Prospects for the use of titanium alloys in laminated composite materials

Arislanov A.A., Goncharova L.J., Nochovnaya N.A., Goncharov V.A.
Arislanov A.A., Goncharova L.J., Nochovnaya N.A., Goncharov V.A. Prospects for the use of titanium alloys in laminated composite materials // Proceedings of VIAM. 2015. No. 10. DOI: 10.18577/2307-6046-2015-0-10-4-4. URL: https://www.viam-works.ru/en/journal/2015/10/4
Abstract

Prospects for application of titanium alloys for creation of new class of laminated metal-polymers are shown. Comparison of properties of composite materials based on titanium with composite materials based on aluminum and glass plastic is given. The results of research in the field of hybrid materials allow speaking about the effectiveness of use of laminated metal-polymers in modern structures. Special attention is focused on high specific properties of hybrid materials based on titanium alloys. Such laminated composite materials combine high strength and fracture toughness.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period to 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N. Materialy i himicheskie tehnologii dlja aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] //Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  3. Kablov E.N., Karimova S.A., Semenova L.V. Korrozionnaja aktivnost' ugleplastikov i zashhita metallicheskih silovyh konstrukcij v kontakte s ugleplastikom [Corrosion activity ugleplastikov and protection of metal load bearing structures in contact with the ugleplastiky] //Korrozija: materialy, zashhita. 2011. №12. S. 1–7.
  4. Tarasov Ju.M., Antipov V.V. Novye materialy VIAM – dlja perspektivnoj aviacion-noj tehniki proizvodstva OAO «OAK» [The VIAM new materials – for perspective aviation engineering of production of JSC OAK] //Aviacionnye materialy i tehnologii. 2012. №2. S. 5–6.
  5. Kablov E.N., Antipov V.V., Senatorova O.G. Sloistye aljumostekloplastiki SIAL-1441 i sotrudnichestvo s Airbus i TU DELFT [Layered alyumostekloplastiki SIAL-1441 and cooperation with Airbus and TU DELFT] //Cvetnye metally. 2013. №9 (849). S. 50–53.
  6. Antipov V.V., Senatorova O.G., Lukina N.F., Sidel'nikov V.V., Shestov V.V. Sloistye metallopo-limernye kompozicionnye materialy [Layered metalpolymeric composite materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 226–230.
  7. Nochovnaja N.A., Panin P.V., Alekseev E.B., Bokov K.A. Jekonomnolegirovannye titanovye splavy dlja sloistyh metallopolimernyh kompozicionnyh materialov [Ekonomnolegirovannye titanium alloys for layered metalpolymeric composite materials] //Trudy VIAM. 2014. №11. St. 02 (viam-works.ru).
  8. Sokolov I.I., Raskutin A.E. Ugleplastiki i stekloplastiki novogo pokolenija [Ugleplastiki and fibreglasses of new generation] //Trudy VIAM. 2013. №4. St. 09 (viam-works.ru).
  9. Lukina N.F., Dement'eva L.A., Anihovskaja L.I. Kleevye prepregi dlja sloistyh aljumostekloplas-tikov klassa SIAL [Glue prepregs for layered alyumostekloplastikov class SIAL] //Trudy VIAM. 2014. №1. St. 05 (viam-works.ru).
  10. Kablov E.N., Antipov V.V., Senatorova O.G., Lukina N.F. Novyj klass sloistyh aljumostekloplastikov na osnove aljuminijlitievogo splava 1441 s ponizhennoj plotnost'ju [New class layered alyumostekloplastikov on the basis of alyuminiylitiyevy alloy 1441 with lowered density] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 174–183.
  11. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemel'nye jelementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of modern and future high technologies] //Trudy VIAM. 2013. №2. St. 01 (viam-works.ru).
  12. Petrova A.P., Lukina N.F. Klei dlja mnogorazovoj kosmicheskoj sistemy [Glues for reusable space system] //Trudy VIAM. 2013. №4. St. 05 (viam-works.ru).
  13. Dement'eva L.A., Serezhenkov A.A., Lukina N.F., Kucevich K.E. Kleevye prepregi i sloistye materialy na ih osnove [Glue prepregs and layered materials on their basis] //Aviacionnye materialy i tehnologii. 2013. №2. S. 19–21.
  14. Postnov V.I., Senatorova O.G., Karimova S.A., Pavlovskaja T.G., Zhelezina G.F., Kazakov I.A., Abramov P.A., Postnova M.V., Kotov O.E. Osobennosti formovanija krupnogabaritnyh listov metallopolimernyh KM, ih struktura i svojstva [Features of formation of large-size sheets of metalpolymeric KM, their structure and properties] //Aviacionnye materialy i tehnologii. 2009. №4. S. 23–32.
  15. Senatorova O.G, Antipov V.V., Lukina N.F., Sidel'nikov V.V., Shestov V.V., Mit-rakov O.V., Popov V.I., Ershov A.S. Vysokoprochnye treshhinostojkie legkie sloistye aljumostekloplastiki klassa SIAL – perspektivnyj material dlja aviacionnyh konstrukcij [High-strength treshchinostoyky lungs layered alyumostekloplastiki class SIAL – perspective material for aviation designs] //Tehnologija legkih splavov. 2009. №2. S. 28–31.
  16. Fridljander I.N., Senatorova O.G., Lukina N.F., Antipov V.V. Sloistye aljumo-polimernye materialy SIAL [SIAL layered alyumo-polymeric materials] /V kn.: 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: Jubilejnyj nauch.-tehnich. sb. M.: VIAM. 2007. S. 188–192.
  17. Zhu J. et al. Influence of boron addition on microstructure and mechanical properties ofdental cast titanium alloys //Mat. Sci. & Eng. A. 2003. V. 339 (1–2). P. 53–62.
  18. Niinomi M. Recent trends in titanium research and development in Japan //Proc. 12th World Conf. on Titanium. 2011. V. I. P. 30–37.
  19. Goncharov V.A., Fedotov M.Ju., Shienok A.M. Modelirovanie polimernyh kompozicionnyh materialov [Modeling of polymeric composite materials] /V sb. trudov konf. «Novye materialy i tehnologii glubokoj pererabotki syr'ja – osnova innovacionnogo razvitija jekonomiki Rossii». M.: VIAM. 2010. S. 8.
  20. Horev A.I., Belov S.P., Glazunov S.G. Metallovedenie titana i ego splavov [Metallurgical science of titanium and its alloys]. M.: Metallurgija. 1992. 352 s.
  21. Il'in A.A., Kolachev B.A., Pol'kin I.S. Titanovye splavy. Sostav, struktura, svojstva [Titanium alloys. Structure, structure, properties]: Spravochnik. M.: VILS–MATI. 2009. 520 s.