Silicium determination in nickel alloys by ICP-AES method in combination with micro-wave preparation
UDC
543.42:661.68
DOI
10.18577/2307-6046-2015-0-12-7-7
Article PDF (Russian)
(484.78 KB)
How to cite
Karachevtsev F.N., Zagvozdkina T.N., Dvoretskov R.M. Silicium determination in nickel alloys by ICP-AES method in combination with micro-wave preparation // Proceedings of VIAM. 2015. No. 12. DOI: 10.18577/2307-6046-2015-0-12-7-7. URL: https://www.viam-works.ru/en/journal/2015/12/7
Keywords
silicon, microwave digestion, nickel alloys, inductively coupled plasma atomic emission spectroscopy, measurement procedure.
Abstract
In various types of nickel alloys silicon is present in a wide concentration range from a few hundredths of a percent in the heat resisting nickel alloys to whole percent in the nickel-based solders. The paper describes a method of measuring the mass fraction of silicon in the nickel-based alloys by atomic emission spectrometry with inductively coupled plasma (ICP-AES) in combination with microwave sample preparation. Compositions of dissolution mixtures and parameters of microwave digestion were selected. Limits of relative measurement error for Si content from 0,01 to 8% don't exceed 2% (±δ, at P=0,95).
Reference list
- Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharo-prochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] //Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
- Kablov E.N., Ospennikova O.G., Petrushin N.V., Visik E.M. Monokristallicheskij zharoprochnyj nikelevyj splav novogo pokoleniya s nizkoj plotnostyu [Single-crystal nickel-based superalloy of a new generation with low-density] //Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 14–25.
- Lomberg B.S., Ovsepyan S.V., Bakradze M.M., Mazalov I.S. Vysokotemperaturnye zharo-prochnye nikelevye splavy dlya detalej gazoturbinnyh dvigatelej [High-temperature heat resisting nickel alloys for details of gas turbine engines] //Aviacionnye materialy i tehnologii. 2012. №S. S. 52–57.
- Shmotin Yu.N., Starkov R.Yu., Danilov D.V., Ospennikova O.G., Lomberg B.S. Novye materialy dlya perspektivnogo dvigatelya OAO «NPO „Saturn”» [New materials for the perspective engine of JSC «NPO „Saturn”»] //Aviacionnye materialy i tehnologii. 2012. №2. S. 6–8.
- Kablov E.N., Ospennikova O.G., Petrushin N.V. Novyj monokristallicheskij intermetallidnyj (na osnove γʹ-fazy) zharoprochnyj splav dlya lopatok GTD [New single crystal heat-resistant intermetallic γʹ-based alloy for GTE blades] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 34–40.
- Kablov E.N. Fiziko-himicheskie i tehnologicheskie osobennosti sozdaniya zharoprochnyh splavov, soderzhashhih renij [Physical and chemical and technological features of creation of the heat resisting alloys containing rhenium] //Vestnik Moskovskogo universiteta. Ser. 2: Himiya. 2005. T. 46. №3. S. 155–167.
- Kablov E.N., Petrushin N.V., Bronfin M.B., Alekseev A.A. Osobennosti monokristallicheskih zharoprochnyh nikelevyh splavov, legirovannyh reniem [Features of the single-crystal heat resisting nickel alloys alloyed by rhenium] //Metally. 2006. №5. S. 47–57.
- Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Litejnye zharoprochnye nikelevye splavy dlya perspektivnyh aviacionnyh GTD [Foundry heat resisting nickel alloys for perspective aviation GTE] //Tehnologiya legkih splavov. 2007. №2. S. 6–16.
- Kablov E.N., Sidorov V.V., Kablov D.E., Rigin V.E., Goryunov A.V. Sovremennye tehnologii polucheniya prutkovyh zagotovok iz litejnyh zharoprochnyh splavov novogo pokoleniya [Modern technologies of receiving the bar stock preparations from foundry heat resisting alloys of new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 97–105.
- Sidorov B.B., Ishodzhanova I.B., Rigin B.E., Folomejkin Yu.I. Ocenka effektivnosti filtratsii pri razlivke slozhnolegirovannogo nikelevogo rasplava [Assessment of efficiency of a filtration when pouring of difficult alloyed nickel fusion] //Elektrometallurgiya. 2011. №11. S. 17–21.
- Sidorov V.V., Rigin V.E., Goryunov A.V., Min P.G., Kablov D.E. Poluchenie Re–Ru-soderzhashhego splava s ispolzovaniem nekondicionnyh othodov [Receiving Re–Ru the containing alloy with use of sub-standard waste] //Metallurgiya mashinostroeniya. 2012. №3. S. 15–17.
- Pripoj na osnove nikelya [Solder on the basis of nickel]: pat. 2452600 Ros. Federacya; opubl. 22.06.2011.
- Pupyshev A.A., Danilova D.A. Ispolzovanie atomno-emissionnoj spektrometrii s induktivno-svyazannoj plazmoj dlya analiza materialov i produktov chernoj metallurgii [Use of nuclear and issue spectrometry with the inductive and connected plasma for the analysis of materials and products of ferrous metallurgy] //Analitika i kontrol. 2007. T. 11. №2–3. S. 131–181.
- Dvoretskov R.M., Karachevcev F.N., Zagvozdkina T.N., Mehanik E.A. Opredelenie himicheskogo sostava vysokolegirovannyh nikelevyh splavov aviacionnogo naznacheniya metodom AES-ISP v sochetanii s mikrovolnovoj probopodgotovkoj [Definition of a chemical composition of the high-alloyed nickel alloys of aviation appointment as the AES-ISP method in combination with microwave preparation of tests] //Zavodskaya laboratoriya. Diagnostika materialov. 2013. T. 79. №9. S. 6–9.
- Karachevtsev F.N., Dvoretskov R.M., Zagvozdkina T.N. Mikrovolnovaya probopodgotovka nikelevyh splavov dya opredeleniya legiruyushhih elementov metodom AES-ISP [Microwave probe preparation of nickel alloying elements using ICP-AES method] //Trudy VIAM. 2014. №11. St. 11 (viam-works.ru).