Improvement of casting technology and composition of single crystal blades made of heat-resistant intermetallic alloy

Gerasimov V. V., Petrushin N.V., Visik E.M.
Gerasimov V. V., Petrushin N.V., Visik E.M. Improvement of casting technology and composition of single crystal blades made of heat-resistant intermetallic alloy // Proceedings of VIAM. 2015. No. 3. DOI: 10.18577/2307-6046-2015-0-3-1-1. URL: https://www.viam-works.ru/en/journal/2015/3/1
Abstract

CAD was used to improve chemical composition of single crystal intermetallic Ni-based superalloy with crystallographic orientation (CGO) providing an attractive combination of operation properties: density – 8,0 g/cm3; long-term strength \( \sigma^{1100}_{100} = 130~\text{MPa} \) at 1100°C and \( \sigma^{1200}_{100} = 53~\text{MPa} \) at 1200°C and σ-1 \( \sigma^{900} = 370~\text{MPa} \) at 900°C on the base of \( 2 \cdot 10^{7} \) cycles. The process parameters for casting of uncooled single crystal small-sized rotor blades of GTE with CGO from the above alloy were developed. Experimental lots of uncooled small-sized rotor blades were produced with the single crystal structure yield at least 95% under conditions of pilot production at VIAM and 80% - under industrial conditions.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih perera-botki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7−17.
  2. Buntushkin V.P., Bazyleva O.A. Litejnye zharoprochnye splavy na osnove intermetallida nikelja i ih primenenie dlja vysokotemperaturnyh detalej GTD [Casting superalloys based intermetallic nickel and their application to high-GTE parts] /V sb.: Aviacionnye materialy i tehnologii. Vyp. «Vysokozharoprochnye materialy dlja sovremennyh i perspektivnyh gazoturbinnyh dvigatelej i progressivnye tehnologii ih proizvodstva». M.: VIAM. 2003. S. 18–24.
  3. Gerasimov V.V., Visik E.M. Tehnologicheskie aspekty lit'ja detalej gorjachego trakta GTD iz intermetallidnyh nikelevyh splavov tipa VKNA s monokristallicheskoj strukturoj [Technological aspects of the casting of turbine engine hot section of the intermetallic nickel alloys such VKNA with single-crystal structure] //Litejshhik Rossii. 2012. №2.
  4. S. 19–23.
  5. Gerasimov V.V., Visik E.M., Nikitin V.A., Zernova M.G. Opyt osvoenija tehnologii lit'ja sektorov soplovyh lopatok s monokristallicheskoj strukturoj iz splava VKNA-4U [Experience in development of casting technology sectors nozzle blades with single-crystal structure of the alloy VKNA-4U] //Aviacionnye materialy i tehnologii. 2012. №4.
  6. S. 13−18.
  7. Bondarenko Ju.A., Kablov E.N. Napravlennaja kristallizacija zharoprochnyh splavov s povyshennym temperaturnym gradientom [Directional solidification of superalloys with a high temperature gradient] //MiTOM. 2002. №7. S. 20–23.
  8. Kablov E.N., Gerasimov V.V., Visik E.M. Tehnologicheskie osobennosti poluchenija monokristallicheskih obrazcov i turbinnyh lopatok iz vysokorenievyh zharoprochnyh splavov na ustanovkah UVNK-9 i VIAM-1790 [Technological features of obtaining single-crystal turbine blades and vysokorenievyh of superalloys installations UVNK-9 and VIAM-1790] /V sb.: Litejnye zharoprochnye splavy. Jeffekt S.T. Kishkina. M.: Nauka. 2006. S. 185−183.
  9. Kablov E.N., Tolorajja V.N. VIAM – osnovopolozhnik otechestvennoj tehnologii lit'ja monokristallicheskih turbinnyh lopatok GTD i GTU [VIAM - founder of the national casting technology of single-crystal turbine blades and turbine engine GTU] //Aviacionnye materialy i tehnologii. 2012. №S. S. 105−117.
  10. Bazyleva O.A., Arginbaeva Je.G., Turenko E.Ju. Zharoprochnye litejnye intermetallidnye splavy [Heat-resistant casting intermetallic alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 57–60.
  11. Kablov E.N., Buntushkin V.P., Bazyleva O.A., Gerasimov V.V., Timofeeva O.B. Zharoprochnye splavy na osnove intermetallida Ni3Al [Heat-resistant alloys based on the intermetallic compound Ni3Al] /V sb. trudov Mezhdunarodnoj nauch.-tehnich. konf. «Nauchnye idei S.T. Kishkina i sovremennoe materialovedenie». M.: VIAM. 2006.
  12. S. 71–75.
  13. Kablov E.N., Buntushkin V.P., Bazyleva O.A. Konstrukcionnye zharoprochnye materialy na osnove soedinenija Ni3Al dlja detalej gorjachego trakta GTD [Structural refractory materials based compound Ni3Al for hot section components GTD] //Tehnologija legkih splavov. 2007. №2. S. 75−80.
  14. Kablov E.N., Gerasimov V.V., Visik E.M., Demonis I.M. Rol' napravlennoj kristalli-zacii v resursosberegajushhej tehnologii proizvodstva detalej GTD [The role of directional solidification in the resource-saving technology of production of gas-turbine] //Trudy VIAM. 2013. №3. St. 01 (viam-works.ru).
  15. Kablov E.N., Svetlov I.L., Petrushin N.V. Nikelevye zharoprochnye splavy dlja lit'ja lopatok s napravlennoj i monokristallicheskoj strukturoj (Chast' I) [Nickel superalloys for casting blades with directional and single-crystal structure] //Materialovedenie. 1997. №4. S. 32–39.
  16. Kablov E.N., Svetlov I.L., Petrushin N.V. Nikelevye zharoprochnye splavy dlja lit'ja lopatok s napravlennoj i monokristallicheskoj strukturoj (Chast' II) [Nickel superalloys for casting blades with directional and single-crystal structure] //Materialovedenie. 1997. №5. S. 14–16.
  17. Kablov E.N., Petrushin N.V. Komp'juternyj metod konstruirovanija litejnyh zharoprochnyh nikelevyh splavov [Computer method for the construction of the casting heat-resistant nickel alloys] /V sb.: Litejnye zharoprochnye splavy. Jeffekt S.T. Kishkina. M.: Nauka. 2006. S. 56−78.
  18. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharo-prochnye splavy novogo pokolenija [Casting nickel superalloys new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 36–52.
  19. Petrushin N.V., Chabina E.B., Nazarkin R.M. Konstruirovanie zharoprochnyh intermetallidnyh splavov na osnove γ′-fazy s vysokoj temperaturoj plavlenija. Chast' 2. [Construction of refractory alloys based intermetallic γ'-phase with a high melting point.] //MiTOM. 2012. №3 (681). S. 20–23.
  20. Morozova G.I. Kompensacija disbalansa legirovanija zharoprochnyh nikelevyh splavov [Imbalance compensation doping of heat-resistant nickel alloys] //MiTOM. 2012. №12 (690). S. 52−56.
  21. Zhang J.S., Hu Z.Q., Murata Y., Morinaga M., Yukawa N. Design and development of hot corrosion-resistant nickel-base single-crystal superalloys by the d-electrons alloy design theory: Part II. Characterization of the phase stability //Metallurgical Transaction A. 1993. V. 24. P. 2443−2450.
  22. Gerasimov V.V., Visik E.M., Koljadov E.V. Vzaimosvjaz' formy fronta kristallizacii so strukturoj zharoprochnyh splavov v processe napravlennoj kristallizacii [The relationship forms the crystallization front with the structure of high-temperature alloys during directional solidification] //Trudy VIAM. 2014. №6. St. 02 (viam-works.ru).