Quantitative analysis of copper in aviation fuel by atomic absorption spectrometry

Mikov D.A., Kravchenko N.G., Petrova V.A., Kutyrev A.E.
Mikov D.A., Kravchenko N.G., Petrova V.A., Kutyrev A.E. Quantitative analysis of copper in aviation fuel by atomic absorption spectrometry // Proceedings of VIAM. 2015. No. 10. DOI: 10.18577/2307-6046-2015-0-10-12-12. URL: https://www.viam-works.ru/en/journal/2015/10/12
Abstract

Procedure of copper quantitative analysis in the fuel after its corrosion attack against structural materials has been developed to improve the methods of aviation fuel quality assessment. Preparation of fuel for the analysis is carried out by mineralization process. The fuel sample is dissolved in concentrated nitric acid in the presence of hydrogen peroxide until the water-fuel phase boundary is disappeared. Copper concentration is measured by atomic absorption spectrometry with the use of acetylene-air flame on the absorption of copper resonance analytical line (324.8 nm). On the basis of the developed procedure VIAM standard STO 1-595-7-461–2015 «Quantitative analysis of copper in the fuel» was published.

Reference list
  1. Bratkov A.A., Seregin E.P., Gorenkov A.F. i dr. Himmotologija raketnyh i reaktivnyh topliv [Himmotologiya of rocket and reactive fuels]. M.: Himija. 1987. 304 s.
  2. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. C. 2–14.
  3. Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] //Nauka i zhizn'. 2010. №4. S. 2–7.
  4. Kablov E.N. Korrozija ili zhizn' [Corrosion or life] //Nauka i zhizn'. 2012. №11. S. 16–21.
  5. Karimova S.A., Pavlovskaja T.G. Razrabotka sposobov zashhity ot korrozii konstrukcij, rabo-tajushhih v uslovijah kosmosa [Development of ways of corrosion protection of the designs working in the conditions of space] //Trudy VIAM. 2013. №4. St. 02 (viam-works.ru).
  6. Shkol'nikova V.M. Topliva. Smazochnye materialy. Tehnicheskie zhidkosti. Assortiment i primenenie [Lubricants. Technical liquids. Range and application]. M.: Tehinform. 1999. S. 62–75.
  7. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  8. Barsukov V.I. Plamenno-jemissionnye i atomno-absorbcionnye metody analiza i instrumental'nye sposoby povyshenija ih chuvstvitel'nosti [Flame and emission and nuclear and absorbing methods of the analysis and tool ways of increase of their sensitivity]. M.: Mashinostroenie. 2004. 172 s.
  9. Butina N.P., Zamjatina Je.R., Zorina L.P. Primenenie atomno-absorbcionnoj spektroskopii dlja opredelenija medi, cinka, magnija i kal'cija v maslah i prisadkah [Application of nuclear and absorbing spectroscopy for definition of copper, zinc, magnesium and calcium in oils and additives] //Neftepererabotka i neftehimija. 1997. №6. S. 21–23.
  10. Privalenko A.N., Balak G.M., Bagramova Je.K. Opredelenie soderzhanija metallov v neftjanyh toplivah metodom atomno-absorbcionnoj spektrometrii [Definition of the content of metals in oil fuels method of nuclear and absorbing spectrometry] /V sb.: Tezisy dokladov Mezhdu-narodnoj nauch.-tehnich. konf. M.: 25 GOSNII Himmotologii. 2014. C. 298–306.
  11. Butina N.P., Zorina L.P. Atomno-absorbcionnoe opredelenie jelementov v tehnologicheskih otlozhenijah s ispol'zovaniem vozdushno-acetilenovogo plameni [Nuclear and absorbing definition of elements in technological deposits with use of acetylene-air flame] //Neftepererabotka i neftehimija. 1998. №1. C. 24–26.
  12. Bricke M.Je. Atomno-absorbcionnyj spektrohimicheskij analiz (Metody analiticheskoj himii) [Nuclear and absorbing spectrochemical analysis (Methods of analytical chemistry)]. M.: Himija. 1982. 224 s.
  13. Prajs V. Analiticheskaja atomno-absorbcionnaja spektroskopija [Analytical nuclear and absorbing spectroscopy]. M.: Mir. 1976. 358 c.
  14. Zagvozdkina T.N., Karachevcev F.N., Dvoreckov R.M. Primenenie model'nyh rastvorov v atomno-absorbcionnom analize [Application of model solutions in the nuclear and absorbing analysis] //Trudy VIAM. 2015. №3. St. 10 (viam-works.ru).
  15. Dvoreckov R.M., Karachevcev F.N., Isachenko Ja.A., Zagvozdkina T.N. Opredelenie os-novnyh i legirujushhih jelementov v termostabil'nyh magnitnyh materialah sistemy RZJe–Fe–Co–B metodom AJeS-ISP [Definition of the main and doping elements in thermostable magnetic materials of RZE-Fe-Co-B system nuclear power plant-ISP method] //Trudy VIAM. 2014. №11. St. 10 (viam-works.ru).
  16. Havezov I., Calev D. Atomno-absorbcionnyj analiz [Nuclear and absorbing analysis]. M.: Himija. 1983. 144 s.
  17. Scott J., Killer F.C.A. The application of microchemical techniques in the Petrochemical and allied industry /Proceedings of the Society for Analytical Chemistry. 1970. V. 7. P. 4–20.
  18. Means E.A., Ratcliffe D. Determination of wear metals in lubricating oils by atomic absorption spectroscopy //At. Absorption Newsletter. 1965. V. 4. P. 174–179.
  19. Sharlo G. Metody analiticheskoj himii [Methods of analytical chemistry]. L.: Himija. 1965. 977 s.