Fireproof fiberglass for interior of passenger aircraft (review)
UDC
678.067.5:614.814.41
DOI
10.18577/2307-6046-2015-0-11-7-7
Article PDF (Russian)
(385.42 KB)
How to cite
Kurnosov A.O., Sokolov I.I., Melnikov D.A., Topunova T.E. Fireproof fiberglass for interior of passenger aircraft (review) // Proceedings of VIAM. 2015. No. 11. DOI: 10.18577/2307-6046-2015-0-11-7-7. URL: https://www.viam-works.ru/en/journal/2015/11/7
Abstract
The article presents information about fiberglass for interior of passenger aircraft developed at VIAM. The basic requirements of fire safety for such materials are pointed out. Methods for determining the combustibility and smoke generation of polymer materials are considered. Main characteristics of fireproof materials based on various types of binders and glass materials are represented. The technology of manufacture of interior panels of different curvature by using the method «crush core» is described.
Reference list
- Davydova I.F., Kavun N.S. Stekloplastiki ‒ mnogofunkcionalnye kompozicionnye materialy [Fibreglasses ‒ multipurpose composite materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 253–260.
- Kirin K.M. Perspektivnye pozharobezopasnye tekstilnye materialy dlya primeneniya v grazhdanskoj aviatsii [Perspective the fire safe textile materials for application in civil aviation]: avtoref. dis. … kand. tehn. M.: GOU VPO RosZITLP. 2004. 16 s.
- Gunyaev G.M., Krivonos V.V., Rumyancev A.F., Zhelezina G.F. Polimernye kompozicionnye materialy v konstrukciyah letatelnyh apparatov [Polymer composire materials in aircraft structure] //Konversiya v mashinostroenii. 2004. №4 (65). S. 65–69.
- Barbotko S.L., Dementeva L.A., Serzhenkov A.A. Gorjuchest steklo- i ugleplastikov na osnove kleevyh prepregov [Flammability glass and carbon fiber based adhesive prepregs] //Klei. Germetiki. Tehnologii. 2008. №7. S. 29–31.
- Surnin E.G., Kondrashov Je.K. Pozharobezopasnye dekorativno-otdelochnye materialy [Fire safe decorative and finishing materials] /V kn. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2002: Jubilejnyj nauch.-tehnich. sb. M.: MISIS–VIAM. 2002. S. 271–281.
- Veshkin E.A., Postnov V.I., Zastrogina O.B., Satdinov R.A. Tehnologiya uskorennogo formovaniya sotovyh panelej interera samoleta [Technology of the accelerated formation of cellular panels of an interior of the plane] //Izvestiya Samarskogo nauchnogo centra Rossijskoj akademii nauk. 2013. T. 15. №4 (4). S. 799–805.
- Avrasin Ya.D., Borodin M.Ya., Kiselev B.A. Stekloplastiki v aviastroenii [Fibreglasses in aircraft industry] //Aviacionnaja promyshlennost'. 1982. №8. S. 80–84.
- Sokolov I.I., Kogan D.I., Raskutin A.E., Babin A.N., Filatov A.A., Morozov B.B. Mnogoslojnye konstrukcii so sferoplastikami [Multilayered designs with the sphere plasticity] //Konstrukcii iz kompozicionnyh materialov. 2014. №1. S. 37–42.
- Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for the aircraft equipment] //Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
- Kablov E.N. Himiya v aviacionnom materialovedenii [Chemistry in aviation materials science] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
- Zastrogina O.B., Shvets N.I., Postnov V.I., Serkova E.A. Fenolformaldegidnye svjazuyushhie novogo pokoleniya dlya materialov interera [Phenolformaldehyde binding new generation for interior materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 265–272.
- Strelnikov S.V., Zastrogina O.B., Veshkin E.A., Shvets N.I. K voprosu o sozdanii vysokoeffektivnyh tehnologij izgotovleniya panelej interera v krupnoserijnom proizvodstve [To a question of creation of highly effective manufacturing techniques of panels of an interior in a large-lot production] //Aviacionnye materialy i tehnologii. 2011. №4. S. 18–24.
- Serkova E.A., Shvets N.I., Zastrogina O.B., Postnov V.I., Petuhov V.I., Barbotko S.L., Veshkin E.A. Bystrootverzhdaemoe fenolformaldegidnoe svyazujushhee, pererabatyvaemoe po «crush-core» tehnologii, dlya pozharobezopasnyh materialov interera [Quickly cured phenolformaldehyde binding, processed on technology «crush-core», for the fire of safe materials of an interior] /V sb. tezisov dokl. HIH konf. «Konstrukcii i tehnologii poluchenija izdelij iz nemetallicheskih materialov». Obninsk. 2010. S. 70–71.
- Dolmatovskij M.G., Sokolov I.I. Osobennosti razrusheniya sotovyh panelej so sferoplastikami [Features of destruction of cellular panels with the sphere plasticity] //Aviacionnye materialy i tehnologii. 2008. №4. S. 19–24.