Oxide-oxide composites for gas-turbine engines

Varrik N.M., Ivakhnenko Yu.A., Maximov V.G.
Varrik N.M., Ivakhnenko Yu.A., Maximov V.G. Oxide-oxide composites for gas-turbine engines // Proceedings of VIAM. 2014. No. 8. DOI: 10.18577/2307-6046-2014-0-8-3-3. URL: https://www.viam-works.ru/en/journal/2014/8/3
Abstract

Ceramic composite oxide-based materials attract the attention of the developers for use in environments where metal materials exhibit a tendency to creep and oxidation. High-temperature ceramic composites, methods of obtaining and properties of the re-sulting materials are the object of special attention at international conferences and congresses on ceramics in the last fifteen years. Aluminum oxide is one of the most promising ceramic materials for a wide range of applications in extreme conditions thanks to its combination of high hardness, heat re-sistance, chemical inertness, with its accessibility and efficiency. However, the use of alumina-based materials in loaded conditions is limited for the low impact resistance, typical for ceramics. Rapid crack propagation under shock loads reduces the reliability of the materials, so the material engineers, conduct research mechanisms of crack propagation, offer many different additives for oxide matrices and processing methods, contrib

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Turchenkov V.A., Baranov D.E., Gagarin M.V., Shishkin M.D. Metodicheskij podhod k provedeniju jekspertizy materialov [Methodical approach to the examination of materials] //Aviacionnye materialy i tehnologii. 2012. №1. S. 47–53.
  3. Grashhenkov D.V., Shhetanov B.V., Tinjakova E.V., Shheglova T.M. O vozmozhnosti ispol'zovanija kvarcevogo volokna v kachestve svjazujushhego pri poluchenii legkovesnogo teplozashhitnogo materiala na osnove volokon Al2O3 [The possibility of using a silica fiber as a binder in the preparation of a lightweight heat-fiber-based material Al2O3] //Aviacionnye materialy i tehnologii. 2011. №4. S. 8‒14.
  4. Ivahnenko Ju.A., Babashov V.G., Zimichev A.M., Tinjakova E.V. Vysokotemperaturnye teploizoljacionnye i teplozashhitnye materialy na osnove volokon tugoplavkih soedinenij [High-temperature and heat-insulating materials based on fibers of refractory compounds] //Aviacionnye materialy i tehnologii. 2012. №S. S. 380–385.
  5. Zimichev A.M., Varrik N.M. Termogravimetricheskie issledovanija nitej na osnove oksida aljuminija [Thermogravimetric studies yarns based on alumina] //Trudy VIAM. 2014. №6. St. 06 (viam-works.ru).
  6. Kablov E.N., Shhetanov B.V., Ivahnenko Ju.A., Balinova Ju.A. Perspektivnye armirujushhie vysokotemperaturnye volokna dlja metallicheskih i keramicheskih kompozicionnyh materialov [Prospective reinforcing fiber for high temperature ceramic composites and metal materials] //Trudy VIAM. 2013. №2. St. 05 (viam.works.ru).
  7. Kablov E.N., Grashhenkov D.V., Isaeva N.V., Solncev S.S., Sevast'janov V.G. Perspektivnye vysokotemperaturnye keramicheskie kompozicionnye materialy [Promising high-temperature ceramic composites] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 20–24.
  8. Grashchenkov D.V., Balinova Yu.A., Tinyakova E.V. Aluminum Oxide Ceramic Fibers and Materials Based on them //Glass and Ceramics. 2012. V. 69. №3–4. P. 130–133.
  9. Basargin O.V., Shcheglova T.M., Kolyshev S.G., Nikitina V.Yu., Maksimov V.G., Babashov V.G. Determination of the high-temperature strength of ceramic oxide materials //Glass and Ceramics. 2013. V. 70. №1–2. P. 43–46.
  10. Papilin N.M., Kapitanov A.F., Babashov V.G., Varrik N.M. Basis for the Formula for the Fibre Suspension //Fibre Chemistry. 2009. V. 41. №5. P. 314–316.
  11. Milejko S.T., Kijko V.M., Kolchin A.A., Novohatskaja N.I., Van K.V., Bazyleva O.A., Bondarenko Ju.A. Polzuchest' oksid-nikelevyh kompozitov [Creep-nickel oxide composites] //Kompozity i nanostruktury. 2009. №4. S. 5–18.
  12. Tanaka R. Research and Development of Ultra-High Temperature Materials in Japan //Materials at High Temperatures. 2000. V. 17. №4. P. 457–464.
  13. Krenkel W., Lamon J. High-Temperature Ceramic Materials and Composites 7-th International Conference on High-Temperature Ceramic Matrix Composites (HT-CMC 7). Bayreuth: 2010. 938 p.
  14. Bender B., Pan M. Selection of a Toughened Mullite for a Miniature Gas Turbine Engine //Ceram. Eng. and Sci. Proc. 2009. T. 30. №2. P. 167–175.
  15. Strength, Fracture Toughness and Slow Crack Growth of Zirconia /Alumina Composites at Elevated Temperature, NASA/TM-2003-212108 www.nasa.gov.
  16. Chokshi A. Densification and High Temperature Deformation on Oxide Ceramics //Key Engineering Materials. 2009. V. 395. P. 39–54.
  17. Günther R., Klassen T., Dickau B., Gärtner F., Bartels A., Bormann R. Advanced Alumina Composites Reinforced with Ti-based Alloy //Journal of the American Ceramic Society. 2001. V. 84. №7. P. 1509–1513.
  18. Keramicheskij kompozicionnyj material i sposob ego poluchenija [The ceramic composite material and method for its preparation]: pat. 1802522 Ros. Federacija; opubl. 20.07.2006.
  19. Sposob poluchenija keramicheskogo kompozita [A method for producing ceramic composite]: pat. 5482673 SShA; opubl. 09.01.1996.
  20. Poluchenie vysokotemperaturnyh materialov metodom jekzotermicheskogo sinteza i posledujushhego dinamicheskogo uplotnenija [Preparation of high-temperature materials by exothermic synthesis and subsequent dynamic compaction]: pat. 5129801 SShA; opubl. 14.07.1992.
  21. Sposob izgotovlenija izdelij iz korundovoj keramiki [Method of manufacture of alumina ceramics]: pat. 2379257 Ros. Federacija; opubl. 20.01.2010.
  22. Xinying Tenga, Hanlian Liu, Chuanzhen Huang. Effect of Al2O3 Particle Size on the Mechanical Properties of Alumina-based Ceramics //Mater. Sci. Eng. A. 2007. V. 452–453. P. 545–551.
  23. Ceramic Material for High-Temperature Service: pat. 7723249 US; opubl. 25.05.2010.
  24. Anciferov V.N., Porozova S.E., Kul'met'eva V.B., Krohaleva E.G. Keramicheskij material na osnove nanokristallicheskogo poroshka ZrO2, stabilizirovannogo koncentratom RZJe [Ceramic material based on nanocrystalline powder ZrO2, stabilized with lanthanide concentrate] //Ogneupory i tehnicheskaja keramika. 2011. №3. S. 3–9.
  25. Sostav shihty dlja izgotovlenija keramicheskogo materiala zernistogo stroenija iz dioksida cirkonija [Composition of the charge for the manufacture of ceramic granular structure of zirconia]: pat. 2249570 Ros. Federacija; opubl. 20.01.2004.
  26. Kompozicionnyj keramicheskij material [The composite ceramic material]: pat. 2341494 Ros. Federacija; opubl. 20.12.2008.
  27. Heyi Ge, Jianye Liu, Xianqin Hou. Effects of ZrO2 Fibers on the Mechanical Properties of Nano ZrO2/Al2O Ceramic Composites //Advanced Materials Research. 2012. V. 455–456. P. 645–649.
  28. Superplastic Extrusion of Ultra Fine-grained 3Y–ZrO2/Al2O3 Ceramic for Turbine Disk Materials //Science Forum. 2007. V. 551–552. P. 501–506.
  29. Lukin E.S. Poluchenie nanostrukturirovannyh poroshkov chastichno stabilizirovannogo dioksida cirkonija dlja keramiki s vysokoj mehanicheskoj prochnost'ju [Preparation of nanostructured powders of partially stabilized zirconia ceramic with high mechanical strength] //Steklo i keramika. 2010. №4. S. 18–21.
  30. Asadi S., Abdizadeh H., Vahidshad Y. Effect of Crystalline Size on the Structure of Copper Doped Zirconia Nanoparticles Synthesized via Sol-Gel //Journal of Nanoctructures. 2012. V. 2. P. 205–212.
  31. Chang-Ju Ho, Wei-Hsing Tuan. Phase stability and Microstructure Evolution of Yttria-stabilized Zirconia during Firing in a Reducing Atmosphere //Ceramics International. 2011. V. 37. P. 1401–1407.
  32. Material oksid aljuminija – mullit – oksid cirkonija i ego poluchenie [Material alumina – mullite – zirconia and acquisition]: pat. 9514492 Koreja; opubl. 02.12.1995.
  33. Nizkotemperaturnoe formovanie mullita s ispol'zovaniem alkoksidov kremnija i aljuminija [The low-temperature molding of mullite using silicon alkoxides and aluminum]: pat. 4687652 SShA; opubl. 18.08.1987.
  34. Sposob poluchenija poroshka keramicheskogo kompozicionnogo materiala [A method for producing ceramic composite powder]: pat. 2292320 Ros. Federacija; opubl. 27.01.2007.
  35. Vysokoprochnoe stojkoe k izmeneniju temperatury keramicheskoe izdelie iz mullita i sposob ego poluchenija [High strength resistant to changes in temperature of the mullite ceramic article and a method for its preparation]: pat. 4421861 Germanija; opubl. 20.12.1983.
  36. Vysokoprochnyj treshhinostojkij oksidnyj keramicheskij kompozit [Ductile crack resistant oxide ceramic composite]: pat. 5948516, SShA; opubl. 07.09.1999.
  37. Mnogoslojnye nanostruktury, detali i sposoby ih poluchenija [Multilayer nanostructures, parts and processes for their preparation]: pat. 2005/079370 SShA; opubl. 14.04.2005.
  38. Krishnamurthy R., Rankin J., Sheldon B.W. Effect of Oxidation on Crack Deflection in SiC/Al2O3 Laminated Ceramic Composites //Journal of the American Ceramic Society. 2005. V. 88. №5. P. 1362–1365.
  39. Uprochnennyj voloknami keramomatrichnyj kompozicionnyj jelement i sposob ego poluchenija [Fiber reinforced composite keramomatrichny element and manufacturing method thereof]: pat. 5601674 SShA; opubl. 11.02.1997.
  40. Sposob poluchenija keramomatrichnogo kompozita [Method for producing a composite keramomatrichnogo]: pat. 7153379 SShA; opubl. 26.12.2006.
  41. Ruggles-Wrenn M.B., Laffey P.D. Creep Behavior in Interlaminar Shear of Nextel 720/alumina Ceramic Composite at Elevated Temperature in Air and in Steam //Composites Science and Technology. 2008. V. 68. №10–11. P. 2260–2266.
  42. Mall S., Ahn J.-M. Frequence Effects on Fatigue Behavior of Nextel 720/alumina at Room Temperature //Journal of the European Ceramic Society. 2008. V. 28. №14.
  43. P. 2783–2789.
  44. Tomaszewski H., Weglarz H., Wajler A. Multilayer Ceramic Composites with High Failure Resistance //Journal of the European Ceramic Society. 2007. V. 27. №23.
  45. P. 1373–1377.
  46. Hay R.S., Zawada L., Cinibulk M., Zelina J. Evaluation of Oxide-Oxide Composites in a Novel Combustor Wall Application //International Journal of Applied Ceramic Technology. 2005. V. 2. №2. P. 122–132.
  47. Vysokotemperaturnaja keramomatrichnaja teploizoljacija [High temperature insulation keramomatrichnaya]: pat. 6287511 SShA; opubl. 11.09.2001.
  48. Gibridnyj keramicheskij material, sostojashhij iz izoljacionnogo i konstrukcionnogo keramicheskih sloev [Hybrid ceramic material consisting of insulating and structural ceramic layers]: pat. 6733907 SShA; opubl. 11.05.2004.
  49. Keramicheskij material, imejushhij keramomatrichnyj kompozitnyj sloj, i sposob ego poluchenija [Ceramic material having keramomatrichny composite layer and its production method]: pat. 7291407 SShA; opubl. 06.11.2007.
  50. Ogneupornaja keramicheskaja voloknistaja izoljacija i sposob ee poluchenija [Refractory ceramic fiber insulation and method thereof]: 6183852 SShA; opubl. 06.02.2001.
  51. Keramicheskaja izoljacija [Ceramic insulation]: pat. 6417125 SShA; opubl. 09.07.2002.
  52. www.siemens.com.