Comprehensive research of the influence of climatic and operational factors on new gen-eration epoxy binding and polymeric composite materials on its basis

Part 1. Research of the influence of sorbate moisture on epoxy matrix and layered car-bon fiber on its basis
Nikolaev E.V., Barbotko S.L., Andreeva N.P., Pavlov M.R.
Nikolaev E.V., Barbotko S.L., Andreeva N.P., Pavlov M.R. Comprehensive research of the influence of climatic and operational factors on new gen-eration epoxy binding and polymeric composite materials on its basis. Part 1. Research of the influence of sorbate moisture on epoxy matrix and layered car-bon fiber on its basis // Proceedings of VIAM. 2015. No. 12. DOI: 10.18577/2307-6046-2015-0-12-11-11. URL: https://www.viam-works.ru/en/journal/2015/12/11
Keywords
epoxy binding, epoxy matrix, layered carbon fiber, moisture absorption, bonded moisture.
Abstract

Processes of sorption and desorption of moisture by epoxy polymeric matrix and layered carbon fiber on its basis are considered. Moisture diffusion factors are estimated on stages of sorption and desorption. The conclusion is drawn on nature of diffusion in epoxy matrix and in polymeric composite material, on the basis of this matrix. The qualitative analysis of epoxy matrix, in the course of moisture sorption, is carried out by FTIR Spectroscopy. The structure and energy of molecule of epoxy matrix is calculated, at absence and presence of the bonded moisture in its composition. Researches of mechanical properties of polymeric composite materials are conducted at different values of moisture content. Changes of thermophysical properties of layered carbon fiber in the course of moisture sorption and desorption are investigated.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N., Gunyaev G.M. Tumanov A.T. – iniciator sozdaniya kompozitov [Tumanov A.T. – initiator of creation of composites] /V sb. tez. dokl. mezhotrasl. nauch.-tehnich. konf. «Kompozicionnye materialy v aviakosmicheskom materialovedenii». M.: VIAM. 2009. S. 6–9.
  3. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznacheniya. III. Znachimye faktory stareniya [Climatic aging of composite materials of aviation assignment. III. Significant factors of aging] //Deformaciya i razrushenie materialov. 2011. №1. S. 34–40.
  4. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svyazujushhie dlya perspektivnyh metodov izgotovleniya konstrukcionnyh voloknistyh PKM [New polymeric binding for perspective methods of manufacturing of constructional fibrous PCM] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  5. Kirillov V.N., Vapirov Yu.M., Drozd E.A. Issledovanie atmosfernoj stojkosti polimernyh kompozicionnyh materialov v usloviyah atmosfery teplogo vlazhnogo i umerenno teplogo klimata [Research of atmospheric firmness of polymeric composite materials in the conditions of the atmosphere of warm wet and moderately warm climate] //Aviacionnye materialy i tehnologii. 2012. №4. S. 31–38.
  6. Mishra G., Mohapatra S.R., Behera P.R., Dash B., Mohanty U.K., Ray B.C. Environmental stability of GFRP laminated composites: an emphasis on mechanical behaviour //Aircraft Eng. and Aerosp. technol. 2010. V. 82. №4. P. 258–266.
  7. Firefighting and emergency responsestudy of advanced composites aircraft. Objective 2: Firefighting Effectiveness of Technologies and Agents on Composite Aircraft Fires. Distribution A: Approved for public release; distribution unlimited. 88ABW-2012-0190. 2012.
  8. Sugita Yoshino, Winkelmann Charles, La Saponara Valeria. Environmental and chemical degradation of carbon/epoxy lap joints for aerospace applications, and effects on their mechanical performance //Compos. Sci. and Technol. 2010. V. 70. №5. P. 829–839.
  9. Kirillov V.N., Efimov V.A. Problemy issledovaniya klimaticheskoj stojkosti aviacionnyh nemetallicheskih materialov [Problems of research of climatic firmness of aviation non-metallic materials] /V sb.: 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: Yubilejnyj nauch.-tehnich. sbornik. M.: VIAM. 2007. S. 379–388.
  10. Mikols W.J., Seferis J.C., Apicella A., Nicolais L. Evaluation of structural changes in epoxy systems by moisture sorption-desorption and dynamic mechanical studies //Polym. Compos. 1982. V. 3 № 3. P. 118–124.
  11. Nikolaev E.V., Kirillov V.N., Skirta A.A., Grashhenkov D.V. Issledovanie zakonomernostej vlagoperenosa i razrabotka standarta po opredeleniyu koefficienta diffuzii i predelnogo vlagosoderzhaniya dlya ocenki mehanicheskih svojstv ugleplastikov [Study of moisture transport rules and development of a standard on measurement of the diffusion coefficient and moisture content limit to evaluate mechanical properties of carbon fiber reinforced plastics] //Aviacionnye materialy i tehnologii. 2013. №3. S. 44–48.
  12. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznacheniya. I. Mehanizmy stareniya [Climatic aging of composite materials of aviation assignment. I. Aging mechanisms] //Deformaciya i razrushenie materialov. 2010. №11. S. 19–27.
  13. Kirillov V.N., Startsev O.V., Efimov V.A. Klimaticheskaya stojkost i povrezhdaemost polimernyh kompozicionnyh materialov, problemy i puti resheniya [Climatic firmness and damageability of polymeric composite materials, problems and solutions] //Aviacionnye materialy i tehnologii. 2012. №S. S. 412–423.
  14. Efimov V.A., Shvedkova A.K., Korenkova T.G., Kirillov V.N. Issledovanie polimernyh konstrukcionnyh materialov pri vozdejstvii klimaticheskih faktorov i nagruzok v laboratornyh i naturnyh usloviyah [Research of polymeric constructional materials at influence of climatic factors and loadings in laboratory and natural conditions] //Trudy VIAM. 2013. №1. St. 05 (viam-works.ru).
  15. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznachenita. II. Relaksaciya ishodnoj strukturnoj neravnovesnosti i gradient svojstv po tolshhine [Climatic aging of composite materials of aviation assignment. II. Relaxation of initial structural non-equilibrium and gradient of properties on thickness] //Deformaciya i razrushenie materialov. 2012. №6. S. 17–19.
  16. Roulend S. Voda v polimerah [Water in polymers]. M.: Mir. 1984. 555 s.
  17. Zimm В.Н. Simplified Relation Between Thermodynamics and Molecular Distribution Functions for a Mixture //J. Chem. Phys. 1953. V. 21 Р. 934–935.
  18. Zimm В.Н., Lundberg J.L. Sorption of Vapors by High Polymers //J. Phys. Chem. 1956. V. 60. P. 425–428.
  19. Igonin N.G. Issledovanie osobennostej (nefikovskih anomalij) diffuzii vody v polimernyh kompozicionnyh materialah [Research of features (nefikovsky anomalies) water diffusions in polymeric composite materials]. M.: Kompaniya Sputnik. 2008. 182 s.
  20. Panin S.V., Startsev O.V., Krotov A.S. Diagnostika nachalnoj stadii klimaticheskogo stareniya PKM po izmeneniyu koefficienta diffuzii vlagi [Initial Stage Environmental Degradation of the Polymer Matrix Composites Evaluated by Water Diffusion Coefficient] //Trudy VIAM. 2014. №7. St. 09 (viam-works.ru).
  21. Antipov V.V., Startsev O.V., Senatorova O.G. Zakonomernosti vlagoperenosa v SIALah [Patterns moisture transfer in SIAL]//Korroziya: materialy, zashhita. 2012. №3. S. 13–18.
  22. Dao B., Hodgkin J., Krstina J., Mardel J., Tian W. Accelerated aging versus realistic aging in aerospace composite materials. I. The chemistry of thermal aging in a low-temperature-cure epoxy composite //Journal of Applied Polymer Science. 2006. V. 102. №5. Р. 4291–4303.
  23. Tian W., Hodgkin J. Long-Term Aging in a Commercial Aerospace Composite Sample: Chemical and Physical Changes //Journal of Applied Polymer Science. 2010. V. 115. Р. 2981–2985.
  24. Eizenberg D., Kaucman V. Struktura i svojstva vody [Structure and properties of water]. L.: Gidrometeoizdat. 1975. 230 s.
  25. Burikov S.A., Dolenko T.A., Karpov D.M. Vklad rezonansa Fermi v formirovanie valentnoj polosy spektra kombinacionnogo rassejaniya vody [Contribution of resonance of Fermi to forming of valency spectral band of combinational dispersion of water] //Optika i spektroskopiya. 2010. T. 109. №2. S. 306–312.
  26. Bessonova A.P., Stas I.E. Vliyanie vysokochastotnogo elektromagnitnogo polya na fiziko-mehanicheskie svojstva vody i ee spektralnye harakteristiki [Influence of high-frequency electromagnetic field on physical and mechanical properties of water and its spectral characteristics] //Polzunovskij vestnik. 2008. №3. S. 305–309.
  27. Pacaeva S.V. Obratnye zadachi spektroskopii kombinacionnogo rassejaniya sveta v zhidkoj vode [Return problems of spectroscopy of combinational dispersion of light in liquid water]: avtoref. dis. … kand. fiz.-mat. nauk. MGU. 1989. 18 s.