Research of an influence of temperature factors on aging of new polymer composite materials for aviation engine nacelle

Nikolaev E.V., Koren’kova T.G., Shvedkova A.K., Valevin E.O.
Nikolaev E.V., Koren’kova T.G., Shvedkova A.K., Valevin E.O. Research of an influence of temperature factors on aging of new polymer composite materials for aviation engine nacelle // Proceedings of VIAM. 2015. No. 3. DOI: 10.18577/2307-6046-2015-0-3-12-12. URL: https://www.viam-works.ru/en/journal/2015/3/12
Abstract

The choice and substantiation of conditions of thermal aging of polymer composite materials intended for aviation components were described in the paper. Researches of changes in PCM strength at compression, interlayer shift and bending, and in glass-transition area and temperature were conducted at various test temperatures both in an initial state and after an impact of thermal aging. Conditions of thermal aging of materials and a strength characteristic most sensitive to temperature influence, i.e. strength at interlayer shift were defined by the results of research of a «strength/test temperatures» dependence and glass-transition area and temperature. Strength of polymer composite materials at interlayer shift was defined depending on temperature and exposition duration within the chosen conditions of thermal aging. An influence of some assumed operation temperatures and considerably higher temperatures was defined. An influence of temperature depending on the exposition duration w

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N., Gunjaev G.M. Tumanov A.T. – iniciator sozdanija kompozitov [Tumanov A.T. – Initiator of the composites] /V sb. tezisov dokl. Mezhotraslevoj nauch.-tehnich. konf. «Kompozicionnye materialy v aviakosmicheskom materialovedenii». M.: VIAM. 2009. S. 6–9.
  3. Kablov E.N., Starcev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznachenija. III. Znachimye faktory starenija [Climatic aging of composite materials aviation applications. III. Significant factors of aging] //Deformacija i razrushenie materialov. 2011. №1. S. 34–40.
  4. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svjazujushhie dlja perspektivnyh metodov izgotovlenija konstrukcionnyh voloknistyh PKM [New polymeric binders for advanced manufacturing methods of structural fiber PCM] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  5. Kirillov V.N., Vapirov Ju.M., Drozd E.A. Issledovanie atmosfernoj stojkosti polimernyh kompozicionnyh materialov v uslovijah atmosfery teplogo vlazhnogo i umerenno teplogo klimata [The study of atmospheric resistance of polymer composite materials in the atmosphere warm, moist and moderately warm climate] //Aviacionnye materialy i tehnologii. 2012. №4. S. 31–38.
  6. Mishra G., Mohapatra S.R., Behera P.R., Dash B., Mohanty U.K., Ray B.C. (National Institute Technology, Rourkela, India) Aircraft Eng. and Aerosp. technol. 2010. V. 82. №4. P. 258–266.
  7. Firefighting and emergency responsestudy of advanced composites aircraft. Objective 2: Fire-fighting Effectiveness of Technologies and Agents on Composite Aircraft Fires. Distribution A: Approved for public release; distribution unlimited. 88ABW-2012-0190, 10 January 2012.
  8. Espec Technology Report. 2007. №25.
  9. Kablov E.N., Starcev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznachenija. I. Mehanizmy starenija [Climatic aging of composite materials aviation applications. I. Mechanisms of aging] //Deformacija i razrushenie materialov. 2010. №11. S. 19–27.
  10. Kirillov V.N., Starcev O.V., Efimov V.A. Klimaticheskaja stojkost' i povrezhdaemost' polimernyh kompozicionnyh materialov, problemy i puti reshenija [Weather resistance and defectiveness of polymer composite materials, problems and solutions] //Aviacionnye materialy i tehnologii. 2012. №S. S. 412–423.
  11. Nikolaev E.V., Kirillov V.N., Skirta A.A., Grashhenkov D.V. Issledovanie zakonomernostej vlagoperenosa i razrabotka standarta po opredeleniju kojefficienta diffuzii i predel'nogo vlagosoderzhanija dlja ocenki mehanicheskih svojstv ugleplastikov [Study patterns of moisture transfer and development of a standard to determine the diffusion coefficient and limit the moisture content to assess the mechanical properties of carbon fiber reinforced plastics] //Aviacionnye materialy i tehnologii. 2013. №3. S. 44–48.
  12. Efimov V.A., Shvedkova A.K., Koren'kova T.G., Kirillov V.N. Issledovanie polimernyh konstrukcionnyh materialov pri vozdejstvii klimaticheskih faktorov i nagruzok v laboratornyh i naturnyh uslovijah [The study of polymeric structural materials under the influence of climatic factors and stress in laboratory and field conditions] //Trudy VIAM. 2013. №1. St. 05 (viam-works.ru).
  13. Skryljov N.S., Vol'nyj O.S., Postnov V.I., Barbot'ko S.L. Issledovanie vlijanija teplovyh faktorov klimata na izmenenie harakteristik pozharobezopasnosti polimernyh kompozicionnyh materialov [Investigation of the influence thermal factors of climate change on fire safety characteristics of polymer composite materials] //Trudy VIAM. 2013. №9. St. 05 (viam-works.ru).
  14. Kirillov V.N., Efimov V.A. Problemy issledovanija klimaticheskoj stojkosti aviacionnyh nemetallicheskih materialov [Problems of research aircraft climatic resistance of nonmetallic materials] /V kn. 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007. M.: VIAM. 2007. S. 379–388.
  15. Grigor'ev M.M., Kogan D.I., Tverdaja O.N., Panina N.N. Osobennosti izgotovlenija PKM metodom RFI [Peculiarities of RMB by RFI] //Trudy VIAM. 2013. №4. St. 03 (viam-works.ru).
  16. Jenciklopedija polimerov [Encyclopedia of polymer]. M.: Sovetskaja jenciklopedija. 1977. T. 3. S. 491–492.
  17. Menson Dzh., Sperling L. Polimernye smesi i kompozity [Polymer blends and composites]. M.: Himija. 1979. S. 200–202.
  18. Simonov-Emel'janov I.D., Kuleznev V.N. Principy sozdanija kompozicionnyh materialov [Principles of creation of composite materials]. M.: MIHM. 1989. 85 s.
  19. Jenciklopedija polimerov. M.: Sovetskaja jenciklopedija [Encyclopedia of polymer]. 1971. T. 2. S. 627–633.
  20. Kablov E.N., Starcev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznachenija. II. Relaksacija ishodnoj strukturnoj neravnovesnosti i gradient svojstv po tolshhine [Climatic aging of composite materials aviation applications. II. Relaxation of the original structural and non-equilibrium properties of gradient across the thickness] //Deformacija i razrushenie materialov. 2012. №6. S. 17–19.