Abstract

Advantages of repair technologies with use of adhesives materials are shown. The main properties of the domestic and foreign epoxy adhesives used at carrying out number of rescue and recovery operations are given: for elimination of failures and carrying out preventive works on vessels, oil and gas pipelines; in the aviation industry, including cellular designs, and also for the solution of actual problem of car repairs.

Reference list
  1. Petrova A.P., Lukina N.F., Dement'eva L.A., Tjumeneva T.Ju., Avdonina I.A., Zhadova N.S. Klei dlja aviacionnoj tehniki [Adhesives for aircraft] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 46–52.
  2. Sharova I.A., Petrova A.P. Obzor po materialam mezhdunarodnoj konferencii po klejam i germetikam (WAC-2012, Francija) [Browse by materials of the international conference on adhesives and sealants (WAC-2012, France)] //Trudy VIAM. 2013. №8. St. 06 (viam-works.ru).
  3. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  4. Kablov E.N. Himija v aviacionnom materialovedenii [Chemistry aviation materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  5. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace Materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  6. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svjazujushhie dlja perspektivnyh metodov izgotovlenija konstrukcionnyh voloknistyh PKM [New polymeric binders for advanced manufacturing techniques of structural fi-brous PKM] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  7. Dement'eva L.A., Serezhenkov A.A., Lukina N.F., Kucevich K.E. Kleevye prepregi i sloistye materialy na ih osnove [The adhesive prepreg and laminates based on their] //Aviacionnye materialy i tehnologii. 2013. №2. S. 19–21.
  8. Vilenc V.S. Remont kleevyh soedinenij v uslovijah jekspluatacii [Repair adhesive joints in operation] //Klei. Germetiki. Tehnologii. 2004. №6. S. 26–29.
  9. Vilenc V.S., Dement'eva L.A Primenenie kleev pri remonte sotovyh konstrukcij [Application of adhesives in the repair of cellular structures] //Klei. Germetiki. Tehnologii. 2006. №2. S. 24–26.
  10. Vilenc V.S. Osobennosti remonta defektov tipa «otsloenie–rassloenie» na sotovyh konstrukcijah iz aljuminievyh splavov i kompozitnyh materialov v uslovijah jekspluatacii [Features of repair of defects such as «peeling-bundle» on the honeycomb structures made of aluminum alloys and composite materials under operating conditions] //Klei. Germetiki. Tehnologii. 2008. №11. S. 14–17.
  11. Kulikov V.V. Kleevye soedinenija v izdelijah serii «Il» [Adhesive compound product series «Il»] //Klei. Germetiki. Tehnologii. 2009. №1. S. 32–33.
  12. Anihovskaja L.I. Klei i materialy na ih osnove dlja remonta konstrukcij aviacionnoj tehniki [Adhesives and materials on their basis to repair aircraft structures] //Klei. Germetiki. Tehnologii. 2006. №2. S. 21–23.
  13. Lukina N.F., Dement'eva L.A., Petrova A.P., Serezhenkov A.A. Konstrukcionnye i teplostojkie klei [Structural and heat-resistant adhesives] //Aviacionnye materialy i tehnologii. 2012. №S. S. 328–335.
  14. Petrova A.P., Lukina N.F., Sharova I.A. Ocenka prochnosti kleevyh soedinenij, vypolnennyh jepoksidnymi klejami, pri vozdejstvii razlichnyh faktorov [Evaluation of the strength of adhesive joints made of epoxy adhesives, under the influence of various factors] //Vse materialy. Jenciklopedicheskij spravochnik. 2013. №8. S. 28–34.
  15. Sharova I.A., Lukina N.F. Zazorozapolnjajushhij jepoksidnyj klej holodnogo otver-zhdenija [Zazorozapolnyayuschy cold curing epoxy adhesive] //Klei. Germetiki. Tehnologii. 2012. №3. S. 10–12.
  16. Lukina N.F., Sharova I.A., Shuklina O.V., Chursova L.V. Novye razrabotki v oblasti kleev aviacionnogo naznachenija [New developments in the field of adhesives aviation applications] //Vse materialy. Jenciklopedicheskij spravochnik. 2013. №2. S. 9–13.
  17. Avdonina I.A., Lukina N.F. Bystrootverzhdajushhijsja jepoksidnyj klej VK-93 holodnogo otverzhdenija [Fast hardening epoxy VC-93 cold-curing] //Klei. Germetiki. Tehnologii. 2009. №3. S. 14–17.
  18. Jepoksidnaja kleevaja kompozicija [Epoxy adhesive composition]: pat. 2368636 Ros. Federacija; opubl. 27.09.2009.
  19. Zhadova N.S., Tjumeneva T.Ju., Sharova I.A., Lukina N.F. Perspektivnye tehnologii dlja vremennogo operativnogo remonta aviacionnoj tehniki [Promising technologies for temporary operative repair of aviation equipment] //Aviacionnye materialy i tehnologii. 2013. №2. S. 67–70.
  20. Sharova I.A., Zhadova N.S., Lukina N.F. Klejashhie materialy i tehnologii dlja vremennogo operativnogo remonta sotovyh agregatov iz polimernyh kompozicionnyh materialov [Adhesives and technologies for the repair of cellular interim operational units of the polymer composites] //Klei. Germetiki. Tehnologii. 2012. №5. S. 36–39.
  21. Gladkih S.N., Kolobkova V.M., Kuznecova L.I. Bystrootverzhdajushhiesja kleevye so-stavy holodnogo otverzhdenija [The fast cold curing adhesives] //Stroitel'nye i dorozh-nye mashiny. 2006. №9. S. 37–38
  22. Smirnov V.S., Parahina N.N., Muroh A.F., Hamidulova Z.S., Milov V.I., Aronovich D.A., Rogacheva I.P., Sineokov A.P., Knjazev E.F. Primenenie kleevyh materialov pri remonte dejstvujushhih gazoprovodov [Application of adhesives in the repair of existing pipelines] //Klei. Germetiki. Tehnologii. 2009. №9. S. 22–25.