. 13–23.