An influence of coupling agent on properties of thermoplastic glass reinforced plastics

Beider E.Ya., Petrova G.N., Izotova T.F.
Beider E.Ya., Petrova G.N., Izotova T.F. An influence of coupling agent on properties of thermoplastic glass reinforced plastics // Proceedings of VIAM. 2014. No. 9. DOI: 10.18577/2307-6046-2014-0-9-7-7. URL: https://www.viam-works.ru/en/journal/2014/9/7
Abstract

Results of investigation of coupling agents chosen for glass fiber reinforced plastics (GFRP) on the basis of thermoplastic heat-resistant binder - polysulfone PSU-150 aimed to get polymer composite materials with advanced properties is given. The influence of such coupling agents as epoxy resins solutions with different epoxy equivalent, rolivsan, furfuryl alcohol, polysulfone etc. was investigated. Mechanical properties of GFRP are shown as a dependence on coupling agent’s na-ture and its quantity. Fireproof characteristics (combustibility, smoke density, heat release) of the developed thermoplastics GFRP and their accordance to domestic (AP-25) and foreign (FAR-25) requirements are considered. It is shown that coupling agent’s nature does not effect on combustibility and smoke density of GFRP but has an influence on their heat release. Recommendations on the use of thermoplastic GFRP based on polysulfone PSU-150 binder are given.

Reference list
  1. Mihajlin Ju.A. Termoustojchivye polimery i polimernye materialy [Heat resistant polymers and polymeric materials]. SPb.: Professija. 2006. S. 267–272.
  2. Bejder Je.Ja., Malyshenok S.V., Petrova G.N. Kompozicionnye termoplastichnye materialy – svojstva i sposoby pererabotki [The composite thermoplastic materials – Properties and processing methods] //Plasticheskie massy. 2013. №7. S. 56–60.
  3. Petrova G.N., Bejder Je.Ja. Konstrukcionnye materialy na osnove armirovannyh termoplastov [Structural materials based on reinforced thermoplastics] //Rossijskij himicheskij zhurnal. 2010. T. LІV. №1. S. 30–40.
  4. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  5. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace Materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  6. Agafonova A.S., Kondrashov S.V. Osobennosti tehnologii izgotovlenija monolitnogo stekloplastika radiotehnicheskogo naznachenija (MSRN) [Features reinforced fiberglass manufacturing technology of Radio destination (MTRD)] //Aviacionnye materialy i tehnologii. 2014. №1. S. 30–33.
  7. Kablov E.N. Himija v aviacionnom materialovedenii [Chemistry aviation materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  8. Komarov G.A. Sostojanie, perspektivy i problemy primenenija PKM v tehnike [Condition, prospects and problems of application of PCM in the art] //Polimernye materialy. 2009. №2. S. 5–9.
  9. Davydova I.F., Kavun N.S. Stekloplastiki – mnogofunkcional'nye kompozicionnye materialy [GRP – multifunctional composite materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 253–260.
  10. Kerber M.L., Vinogradov V.M., Golovkin G.S. i dr. Polimernye kompozicionnye materialy: struktura, svojstva, tehnologija [Polymer composites: Structure, properties and Technology]. SPb.: Professija. 2011. S. 32–33, 104–140, 180–188.
  11. Stepashkin A.A., Churkov D.N. i dr. Poverhnostnaja obrabotka uglerodnyh volokon [Surface treatment of carbon fibers] //Materialovedenie. 2013. №2. S. 44–50.
  12. Bejder Je.Ja., Petrova G.N., Izotova T.F., Barbot'ko S.L. Stekloplastiki na termoplastichnoj matrice [Glass-reinforced thermoplastic matrix on] //Trudy VIAM. 2013. №7. St. 03 (viam-works.ru).
  13. Petrova G.N., Bejder Je.Ja., Izotova T.F., Malyshenok S.V. Kompozicionnye termoplastichnye materialy – sposoby poluchenija i pererabotki [Composite thermoplastic materials – methods of obtaining and processing] //Vse materialy. Jenciklopedicheskij spravochnik. 2013. №10. S. 10–17.
  14. Bejder Je.Ja., Petrova G.N., Izotova T.F., Gureeva E.V. Kompozicionnye termoplastichnye materialy i penopoliimidy [Thermoplastic composite materials and partly penopoliimidy] //Trudy VIAM. 2013. №11. St. 01 (viam-works.ru).
  15. Petrova G.N., Barbot'ko S.L., Bolotina L.M., Chebotarev V.P. i dr. Pozharobezopasnye svojstva polisul'fonov [Fireproof properties of polysulfones] //Plasticheskie massy. 2005. №1. S. 46–48.
  16. Barbot'ko S.L., Vol'nyj O.S., Izotova T.F. Matematicheskoe modelirovanie teplovy-delenija pri gorenii dlja polimernyh kompozicionnyh materialov razlichnoj tolshhiny [Mathematical modeling of heat during combustion to polymer composite materials of different thicknesses] //Pozharovzryvobezopasnost'. 2007. T. 16. №4. S. 16–20.
  17. Korotkov M.M., Izotova T.F., Zuev A.V., Barbot'ko S.L. Vlijanie teplofizicheskih svojstv na pozharobezopasnost' termostojkih polimerov na osnove polisul'fona [Influence of thermo-physical properties on heat-resistant fire safety polysulfone-based polymers] //Pozharovzryvobezopasnost'. 2008. T. 17. №6. S. 11–15.
  18. Shurkova E.N., Vol'nyj O.S., Izotova T.F., Barbot'ko S.L. Issledovanie vozmozhnosti snizhenija teplovydelenija pri gorenii kompozicionnogo materiala putem izmenenija ego struktury [Feasibility study for reducing the combustion heat of the composite material by modifying its structure] //Aviacionnye materialy i tehnologii. 2012. №1. S. 27–30.