Parameters that influence the formation of porosity in the products made of polymer composite materials (PCM) produced by out-of-autoclave methods

Dushin M.I., Khrulkov A.V., Karavaev R.Y.
Dushin M.I., Khrulkov A.V., Karavaev R.Y. Parameters that influence the formation of porosity in the products made of polymer composite materials (PCM) produced by out-of-autoclave methods // Proceedings of VIAM. 2015. No. 2. DOI: 10.18577/2307-6046-2015-0-2-10-10. URL: https://www.viam-works.ru/en/journal/2015/2/10
Abstract

Causes of porosity formation in the products made of polymer composite materials prepared by the autoclave and out-of-autoclave methods are discussed in the paper and recommendations for porosity reduction are given.

Reference list
  1. Mihajlin Ju.A. Konstrukcionnye polimernye kompozicionnye materialy [Structural polymer composite materials]. SPb.: Nauchnye osnovy i tehnologi. 2008. 822 s.
  2. Brautman L. Razrushenie i ustalost' [Destruction and fatigue]. M.: Mir. 1978. 153 s.
  3. ASTM D/Void Content of Reinforced Plastic.
  4. Tavares S.S., Michaud V., Manson J.A.E. Through thickness air permeability of prepregs during cure //Composites. A. 2009. V. 40. P. 1587–1596.
  5. Thomas S., Nutt S.R. In situ estimation of though-thickness resin flow using ultrasound //Compos. Sci. Technol. 2008. V. 68. P. 3093–3098.
  6. Tavares S.S., Michaud V., Manson J.A.E. Assessment of semi-impregnated fabrics in honeycomb sandwich structures //Composites. A. 2010. V. 41. P. 8–15.
  7. Jackson K., Crabtree M. Autoclave guality composites tooling for composite from vacuum bag only processing /In: 47-th International SAMPLE symposium. 2002. P. 800–807.
  8. Repecka L., Boyd J. Vacuum-bag-only-curable prepregs that produce void-free parts /In: 47-th International SAMPLE symposium. 2002. P. 1862–1875.
  9. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  10. Kablov E.N., Kondrashov S.V., Jurkov G.Ju. Perspektivy ispol'zovanija uglerodsoderzhashhih nanochastic v svjazujushhih dlja polimernyh kompozicionnyh materialov [Prospects for the use of carbonaceous nanoparticles in binders for polymer composites] //Rossijskie nanotehnologii. 2013. T. 8. №3–4. S. 24–42.
  11. Kablov E.N., Starcev O.V., Deev I.S., Nikishin E.F. Svojstva polimernyh kompozicionnyh materialov posle vozdejstvija otkrytogo kosmosa na okolozemnyh orbitah [Properties of polymer composition-tional materials after exposure to the open space in Earth orbits] //Vse materialy. Jenciklopedicheskij spravochnik. 2012. №11. S. 2–16.
  12. Kablov E.N. Materialy i himicheskie tehnologii dlja aviacionnoj tehniki [Materials and chemical technologies, aircraft] //Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  13. Grashhenkov D.V., Chursova L.V. Strategija razvitija kompozicionnyh i funkcional'nyh materialov [The development strategy of composite and functional materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 231–242.
  14. Hrul'kov A.V., Dushin M.I., Popov Ju.O., Kogan D.I. Issledovanija i razrabotka avto-klavnyh i bezavtoklavnyh tehnologij formovanija PCM [Research and development autoclave and non-autoclave molding technology PCM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 292–301.
  15. Dushin M.I., Hrul'kov A.V., Muhametov R.R. Vybor tehnologicheskih parametrov avtoklavnogo formovanija detalej iz polimernyh kompozicionnyh materialov [The choice of process parameters autoclave molding parts from polymeric composite materials] //Aviacionnye materialy i tehnologii. 2011. №3. S. 20–26.
  16. Jepoksidnoe svjazujushee, prepreg na ego osnove i izdelie, vypolnennoe iz nego [Svyazuyushee epoxy prepreg at its base and a product made therefrom]: pat. 2424259 Ros. Federacija; opubl. 22.10.2009.
  17. Muhametov R.R., Ahmadieva K.R., Kim M.A., Babin A.N. Rasplavnye svjazujushhie dlja perspektivnyh metodov izgotovlenija PCM novogo pokolenija [Melt binders promising methods of manufacture of a new generation of PCM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 260–265.
  18. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svjazujushhie dlja perspektivnyh metodov izgotovlenija konstrukcionnyh voloknistyh PCM [New polymeric binders for advanced manufacturing methods of structural fiber PCM] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  19. Dushin M.I., Hrul'kov A.V., Muhametov R.R., Chursova L.V. Osobennosti izgotovlenija izdelij iz PCM metodom propitki pod davleniem [Especially the manufacture of PCM by pressure impregnation] //Aviacionnye materialy i tehnologii. 2012. №1. S. 18–26.
  20. Dushin M.I., Hrul'kov A.V., Platonov A.A., Ahmadieva K.R. Bezavtoklavnoe formovanie ugleplastikov na osnove prepregov, poluchennyh po rastvornoj tehnologii [Bezavtoklavnogo molding CFRP-based prepregs obtained by mortar technology] //Aviacionnye materialy i tehnologii. 2012. №2. S. 43–48.
  21. Grunenfelder L.K., Nutt S.R. Void formation in composite prepregs – effect of dissolved moisture //Composites Science and Technology. 2010. V. 70. P. 2304–2309.
  22. Kardos J.L., Dudukovic M.P., Dave R. Void growth and resin transport during processing of thermosetting-matrix composites //Adv. Polym. Sci. 1986. V. 80. P. 102–123.
  23. Olivier P., Cottu J.P., Ferret B. Effects of cure cycle pressure and voids on some mechanical properties of carbon/epoxy laminates //Composites. 1995. V. 26 (7). P. 509–515.
  24. Costa M.L., Almedia S.F.M., Rezende M.C. The influence of porosity on the interlaminar shear strength of carbon/epoxy and carbon/bismaleimide fabric laminates //Compos. Sci. Technol. 2001. V. 61. P. 2101–2108.
  25. Campbell F.C., Mallow A.R. Porosity in carbon fiber composites, an overview of causes //J. Adv. Mater. 1994. P. 18–23.
  26. Wood J.R., Bader M.G. Void control for polymer-matrix composites (1) theoretical and experimental evaluation of a diffusion model for the growth and collapse of gas bubbles //Compos. Manuf. 1994. №5(3). P. 149–158.
  27. Scriven L.E. On the dynamics of phase growth //Chen. End Sci. 1959. №10 (1/2). P. 1–13.
  28. Subramanian R.S., Weinberg M.C. The role of convective transport in the dissolution or growth of a gas bubble //J. Chem. Phys. 1980. V. 72(12). P. 6811–6813.
  29. Liu L., Zhang B., Wu Z., Wang D. Effects of cure pressure induced voids on the mechanical strength of carbon/epoxy laminates //J. Mater. Sci. Technol. 2005. V. 21(1). P. 87–91.
  30. Boey F.Y.C., Lye S.W. Void reduction in autoclave processing of thermoset composites part 1: high pressure effects on void reduction //Composites. 1992. V. 23(4). P. 261–265.
  31. Hayward J.S., Harris B. Effect of process variables on the quality of RTM mouldings //Sampe J. 1990. V. 26(3). P. 39–46.
  32. Hayward J.S., Harris B. Effect of vacuum assistance in resin transfer moulding //Compos. Manuf.1990. №1(33). P. 161–166.
  33. Lundstrom T.S., Gebart B.R., Lundemo C.Y. Void formation in RTM /In: The 49-th annual conference. Composite Institute of the Society of the Plastics Industry. 1992. Session 16-F.
  34. Patel N., Lee L.J. Effect of fiber mat architecture on void formation and removal in liquid composite molding //Polym. Compos. 1995. V. 16(5). P. 386–399.
  35. Greszczuk L.B. Effect of voids on strength properties of filamentary composites /In: Proceedings of 22-nd annual meeting of the reinforced plastics. Division of the Society of the Plastics Industry. 1967. P. 20(A-1)–20(A-10).
  36. Rudobashta S.P. Massoperenos v sistemah s tverdoj fazoj [Mass transfer systems with a solid phase]. M.: Himija. 1980. 248 s.
  37. Patel N., Rohatgi V., Lee L.J. Modeling of void formation and removal in liquid composite molding. Part II. Model development //Polym. Compos. 1996. V. 17(1). P. 104–114.
  38. Chen Y.T., Davis H.T., Macosko C.W. Wetting of fiber mats for composite manufacturing. Part I. Visualization experiments AlChE //Polym. Compos. 1995. V. 41(10). P. 2261–2273.
  39. Rohatgi V., Patel N., Lee L.J. Experimental investigation of flow induced microvoids during impregnation of unidirectional stitched fiberglass mat //Polym. Compos. 1996. V. 17(2). P. 161–170.
  40. Patel N., Rohatgi V., Lee L.J. Micro scale flow behavior and void formation mechanism during impregnation through a unidirectional stitched fiberglass //Mat. Polym. Eng. Sci. 1995. V. 35(10). P. 837–851.
  41. Kotov V., Pashhenko E. Kompleks dlja razrabotki i optimizacii tehnologij propitki kompozitnyh konstrukcij [Complex for the development and optimization of composite structures technology impregnation] //Ajerokosmicheskij kur'er. 2010. №3–4. S. 75.
  42. Vojuckij S.S. Fiziko-himicheskie osnovy propityvanija impregnirovanija voloknistyh materialov dispersijami polimerov [Physico-chemical basis impregnation impregnation of fibrous materials polymer dispersions]. M.: Himija. 1969. 334 s.
  43. Vacuum resin impregnation process: pat. 4942013 US; pabl. 17.07.1990.
  44. Double bag vacuum in fusion process: pat. 7413694 US; pabl. 07.12.2000.
  45. Method and device for producing fiber – reinforced components am injection method: pat. 68353 WO; pabl. 20.09.2001.
  46. Sposob izgotovlenija voloknistyh kompozitov vakuumnoj infuziej i ustrojstvo dlja osushhestvlenija sposoba [A method of manufacturing fiber composites vacuum infusion and apparatus for wasp-out the process]: pat. 2480335 Ros. Federacija; opubl. 2006.