Spektrofotometric definition niobium in the heat resisting nickel alloys containing tantalum

Goundobin N.V., Titov V.I., Pilipenko L.V., Dvoretskov R.M.
Goundobin N.V., Titov V.I., Pilipenko L.V., Dvoretskov R.M. Spektrofotometric definition niobium in the heat resisting nickel alloys containing tantalum // Proceedings of VIAM. 2014. No. 8. DOI: 10.18577/2307-6046-2014-0-8-10-10. URL: https://www.viam-works.ru/en/journal/2014/8/10
Abstract

The technique definitions of mass fraction Nb in heat resisting nickel alloys in a range of concentration of 0,5–3,5% of weights by absorption spectrofotometrical method is developed at the simultaneous maintenance in alloys Ta (0,5–6,0% of weights). For increase of accuracy and cleanliness of carrying out of analysis Nb and Ta preliminary separates from disturbe components and from basis of alloy by phenilarsenium acid. The disturbe cous of Zr and Hf, what separates together with Nb and Ta, separetes with binding it’s a stable complex with a reagent complexon III. The analysis is conducted with a reagent sulphonitrazo E by spectrofotomttrical measurement of optical density of a solution on length of a wave λ=560 nanometers. Calculation of maintenance Nb is made on the standard sample of a nickel alloy with the certified maintenance Nb spent through all stadies of the analysis with addition in its a standart solution Ta in quantity equal its maintenance in the analyzed alloy.

Reference list
  1. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokolenija [Casting nickel superalloys new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 36–52.
  2. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih perera-botki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  3. Kablov E.N., Mubojadzhjan S.A. Teplozashhitnye pokrytija dlja lopatok turbiny vysokogo davlenija perspektivnyh GTD [Thermal barrier coatings for turbine blades of high pressure promising GTD] //Metally. 2012. №1. S. 5–13.
  4. Kablov E.N., Sidorov V.V., Kablov D.E., Rigin V.E., Gorjunov A.V. Sovremennye tehnologii poluchenija prutkovyh zagotovok iz litejnyh zharoprochnyh splavov novogo pokolenija [Modern technologies for bar stock of casting superalloys new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 97–105.
  5. Petrushin N.V., Svetlov I.L., Samoylov A.I., Morozova G.I. Physicochemical properties and creep strength of a single crystal of nickel-base superalloy containing rhenium and ruthenium //J. Mat. Res. (formerly metallkd). 2010. V. 101. №5. P. 594–600.
  6. Kablov E.N., Bondarenko Ju.A., Echin A.B., Surova V.A. Razvitie processa napravlennoj kristallizacii lopatok GTD iz zharoprochnyh splavov s monokristallicheskoj i kompozicionnoj strukturoj [The development process of directional solidification of GTE blades with single crystal superalloys and composite structure] //Aviacionnye materialy i tehnologii. 2012. №1. S. 3–8.
  7. Kablov E.N., Ospennikova O.G., Bazyleva O.A. Materialy dlja vysokoteplonagruzhennyh detalej gazoturbinnyh dvigatelej [Materials for high-thermal components of gas turbine engines] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. C. 13–19.
  8. Morozova G.I., Timofeeva O.B., Petrushin N.V. Osobennosti struktury i fazovogo so-stava vysokorenievogo zharoprochnogo splava [Features of the structure and phase composition vysokorenievogo superalloy] //MiTOM. 2009. №2. (644). S. 10–16.
  9. Kablov E.N., Petrushin N.V., Nazarkin R.M. Designing of intermetallic Ni3Al-based superalloy /In: 9-th liege conf. materials for advanced power engineering. 2010. P. 646–651.
  10. Kablov E.N., Ospennikova O.G., Sidorov V.V., Rigin V.E. Proizvodstvo lityh prutkovyh (shihtovyh zagotovok) iz sovremennyh litejnyh vysokozharoprochnyh splavov [Production of cast semifinished (blanks of charge) from the modern foundry alloys highly heat] /V sb. trudov nauchn.-tehn. konf. «Problemy i perspektivy razvitija metallurgii i mashinostroenija s ispol'zovaniem zavershennyh fundamental'nyh issledovanij i NIOKR». Ekaterinburg: Nauka Servis. 2011. T. 1. S. 31–38.
  11. Ospennikova O.G., Svetlov I.L. Vysokotemperaturnye Nb–Si kompozity – zamena monokristallicheskim nikelevym zharoprochnym splavam [High-Nb-Si composites - replacing a single crystal nickel-base superalloy] //Dvigatel'. 2010. №5(71). S. 36–37.
  12. Kishkin S.T., Petrushin N.V., Svetlov I.L. Zharoprochnye jevtekticheskie splavy [Heat-resistant eutectic alloys] /V sb. Aviacionnye materialy na rubezhe HH–HHI vekov. M.: VIAM. 1994. S. 252–258.
  13. Lomberg B.S., Ovsepjan S.V., Bakradze M.M. Novyj zharoprochnyj nikelevyj splav dlja diskov gazoturbinnyh dvigatelej (GTD) i gazoturbinnyh ustanovok (GTU) [New heat resistant nickel alloy disc turbine engine (GTE) and gas turbine units (GTU)] //Materialovedenie. 2010. №7. S. 24–28.
  14. Evgenov A.G., Nerush S.V. Tehnologija poluchenija poroshkov i polufabrikatov pripoev dlja diffuzionnoj vakuumnoj pajki, poluchennyh metodom optimizacii rasplava [Technology for producing powders and semi solders for the diffusion of vacuum brazing, obtained by optimizing the melt] /V sb. tezisov dokladov VI Vserossijskоj nauch.-tehn. konf. molodyh specialistov. Sekcija 3. Tehnologicheskaja. Ufa. 2011. S. 162.
  15. Mubojadzhjan S.A., Aleksandrov D.A., Gorlov D.S., Egorova L.P., Bulavinceva E.E. Zashhitnye i uprochnjajushhie ionno-plazmennye pokrytija dlja lopatok i drugih otvetstvennyh detalej kompressora GTD [Protecting and strengthening the ion-plasma coatings for blades and other critical parts of the compressor turbine engine] //Aviacionnye materialy i tehnologii. 2012. №S. S. 71–81.
  16. Mubojadzhjan S.A., Aleksandrov D.A., Gorlov D.S. Ionno-plazmennye i nanoslojnye jerozionnostojkie pokrytija na osnove karbidov i nitridov metallov [Ion-plasma and Nanolayer erosionproofed coatings based on carbides and nitrides] //Metally. 2010. №5. S. 39–51.
  17. Kablov E.N., Mubojadzhjan S.A. Zharostojkie i teplozashhitnye pokrytija dlja lopatok turbiny vysokogo davlenija perspektivnyh GTD [Heat-resistant and heat-resistant coatings for high-pressure turbine blades promising GTD] //Aviacionnye materialy i tehnolo-gii. 2012. №S. S. 60–70.
  18. Mubojadzhjan S.A. Zashhitnye pokrytija dlja detalej gorjachego trakta GTD [Protective coatings for turbine engine hot section parts] //Vse materialy. Jenciklopedicheskij spravochnik. 2011. №3. S. 26–30. №4. S. 13–20.
  19. Mosheer R. Analytical Chemistry of Niobium and tantalum. N.-Y. Pergamon Press. 1964. P. 78.
  20. Chugaev L.A. Issledovanija v oblasti kompleksnyh soedinenij [Research in the field of complex compounds]. M.: Nauka. 1962. T. 1. S. 10.
  21. Golubeva I.A., Dobkina V.M. Opredelenie i analiz niobija i tantala [Identification and analysis of niobium and tantalum]. M.: NII inf. Mincvetmet SSSR. 1971.
  22. Elinson S.V. Spektrofotometrija niobija i tantala [Spectrophotometry of niobium and tantalum]. M.: Atomizdat. 1973. 288 s.
  23. Gibalo I.M. Analiticheskaja himija niobija i tantala [Analytical chemistry of niobium and tanta-lum]. M.: Nauka. 1967. 352 s.