Features of producing zirconia fibers (review)

Varrik N.M., Ivakhnenko Yu.A.
Varrik N.M., Ivakhnenko Yu.A. Features of producing zirconia fibers (review) // Proceedings of VIAM. 2015. No. 10. DOI: 10.18577/2307-6046-2015-0-10-8-8. URL: https://www.viam-works.ru/en/journal/2015/10/8
Abstract

Data from scientific publications regarding methods of production of zirconia fiber are provided in the article. Zirconia fiber has good prospects for use as high-temperature thermal insulation due to the highest refractoriness among oxide ceramics, high durability and chemical resistance, especially alkalin. Now there are various techniques for producing zirconia fiber, each of them has both merits and demerits. The review includes the description of the main methods according to the data available in information sources.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N. Materialy dlja izdelija «Buran» – innovacionnye reshenija formirovanija shestogo tehnologicheskogo uklada [Materials for the product «Buran» – innovative solutions of forming of the sixth technological way] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
  3. Kablov E.N., Shhetanov B.V., Ivahnenko Ju.A., Balinova Ju.A. Perspektivnye armiruju-shhie vysokotemperaturnye volokna dlja metallicheskih i keramicheskih kompozicionnyh materialov [Perspective reinforcing high-temperature fibers for metal and ceramic composite materials] //Trudy VIAM. 2013. №2. St. 05 (viam-works.ru).
  4. Kablov E.N., Shhetanov B.V., Ivahnenko Ju.A., Balinova Ju.A., Semenova E.V. Volokna dioksida cirkonija dlja novogo pokolenija materialov aviacii i kosmosa [Zirconium dioxide fibers for new generation of materials of aircraft and space] /V sb. materialov XXV Mezhdunarodnoj konf. «Kompozicionnye materialy v promyshlennosti». Jalta. 2005. S. 320–323.
  5. Zimichev A.M., Solov'eva E.P. Volokno dioksida cirkonija dlja vysokotemperaturnogo primenenija [Zirconium dioxide fiber for high-temperature application] //Aviacionnye materialy i tehnologii. 2014. №3. S. 55–61.
  6. Coated zirconia ceramic fibers partially stabilized with yttria: pat. 0885860 EU; pabl. 23.12.1998.
  7. Kamiya K., Takahashi K., Maeda T., Nasu H. Sol-gel-derived CaO- and CeO2-stabilized ZrO2 fibers – conversion process of gel to oxide and tensile strength //Journal of the European Ceramic Society. 1991. V. 7. P. 295–305.
  8. Stabilized tetragonal zirconia fibers and textiles: pat. 3860529 USA; pabl. 14.01.1975.
  9. Process for the preparation of zircon coated zirconia fibers of zircon coated zirconia fibers: pat. 3861947 USA; pabl. 21.01.1975.
  10. www.zircarzirconia.com.
  11. www.shangze.info.
  12. Shhetanov B.V., Balinova Ju.A., Ljuljukina G.Ju., Solov'eva E.P. Struktura i svojstva nepreryvnyh polikristallicheskih volokon α-Al2O3 [Structure and properties of continuous polycrystalline fibers α-Al2O3] //Aviacionnye materialy i tehnologii. 2012. №1. S. 13–17.
  13. Sposob poluchenija vysokotemperaturnogo volokna na osnove oksida aljuminija [Way of receiving high-temperature fiber on the basis of aluminum oxide]: pat. 2212388 Ros. Federacija; opubl. 20.09.2003.
  14. Shhetanov B.V., Kablov E.N., Shheglova T.M. Mehanizm formirovanija stabilizirovan-noj struktury v vysokotermostojkih polikristallicheskih voloknah sistemy Al2O3–SiO2, poluchaemyh po zol'-gel' tehnologii [The mechanism of forming of the stabilized structure in the high-heat-resistant polycrystalline fibers of Al2O3–SiO2 system received on sol-gel of technology] /V sb. materialov XXIV Mezhdunarodnoj konf. «Kompozicionnye materialy v promyshlennosti». Jalta. 2004. S. 324–326.
  15. Marshall D.B., Lange F.F., Morgan P.D. High-strength zirconia fibers //Journal of the American Ceramic Society. 1987. V. 70. №8. P. 187–188.
  16. Zirconium oxide fibers and process for their preparation: pat. 4937212 USA; pabl. 26.01.1990.
  17. Pullar R.C., Taylor M.D., Bhattaccharya A.K. The manufacture of partially-stabilised and fully-stabilised zirconia fibers blow spun from an from an alkoxide derived aqueous sol-gel precursor //Journal of the European Ceramic Society. 2001. V. 21. P. 19–27.
  18. Abe Y., Kudo T., Tomioka H., Gunji T., Nagao Y., Misono T. Preparation of continuous zirconia fibers from polyzirconoxane synthesized by the facile one-pot reaction //Journal of Material Science. 1998. V. 33. P. 1863–1870.
  19. Preparation method of polycrystal zirconia fiber and zirconia/alumina composite fiber: pat. 102465357 China; pabl. 23.05.2012.
  20. Zhang H.B., Edirisinghe M.J. Electrospinning zirconia fiber from a suspension //Journal of the American Ceramic Society. 2006. V. 89. №6. P. 1870–1875.
  21. Qin D., Gu A., Liang G., Yuan L. A facile method to prepare zirconia electrospun fibers with different morphologies and their novel composites based on cyanate ester resin //RSC Advances. 2012. №2. P. 1364–1372.
  22. Korenkov V.V., Rodaev V.V., Shuklinov A.V., Stoljarov R.A., Zhigachev A.O., Tjurin A.I., Lovcov A.R., Razlivalova S.S. Sintez i svojstva mnogofunkcional'nyh keramicheskih nanovolokon, poluchennyh metodom jelektrospinninga [Synthesis and properties of the multifunction ceramic nanofibres received by method of electrospinning] //Vestnik TGU. 2013. T. 18. №6. S. 3156–3159.
  23. Ksapabutr B., Panapoy M. Fabrication of ceramic nanofibers using atrane precursor /In: Nanofibers. Intech. 2010. P. 367–382.
  24. Shida K., Ohara Y., Matsuda M., Suyama Y. Preparation of yttria-stabilized zirconia fibers from a zirconia sol and their properties //Journal of the Ceramic Society of Japan. 2012. V. 120. №11. P. 478–482.