The irreversible structural modifications of single crystals fine structure of Ni-based superalloys at enduring operation of turbine blades

Nazarkin R.M., Kolodochkina V.G., Ospennikova O.G., Orlov M.R.
Nazarkin R.M., Kolodochkina V.G., Ospennikova O.G., Orlov M.R. The irreversible structural modifications of single crystals fine structure of Ni-based superalloys at enduring operation of turbine blades // Proceedings of VIAM. 2015. No. 12. DOI: 10.18577/2307-6046-2015-0-12-3-3. URL: https://www.viam-works.ru/en/journal/2015/12/3
Abstract

The results of researches of single-crystal rotor blades from cast Ni-based superalloy ZhS32-VI in process of long-time life cycle testing of gas turbine engine (high-pressure turbine) are represented for microstructure and substructure. It is shown that precipitation of TCP-phases particles in the alloy during high-temperature testing is accompanied by the decreasing of crystal lattice constant of γ-solid solution. It is verified by data of x-ray diffraction analysis, x-Ray microanalysis and scanning electron microscopy. The point is proposed that decreasing of alloying element content in the γ-solid solution as result of TCP-phases precipitation (rich with the refractory elements) leads to the fall of the high-temperature resistance of the material. Also, a TCP-phases make negative influence on mechanical properties of the alloy due to the local destruction of coherency for interphase boundaries in zone of development of TCP-phases particles.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Ospennikova O.G. Strategiya razvitiya zharoprochnyh splavov i stalej specialnogo naznacheniya, zashhitnyh i teplozashhitnyh pokrytij [Strategy of development of hot strength alloys and steels special purpose, protective and heat-protective coverings] //Aviacionnye materialy i tehnologii. 2012. №S. S. 19–36.
  3. Kablov E.N., Lomberg B.S., Ospennikova O.G. Sozdanie sovremennyh zharoprochnyh materialov i tehnologij ih proizvodstva dlya aviacionnogo dvigatelestroeniya [Creation of modern heat resisting materials and technologies of their production for aviation engine building] //Krylya Rodiny. 2012. №3–4. S. 34–38.
  4. Orlov M.R. Strategicheskie napravleniya razvitiya Ispytatelnogo centra FGUP «VIAM» [Strategic directions of development of the Test center FSUE «VIAM»] //Aviacionnye materialy i tehnologii. 2012. №S. S. 387–393.
  5. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharo-prochnye splavy novogo pokoleniya [Nickel foundry hot strength alloys of new generation] //Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
  6. Petrushin N.B., Ospennikova O.G., Visik E.M., Rassohina L.I., Timofeeva O.B. Zharoprochnye nikelevye splavy nizkoj plotnosti [Heat resisting nickel alloys of low density] //Litejnoe proizvodstvo. 2012. №6. S. 5–11.
  7. Kablov E.N. Fiziko-mehanicheskie i tehnologicheskie osobennosti sozdaniya zharoprochnyh splavov, soderzhashhih renij [Physicomechanical and technological features of creation of the hot strength alloys, containing reniye] //Vestnik Moskovskogo universiteta. Ser. 2: Himiya. 2005. T. 46. №3. S. 155–167.
  8. 4. Kablov E.N., Muboyadzhyan S.A. Zharostojkie i teplozashhitnye pokrytiya dlja lopatok turbiny vysokogo davleniya perspektivnyh GTD [Heat resisting and heat-protective coverings for turbine blades of high pressure of perspective GTE] //Aviacionnye materialy i tehnologii. 2012. №S. S. 60–70.
  9. Kablov E.N., Petrushin N.V., Bronfin M.B., Alekseev A.A. Osobennosti monokristallicheskih zharoprochnyh nikelevyh splavov, legirovannyh reniem [Features of the single-crystal heat resisting nickel alloys alloyed by rhenium] //Metally. 2006. №5. S. 47–57.
  10. Bondarenko Yu.A., Kablov E.N. Napravlennaya kristallizaciya zharoprochnyh splavov s povyshennym temperaturnym gradientom [The directed crystallization of hot strength alloys with the raised temperature gradient] //MiTOM. 2002. №7. S. 20–23.
  11. Bondarenko Yu.A., Kablov E.N., Morozova G.I. Vliyanie vysokogradientnoj napravlennoj kristallizacii na strukturu i fazovyj sostav zharoprochnogo splava tipa Rene-N5 [Influence of the high-gradient directed crystallization on structure and phase composition of hot strength alloy of the Rene-N5 type] //MiTOM. 1999. №2. S. 15–18.
  12. Morozova G.I. Zakonomernost formirovaniya himicheskogo sostava γ′/γ-matricy mnogokomponentnyh nikelevyh splavov [Pattern of forming of chemical composition γ′/γ-matrix multicomponent nickel alloys] //Doklady Akademii nauk. 1991. T. 320. №6. S. 1413–1416.
  13. Kablov E.N., Petrushin N.V. Kompyuternyj metod konstruirovaniya litejnyh zharoprochnyh nikelevyh splavov [Computer method of designing of cast heat resisting nickel alloys] /V kn. Litejnye zharoprochnye splavy. Effekt S.T. Kishkina /Pod red. E.N. Kablova. M.: Nauka. 2006. S. 56–78.
  14. Ospennikova O.G., Orlov M.R., Kolodochkina V.G., Nazarkin R.M. Strukturnye izmeneniya i povrezhdenie monokristallicheskih rabochih lopatok turbiny v processe resursnyh ispytanij aviacionnogo gazoturbinnogo dvigatelya [Structural changes and injury of single-crystal working turbine blades in the course of resource tests of the aviation gas turbine engine] //Deformaciya i razrushenie materialov. 2014. №8. S. 22–29.
  15. Orlov M.R., Yakimova M.S., Letov A.F. Analiz rabotosposobnosti monokristallicheskih lopatok turbiny vysokogo davleniya v sostave nazemnyh gazoturbinnyh ustanovok [The analysis of operability of single-crystal turbine blades of high pressure as a part of land gas turbine units] //Aviacionnye materialy i tehnologii. 2012. №S. S. 399–407.
  16. Samojlov A.I., Nazarkin R.M., Moiseeva N.S. Opredelenie misfita vo fragmentirovannyh monokristallah nikelevyh zharoprochnyh splavov [Definition miss-fit in fragmental single crystals of nickel hot strength alloys] //Trudy VIAM. 2013. №5. St. 02 (viam-works.ru).
  17. Samojlov A.I., Nazarkin R.M., Moiseeva N.S. Misfit kak istochnik i kriterij rabotosposobnosti zharoprochnyh nikelevyh splavov [Misfit as source and criterion of operability of heat resisting nickel alloys] //Zavodskaya laboratoriya. Diagnostika materialov. 2013. T. 79. №6. S. 33–36.
  18. Kablov E.N., Orlov M.R., Ospennikova O.G. Mehanizmy obrazovanija poristosti v monokristallicheskih lopatkah turbiny i kinetika ee ustranenija pri gorjachem izostaticheskom pressovanii [Mechanisms of formation of porosity in single-crystal turbine blades and kinetics of its elimination at hot isostatic pressing] //Aviacionnye materialy i tehnologii. 2012. №S. S. 117–129.