Stress relaxation as a method for estimation of the network structure parameters of cross-linked polyethylene

Kachalina A.L., Melnikov D.A., Kurnosov A.O., Sokolov I.I.
Kachalina A.L., Melnikov D.A., Kurnosov A.O., Sokolov I.I. Stress relaxation as a method for estimation of the network structure parameters of cross-linked polyethylene // Proceedings of VIAM. 2015. No. 2. DOI: 10.18577/2307-6046-2015-0-2-12-12. URL: https://www.viam-works.ru/en/journal/2015/2/12
Abstract

A methodology has been developed to define parameters of the topological structure of the polymer network in cross-linked polyethylene by the stress relaxation method. The obtained experimental data were used to calculate parameters of the polymer network of cross-linked polyethylene. Parameters of the topological structure of peroxide cross-linked polyethylene obtained by stress relaxation and equilibrium swelling methods were compared.

Reference list
  1. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  2. Kablov E.N. Himija v aviacionnom materialovedenii [Chemistry aviation materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  3. Kablov E.N. Materialy i himicheskie tehnologii dlja aviacionnoj tehniki [Materials and chemical technologies, aircraft] //Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  4. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  5. Sirotkin O.S., Andrjunina M.A., Bejder Je.Ja. Novye konstrukcionnye i funkcional'nye PCM na osnove termoplastov i tehnologii ih formovanija [New structural and functional PTP-based thermoplastics and their molding technology] //Aviacionnaja promyshlennost'. 2011. №4. S. 12–18.
  6. Petrova G.N., Bejder Je.Ja. Konstrukcionnye materialy na osnove armirovannyh termoplastov [Structural materials on the basis of reinforced thermoplastics] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 31–44.
  7. Nozdrina L.V., Korotkova V.I., Bejder Je.Ja. Termoplastichnye polimery dlja konstrukcionnyh kompozicionnyh materialov [Thermoplastic resins for structural composites] //Konstrukcii iz kompozicionnyh materialov. 1991. №1. S. 9–21.
  8. Ustinov V.A., Bejder Je.Ja. Primenenie kompozicionnyh materialov s termoplastichnoj matricej [The use of composite materials with a thermoplastic matrix] //Konstrukcii iz kompozicionnyh materialov. 1991. №1. S. 24–37.
  9. Petrova G.N., Bejder Je.Ja. Lit'evye termoplastichnye materialy aviakosmicheskogo naznachenija [Molded thermoplastic materials aerospace destination] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 17–30.
  10. Kikel' V.A. Tehnologii sshivanija polijetilena i sravnenie s polipropilenom [Crosslinking technology and comparison of polyethylene and polypropylene] //Cantehnika, otoplenie, kondicionirovanie. 2003. №11. S. 1–4.
  11. Medvedev V.P., Solov'eva Ju.V. Opredelenie parametrov, harakterizujushhih vulkanizacionnuju setku i stepen' sshivanija metodom ravnovesnogo nabuhanija [Determination of the parameters characterizing the vulcanization grid and the degree of crosslinking method of equilibrium swelling]. Volgograd: VGTU. 2009. 12 s.
  12. Medvedev V.P., Ukrainskaja S.I., Solov'eva Ju.V. Opredelenie stepeni relaksacii i ravnovesnogo modulja vysokojelastichnosti sshityh jelastomerov [Determining the degree of relaxation and equilibrium modulus of high elasticity crosslinked elastomers]. Volgograd: VGTU. 2010. 12 s.
  13. Sokolov I.I., Raskutin A.E. Ugleplastiki i stekloplastiki novogo pokolenija [Carbon and fiberglass new generation] //Trudy VIAM. 2013. №4 (viam-works.ru).
  14. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svjazujushhie dlja perspektivnyh metodov izgotovlenija konstrukcionnyh voloknistyh PCM [New polymeric binders for advanced manufacturing methods of structural fiber PCM] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  15. Zheleznjak V.G., Chursova L.V., Grigor'ev M.M., Kosarina E.I. Issledovanie povyshenija soprotivljaemosti udarnym nagruzkam policianurata s modifikatorom na osnove linejnyh termostojkih polimerov [Investigation increase resistance to impact loads polycyanurates modifier based on the linear heat-resistant polymers] //Aviacionnye materialy i tehnologii. 2013. №2. S. 26–28.
  16. Muhametov R.R., Ahmadieva K.R., Kim M.A., Babin A.N. Rasplavnye svjazujushhie dlja perspektivnyh metodov izgotovlenija PCM novogo pokolenija [Melt binders promising methods of manufacture of a new generation of PCM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 260–265.
  17. Dolmatovskij M.G., Sokolov I.I. Osobennosti razrushenija sotovyh panelej so sferoplastikami [Features destruction of honeycomb panels with spheroplastic] //Aviacionnye materialy i tehnologii. 2008. №4. S. 19–24.