Application of natural fibers for manufacturing of polymer composite materials

Donetskiy K.I., Khrulkov A.V.
Donetskiy K.I., Khrulkov A.V. Application of natural fibers for manufacturing of polymer composite materials // Proceedings of VIAM. 2015. No. 2. DOI: 10.18577/2307-6046-2015-0-2-9-9. URL: https://www.viam-works.ru/en/journal/2015/2/9
Abstract

Currently, the use of natural fibers in production of up-to-date polymer composite materials (PCM) becomes much more important. Replacement of conventional glass and carbon fillers with natural ones reduces both production cost and the effect of polymer composite materials production on the environment. Furthermore, application of natural fibers for manufacturing of polymer composite materials boosts development of agricultural industries traditional for Russia.

Reference list
  1. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  2. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  3. Kablov E.N. Himija v aviacionnom materialovedenii [Chemistry aviation materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  4. Gunjaev G.M., Krivonos V.V., Rumjancev A.F., Zhelezina G.F. Polimernye kompozicionnye materialy v konstrukcijah letatel'nyh apparatov [Polymer composite materials in aircraft structure] //Konversija v mashinostroenii. 2004. №4 (65). S. 65–69.
  5. Kablov E.N. Materialy i himicheskie tehnologii dlja aviacionnoj tehniki [Materials and chemical technologies, aircraft] //Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  6. Doneckij K.I., Hrul'kov A.V., Kogan D.I., Belinis P.G., Luk'janenko Ju.V. Primenenie ob#emno-armirujushhih preform pri izgotovlenii izdelij iz PKM [Use volumetric reinforcing preforms in the manufacture of FRP articles] //Aviacionnye materialy i tehnologii. 2013. №1. S. 35–39.
  7. Grigor'ev M.M., Kogan D.I., Tverdaja O.N., Panina N.N. Osobennosti izgotovlenija PKM metodom RFI [Peculiarities of RMB by RFI] //Trudy VIAM. 2013. №4. St. 03 (viam-works.ru).
  8. Doneckij K.I., Kogan D.I., Hrul'kov A.V. Ispol'zovanie tehnologij pletenija pri proizvodstve jelementov konstrukcij iz PCM [use of technology in the production of weaving elements of PCM constructions] //Trudy VIAM. 2013. №10. St. 04 (viam-works.ru).
  9. Dushin M.I., Hrul'kov A.V., Raskutin A.E. K voprosu udalenija izlishkov svjazujushhego pri avtoklavnom formovanii izdelij iz polimernyh kompozicionnyh materialov [On the question of the removal of excess binder in autoclave molding products from polymeric composite materials] //Trudy VIAM. 2013. №1. St. 03 (viam-works.ru).
  10. Dushin M.I., Kogan D.I., Hrul'kov A.V., Gusev Ju.A. Prichiny obrazovanija poristosti v izdelijah iz polimernyh kompozicionnyh materialov [Causes of porosity in products from polymeric composite materials] //Kompozity i nanostruktury. 2013. №3 (19). S. 60–71.
  11. Dushin M.I., Chursova L.V., Hrul'kov A.V., Kogan D.I. Osobennosti izgotovlenija polimernyh kompozicionnyh materialov metodom vakuumnoj infuzii [Features of the production of polymeric composite materials by vacuum infusion] //Voprosy materialovedenija. 2013. №3 (75). S. 33–40.
  12. Hrul'kov A.V., Dushin M.I., Popov Ju.O., Kogan D.I. Issledovanija i razrabotka avtoklavnyh i bezavtoklavnyh tehnologij formovanija PCM [Research and development autoclave and non-autoclave molding technology PCM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 292–301.
  13. Timoshkov P.N., Kogan D.I. Sovremennye tehnologii proizvodstva polimernyh kompozicionnyh materialov novogo pokolenija [Modern production technology of polymer composite materials of new generation] //Trudy VIAM. 2013. №4 (viam-works.ru).
  14. Kobets L.P., Deev I.S. Carbon fibres: structure and mechanical properties //Composites Science and Technology. 1998. Т. 57. №12. С. 1571–1580.
  15. Kablov E.N., Shhetanov B.V., Ivahnenko Ju.A., Balinova Ju.A. Perspektivnye armirujushhie vysokotemperaturnye volokna dlja metallicheskih i keramicheskih kompozicionnyh materialov [Prospective reinforcing fibers for high temperature ceramic composites and metal materials] //Trudy VIAM. 2013. №2. St. 05 (viam-works.ru).
  16. Kirillov V.N., Starcev O.V., Efimov V.A. Klimaticheskaja stojkost' i povrezhdaemost' polimernyh kompozicionnyh materialov, problemy i puti reshenija [Weather resistance and defectiveness of polymer composite materials, problems and solutions] //Aviacionnye materialy i tehnologii. 2012. №S. S. 412–423.
  17. Kogan D.I., Chursova L.V., Petrova A.P. Tehnologija izgotovlenija PKM sposobom propitki plenochnym svjazujushhim [Manufacturing technology RMB impregnation method bonding film] //Klei. Germetiki. Tehnologii. 2011. №6. S. 25–29.
  18. Muhametov R.R., Ahmadieva K.R., Kim M.A., Babin A.N. Rasplavnye svjazujushhie dlja perspektivnyh metodov izgotovlenija PCM novogo pokolenija [Melt binders promising methods of manufacture of a new generation of PCM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 260–265.
  19. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svjazujushhie dlja perspektivnyh metodov izgotovlenija konstrukcionnyh voloknistyh PCM [New polymeric binders for advanced manufacturing methods of structural fiber PCM] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  20. Kiselev M.V. Modelirovanie stroenija l'njanogo chesanogo volokna i processa droblenija l'njanyh kompleksov: monografija [Modeling the structure combed flax fiber and flax complexes crushing process: a monograph]. Kostroma: Izd-vo KGTU. 2009. 110 s.
  21. Bos H. The potential of flax fibres as reinforcement for composite materials /In: Technische Universiteit Eindhoven. Eindhoven: 2004. P. 192.
  22. Ugrjumov S.A. Sovershenstvovanie tehnologii proizvodstva kompozicionnyh materialov na osnove drevesnyh napolnitelej i kostry l'na [Improving the technology of composite materials based on wood fillers and fires flax]: Avtoref. dis. d.t.n. M. 2009. 39 s.
  23. Zhivetin V.V., Ginzburg L.N. Maslichnyj len i ego kompleksnoe razvitie [Oilseed flax and its complex development]. M.: CNIILKA. 2000. 92 s.