Research of samples of the cord from «Fiberfrax» fibers

Shcheglova T.M., Zimichev A.M., Varrik N.M.
Shcheglova T.M., Zimichev A.M., Varrik N.M. Research of samples of the cord from «Fiberfrax» fibers // Proceedings of VIAM. 2014. No. 9. DOI: 10.18577/2307-6046-2014-0-9-5-5. URL: https://www.viam-works.ru/en/journal/2014/9/5
Abstract

Samples of a cord produced by a foreign company were investigated for high-temperature use. Appearance and cord structure, threads of the first and second type as a part of a cord were investigated. In addition, the structure of threads of the first and second type was studied by binocular microscope, SEM and RFA. The linear density of thr cord and its components was determined. The analysis of behavior of samples of threads of the first and second type after calcining at various temperatures was carried out (loss of weight, RFA, SEM, an optical microscope). As a result of the conducted re-search it was found out that for production of Ø8 mm cord with linear density of 18 ktex, two types of threads were used: two threads of 3 mm in diameter with glass fabric warp were used as the core and six threads of ~1.5 mm diameter, reinforced with metal wire as the braid. Each of threads, i.e. the thread of the first type (with the wire) and the thread of the second type (with glass fabric), cons

Reference list
  1. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace Materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  2. Ivahnenko Ju.A., Babashov V.G., Zimichev A.M., Tinjakova E.V. Vysokotemperaturnye tep-loizoljacionnye i teplozashhitnye materialy na osnove volokon tugoplavkih soedinenij [High-temperature and heat-insulating materials based on fibers of refractory compounds] //Aviacionnye materialy i tehnologii. 2012. №S. S. 380–385.
  3. Tinjakova E.V., Grashhenkov D.V. Teploizoljacionnyj material na osnove mullito-korundovyh i kvarcevyh volokon [Thermal insulation material on the basis of mullite-corundum and quartz fibers] //Aviacionnye materialy i tehnologii. 2012. №3. S. 43–46.
  4. Kablov E.N., Shhetanov B.V., Abuzin Ju.A., Ivahnenko Ju.A. Metallicheskie i keramicheskie kompozicionnye materialy [Metal and ceramic composite materials] /V sb. materialov Mezhdunarodnoj nauch.-praktich. konf. «Sovremennye tehnologii – kljuchevoe zveno v vozrozhdenii otechestvennogo aviastroenija». T. 1. Kazan'. 2008. S. 181–188.
  5. Kablov E.N., Grashhenkov D.V., Isaeva N.V., Solncev S.S. Perspektivnye vysokotemperaturnye keramicheskie kompozicionnye materialy [Promising high-temperature ceramic composites] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 20–24.
  6. Kablov E.N., Shhetanov B.V., Ivahnenko Ju.A., Balinova Ju.A. Perspektivnye armirujushhie vysokotemperaturnye volokna dlja metallicheskih i keramicheskih kompozicionnyh materialov [Prospective reinforcing fibers for high temperature ceramic composites and metal materials] //Trudy VIAM. 2013. №2. St. 05 (viam-works.ru).
  7. Grashhenkov D.V., Shhetanov B.V., Tinjakova E.V., Shheglova T.M. O vozmozhnosti ispol'zovanija kvarcevogo volokna v kachestve svjazujushhego pri poluchenii legkovesnogo teplozashhitnogo materiala na osnove volokon Al2O3 [The possibility of using a silica fiber as a binder in the preparation of a lightweight heat-fiber-based material Al2O3] //Aviacionnye materialy i tehnolo-gii. 2011. №4. S. 8–14.
  8. Zimichev A.M., Varrik N.M., Dalin M.A. Izmerenie modulja uprugosti volokon iz tugo-plavkih oksidov [Measurement of modulus fibers of refractory oxides] //Trudy VIAM. 2014. №6. St. 05 (viam-works.ru).
  9. Zimichev A.M., Varrik N.M. Termogravimetricheskie issledovanija nitej na osnove oksida aljuminija [Thermogravimetric studies yarns based on alumina] //Trudy VIAM. 2014. №6. St. 06 (viam-works.ru).
  10. Varrik N.M. Termostojkie volokna i teplozvukoizoljacionnye ognezashhitnye materialy [Heat and sound insulation, heat-resistant fiber and fire-retardant materials] //Trudy VIAM. 2014. №6. St. 07 (viam-works.ru).
  11. Kablov E.N. Materialy dlja izdelija «Buran» – innovacionnye reshenija formirovanija shestogo tehnologicheskogo uklada [Materials for the product «Buran» – innovative solutions forming the sixth technological order] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
  12. Dospehi dlja «Burana». Materialy i tehnologii VIAM dlja MKS «Jenergija–Buran» [Armor for the «Buran». Materials and technologies for VIAM ISS «Energia–Buran»] /Pod obshh. red. E.N. Kablova. M.: Fond «Nauka i zhizn'». 2013. 128 s.
  13. Shhetanov B.V., Ivahnenko Ju.A., Babashov V.G. Teplozashhitnye materialy [Heat-proof materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 12–20.
  14. Arambakam R., Vahedi Tafreshi H. A simple simulation method for designing fibrous insulation materials //Materials & Design. 2013. V. 44. №2. P. 99–106.
  15. Ning Du, Weiwei Sun. Optimal porosity distribution of fibrous insulation International //Journal of Heat and Mass Transfer. 2009. V. 52. №19–20. P. 4350–4357.
  16. Krenkel W., Lamon J. Hight-Temperature Ceramic Materials and Composites /In: 7-th Internatiolal Conference on Ceramic Matrix Composites (HT-CMC 7). 2010. 938 p.
  17. Ceramic Fibers and Coatings. Advanced Materials for the Twenty-First Century Committee on Advanced Fibers for High-Temperature Ceramic Composites. Washington: National Academy Press. 1998. 95 р.
  18. Wilson D.M., Visser L.R. High performance oxide fibers for metal and ceramic composites /In: Processing of fibers & Сomposites. Barga. 2000. 31 p.
  19. Parlier M., Ritti M.-H., Jankowiak A. Potential and Perspectives for Oxide-Oxide Composites //Journal Aerospacelab. 2011. №3. Р. 1–12.
  20. Веб-сайт компании Johns Manville (США) www.jm.com.
  21. Веб-сайт компании VitCas (Великобритания) www.vitcas.com.
  22. Веб-сайт международного холдинга Unifrax www.unifrax.com.
  23. Bunsell A.R. Oxide fibers for high-temperature reinforcement and insulation //JOM. 2005. V. 57. №2. Р. 48–51.