On the issue of application of discrete fibers of refractory oxides to form cores of heat-resistant sealing cords
Zimichev A.M., Varrik N.M. On the issue of application of discrete fibers of refractory oxides to form cores of heat-resistant sealing cords // Proceedings of VIAM. 2015. No. 2. DOI: 10.18577/2307-6046-2015-0-2-11-11. URL: https://www.viam-works.ru/en/journal/2015/2/11
Abstract
Possibility of production of continuous cords from short oxide fibers by direct formation of aqueous pulp was investigated. The laboratory unit for production of cords equipped with forming assembly, heat chamber and winding assembly was designed and installed. The experiment showed the possibility in principle to produce cords from short oxide fibers.
Reference list
- Kablov E.N., Shhetanov B.V., Ivahnenko Ju.A., Balinova Ju.A. Perspektivnye armirujushhie vysokotemperaturnye volokna dlja metallicheskih i keramicheskih kompozicionnyh materialov [Prospective reinforcing fibers for high temperature ceramic composites and metal materials] //Trudy VIAM. 2013. №2. St. 05 (viam-works.ru).
- Kablov E.N. Materialy i himicheskie tehnologii dlja aviacionnoj tehniki [Materials and chemical technologies, aircraft] //Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
- Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
- Kablov E.N., Grashhenkov D.V., Isaeva N.V., Solncev S.S. Perspektivnye vysokotemperaturnye keramicheskie kompozicionnye materialy [Promising high-temperature ceramic composite materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 20–24.
- Kobets L.P., Deev I.S. Carbon fibres: structure and mechanical properties //Composites Science and Technology. 1998. Т. 57. №12. С. 1571–1580.
- Grashhenkov D.V., Balinova Ju.A., Tinjakova E.V. Keramicheskie volokna oksida aljuminija i materialy na ih osnove [Ceramic alumina fibers and materials based on them] //Steklo i keramika. 2012. №4. S. 32–36.
- Ivahnenko Ju.A., Babashov V.G., Zimichev A.M., Tinjakova E.V. Vysokotemperaturnye teploizoljacionnye i teplozashhitnye materialy na osnove volokon tugoplavkih soedinenij [High-temperature insulating and heat-proof materials for fiber-based refractory compounds] //Aviacionnye materialy i tehnologii. 2012. №S. S. 380–385.
- Balinova Ju.A., Kirienko T.A. Nepreryvnye vysokotemperaturnye oksidnye volokna dlja teplozashhitnyh, teploizoljacionnyh i kompozicionnyh materialov [Continuous high temperature oxide fibers for thermal protection, thermal insulation and composite materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2012. №4. S. 24–29.
- Sposob poluchenija vysokotemperaturnogo volokna na osnove oksida aljuminija [A method for producing high-fiber alumina-based]: pat. 2212388 Ros. Federacija; opubl. 20.09.2003. Bjul. №34. 6 s.
- Balinova Ju.A. Nepreryvnye polikristallicheskie volokna oksida aljuminija dlja kompozicionnyh materialov [Continuous polycrystalline alumina fibers for composite materials]: Avtoref. dis. k.t.n. M.: VIAM. 2012. 19 s.
- Shhetanov B.V., Shheglova T.M., Balinova Ju.A. Izgotovlenie, struktura i svojstva polikristallicheskih volokon oksida aljuminija [Manufacturing, Structure and properties of polycrystalline alumina fibers] /V sb. materialov 29-j Mezhdunarodnoj konf. «Kompozicionnye materialy v tehnologii». Jalta. 2009. S. 148–150.
- Varrik N.M., Ivahnenko Ju.A., Maksimov V.G. Oksid-oksidnye kompozicionnye materialy dlja gazoturbinnyh dvigatelej (obzor) [Oxide-oxide composite materials for gas turbine engines (review)] //Trudy VIAM. 2014. №8. St. 03 (viam-works.ru)
- Shhetanov B.V., Balinova Ju.A., Ljuljukina G.Ju., Solov'eva E.P. Struktura i svojstva nepreryvnyh polikristallicheskih volokon α-Al2O3 [Structure and properties of continuous fibers of polycrystalline α-Al2O3] //Aviacionnye materialy i tehnologii. 2012. №1. S. 13–17.
- Balinova Ju.A., Shheglova T.M., Ljuljukina G.Ju., Timoshin A.S. Osobennosti formiro-vanija α-Al2O3 v polikristallicheskih voloknah s soderzhaniem oksida aljuminija 99% v prisutstvii dobavok Fe2O3, MgO, SiO2 [Features of forming α-Al2O3 in polycrystalline fibers with an alumina content of 99% in the presence of additives Fe2O3, MgO, SiO2] //Trudy VIAM. 2014. №3. St. 03 (viam-works.ru).
- Basalt fibre rope: pat. 102465389 CN; pabl. 23.05.2012.
- Refractory fiber rope packing: pat. 4581882 US; pabl. 15.04.1986.
- Shnur [Cord]: pat.2233356 Ros. Federacija; opubl. 27.04.2004.
- Heat resistant fibrous products containing ceramic fibers and method of making the same: pat. 3090103 US; pabl.21.05.1963.
- Shheglova T.M., Zimichev A.M., Varrik N.M. Issledovanie obrazcov shnura iz volokon Fiberfrax [The study samples of cord fibers Fiberfrax] //Trudy VIAM. 2014. №9. St. 05 (viam-works.ru).
- www.unifrax.com.
- Sposob poluchenija kombinirovannoj niti na osnove korotkih volokon i ustrojstvo dlja ego osushhestvlenija [A method for producing a combination yarn based short fibers and an apparatus for its implementation]: pat. 2419692 Ros. Federacija; opubl. 27.05.2011 Bjul. №15.
- Papilin N.M., Kapitanov A.F., Volkov V.A., Gladyshev A.Ju., Babashov V.G., Varrik N.M. Obosnovanie receptury voloknistoj suspenzii [Justification formulation of the fiber suspension] //Himicheskie volokna. 2009. №5. S. 31–33.