Disadvantages of waveguide techniques for measurement of radar-absorbing material characteristics
Romanov A.M., Beljaev А.А., Bespalova E.E. Disadvantages of waveguide techniques for measurement of radar-absorbing material characteristics // Proceedings of VIAM. 2015. No. 3. DOI: 10.18577/2307-6046-2015-0-3-11-11. URL: https://www.viam-works.ru/en/journal/2015/3/11
Abstract
It was shown in the paper that the measurement results of reflection ratios of radar-absorbing materials performed in the waveguide for each frequency corresponded to the results of measurements at a certain angle of incidence in case of polarization of the electric vector perpendicular to the plane of incidence; thus, they do not correspond to the measurements at normal incidence. Material permittivity measurement errors caused by a gap between a specimen and waveguide wall were estimated. A simplified expression for estimation of the relative error of permittivity measurements and some examples of errors calculation for the above two cases are given in the paper.
Reference list
- Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih perera-botki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Kablov E.N. Himija v aviacionnom materialovedenii [Chemistry aviation materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
- Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
- Beljaev A.A., Kondrashov S.V., Lepeshkin V.V., Romanov A.M. Radiopogloshhajushhie materialy [Radio-absorbing materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 348–352.
- Beljaev A.A., Bespalova E.E., Romanov A.M. Pozharobezopasnye radiopogloshhajushhie materialy dlja bezjehovyh kamer [Fireproof materials for radio-anechoic chambers] //Aviacionnye materialy i tehnologii. 2013. №1. S. 53–55.
- Agafonova A.S., Beljaev A.A., Kondrashov Je.K., Romanov A.M. Osobennosti formirovanija monolitnyh konstrukcionnyh radiopogloshhajushhih materialov na osnove kompozitov, napolnennyh rezistivnym voloknom [Features of formation of monolithic structural radar absorbing materials based composites filled with resistive fiber] //Aviacionnye materialy i tehnologii. 2013. №3. S. 56–59.
- Brandt L.A. Issledovanija dijelektrikov na sverhvysokih chastotah [Studies dielectrics at microwave frequencies]. M.: Gos. izd-vo fiz.-mat. lit. 1963. S. 191–201.
- Shirokov V.V., Romanov A.M. Issledovanie dijelektricheskih harakteristik steklosotoplasta volnovodnym metodom [Study of the dielectric characteristics of the waveguide method steklosotoplasta] //Aviacionnye materialy i tehnologii. 2013. №4. S. 62–68.
- Beljaev A.A., Shirokov V.V., Romanov A.M. Issledovanie dijelektricheskih harakteristik monolitnyh stekloplastikov radiotehnicheskogo naznachenija [The study of dielectric properties of monolithic fiberglass radio engineering] //Kompozitnyj mir. 2014 (v pechati).
- Bespalova E.E., Beljaev A.A., Romanov A.M., Shirokov V.V. Issledovanie dijelektricheskih harakteristik sloev mnogoslojnogo radiopogloshhajushhego materiala dlja bezjehovyh kamer na osnove vspenennogo asbesta, napolnennogo nauglerozhennym voloknom [Study of the dielectric characteristics of radar absorbing layers of the multilayer material for anechoic chambers on the basis of foam asbestos filled with carbonized fiber] //Trudy VIAM. 2014. №8. St. 12 (viam-works.ru).
- Lushina M.V., Parshin S.G., Rzhevskij A.A. Sovremennye jekranirujushhie i radiopogloshhajushhie materialy [Modern shielding and radio absorbing materials] //Sistemy upravlenija i obrabotka informacii. 2011. №22.S. 208–214, 223.
- Nikol'skij V.V., Nikol'skaja T.I. Jelektrodinamika i rasprostranenie radiovoln [Electrodynamics and Propagation]. M.: URSS. 2012. S. 44, 163–164.
- Bibikov S.B., Titov A.N., Cherepanov A.K. Sintez materiala s zadannym kojefficientom otrazhenija v shirokom diapazone chastot i uglov padenija [Synthesis of a material with a specified reflectivity in a wide range of frequencies and angles of incidence] /V sb. dokl. XV Mezhdunarodnoj nauch.-tehnich. konf. «Radiolokacija. Navigacija. Svjaz'». Voronezh. 2009. S. 1578–1584.
- Korn G.A., Korn T.M. Spusk s vychisleniem koordinat gradient [Descent from the calculation of the coordinates of the gradient]: Spravochnik po matematike. M.: Nauka. 1984. 660 s.
- Rosenbrock H.H. An automatic method for finding the greatest or least value of a function //The Computer Journal. 1960. V. 3. Р. 175–184.
- Brehovskih A.M. Volny v sloistyh sredah [Waves in layered media]. M.: Nauka. 1957. S. 52–56.
- Odelevskij V.I. Raschet obobshhennoj provodimosti geterogennyh struktur. 1-matrichnye dvuhfaznye sistemy s nevytjanutymi vkljuchenijami [Calculation of generalized conductivity heterogeneous structures. 1-matrix two-phase system with unstretched inclusions] //ZhTF. 1951. T. XXI. №5. S. 668–676.
- Fal'kovskij O.I. Tehnicheskaja jelektrodinamika [Technical electrodynamics]. SPb.: Lan'. 2009. 244 s.
- Kolosov Ju.A., Levkov F.E. Tochnostnye harakteristiki volnovodnogo metoda opredelenija jelektricheskih parametrov dijelektrikov [Performance characteristics of the waveguide method for determining the parameters of electrical insulators] //Voprosy radiojelektroniki. Ser. Obshhie voprosy radiojelektroniki. 1985. №12. S. 18–33.
- Kolosov Ju.A., Levkov F.E. O volnovodnom metode opredelenija jelektricheskih parametrov dijelektrikov [About waveguide method for determining the electrical parameters of dielectrics] //Voprosy radiojelektroniki. Ser. Obshhie voprosy radiojelektroniki. 1986. №1. S. 41–45.