Research the influence of temperature and humidity factors on change of fire safety characteristics for polymeric composite materials which are subject to climatic aging
UDC
678.747.2:536.46
DOI
10.18577/2307-6046-2014-0-7-12-12
Article PDF (Russian)
(524.02 KB)
How to cite
Skrylyov N.S., Volnyj O.S., Abramov D.V., Shurkova E.N. Research the influence of temperature and humidity factors on change of fire safety characteristics for polymeric composite materials which are subject to climatic aging // Proceedings of VIAM. 2014. No. 7. DOI: 10.18577/2307-6046-2014-0-7-12-12. URL: https://www.viam-works.ru/en/journal/2014/7/12
Abstract
The influence of climatic aging factors (temperature and humidity) on change of characteristics of fire safety for standard representatives of polymeric composite mate-rials is investigated. It is shown that after exposure at elevated temperature and humidity, depending on the chemical nature of polymeric matrix, characteristics of smoke density and heat release can considerably variation, and change of characteristics can occur as towards improvement, and deterioration.
Reference list
- Efimov V.A., Shvedkova A.K., Koren'kova T.G., Kirillov V.N. Issledovanie polimernyh konstrukcionnyh materialov pri vozdejstvii klimaticheskih faktorov i nagruzok v laboratornyh i naturnyh uslovijah [Investigation of polymeric structural materials under the influence of climatic factors and stress in laboratory and field conditions] //Trudy VIAM. 2013. №1. St. 05 (viam-works.ru).
- Kablov E.N., Kirillov V.N., Zhirnov A.D., Starcev O.V., Vapirov Ju.M. Centry dlja klimaticheskih ispytanij aviacionnyh PKM [Centers for climatic test aircraft RMB] //Aviacionnaja promyshlennost'. 2009. №4. S. 36–46.
- Kablov E.N., Grashhenkov D.V., Erasov V.S., Anchevskij I.Je., Il'in V.V., Val'ter R.S. Stend dlja ispytanija na klimaticheskoj stancii GCKI krupnogabaritnyh konstrukcij iz PKM [Stand for testing climate station GTSKI large structures of PCM] /V sb. dokl. IX Mezhdunarod. nauch. konf. po gidroaviacii «Gidroaviasalon–2012». 2012. S. 122–123.
- Kirillov V.N., Efimov V.A., Barbot'ko S.L., Nikolaev E.V. Metodicheskie osobennosti provedenija i obrabotki rezul'tatov klimaticheskih ispytanij polimernyh kompozicionnyh materialov [Methodological features and processing of results of environmental tests of polymeric composite materials] //Plasticheskie massy. 2013. №1. S. 37–41.
- Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Kirillov V.N., Efimov V.A., Shvedkova A.K., Nikolaev E.V. Issledovanie vlijanija klimaticheskih faktorov i mehanicheskogo nagruzhenija na strukturu i mehanicheskie svojstva PKM [Investigation of the influence of climatic factors and mechanical loading on the structure and mechanical properties of the PCM] //Aviacionnye materialy i tehnologii. 2011. №4. S. 41–45.
- Barbot'ko S.L. Pozharobezopasnost' aviacionnyh materialov [Fire safety of aircraft materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 431–439.
- Barbot'ko S.L., Nagaev A.S. K voprosu ob obespechenii pozharnoj bezopasnosti vneshnego kontura samoletov [On the issue of fire safety outer contour aircraft] /V sb. dokladov VIII nauch. konf. po gidroaviacii «Gidroaviasalon-2010». Chast' II. M.: CAGI. 2010. S. 107–110.
- Barbot'ko S.L., Shurkova E.N. O pozharnoj bezopasnosti materialov, ispol'zuemyh dlja izgotovlenija vneshnego kontura samoletov [On fire safety of materials used for the manufacture of the outer contour aircraft] //Pozharovzryvobezopasnost'. 2011. T. 20. №10. S. 19–24.
- Barbot'ko S.L., Shurkova E.N., Vol'nyj O.S., Skryljov N.S. Ocenka pozharnoj bezopasnosti polimernyh kompozicionnyh materialov dlja vneshnego kontura aviacionnoj tehniki [Evaluation of fire safety of polymeric composite materials for the outer contour aircraft] //Aviacionnye materialy i tehnologii. 2013. №1. S. 56–59.
- GOST 16363–98. Sredstva ognezashhitnye dlja drevesiny. Metody opredelenija ognezashhitnyh svojstv [Tools retardants for wood. Methods for determination of flame retardant properties].
- The Impact of Thermal Aging on the Flammability of Electric Cables. Prepared by S.P. Nowlen //NUREG/CR-5619 SAND90-2121 Sandia National Laboratories. 1991. 44 p. http://pbadupws.nrc.gov/docs/ML0625/ML062510133.pdf.
- Tian W., Hodgkin J. Long-Term Aging in a Commercial Aerospace Composite Sample: Che-mical and Physical Changes //Journal of Applied Polymer Science. 2010. V. 115. P. 2981–2985.
- Skryljov N.S., Vol'nyj O.S., Postnov V.I., Barbot'ko S.L. Issledovanie vlijanija teplovyh faktorov klimata na izmenenie harakteristik pozharobezopasnosti polimernyh kompozicionnyh materialov [Investigation of influence of thermal factors on climate change in the characteristics of fire safety of polymeric composite materials] //Trudy VIAM. 2013. №9. St. 05 (viam-works.ru).
- Barbotko S.L. Ways of providing fire safety of aviation materials //Russian Journal of General Chemistry. 2011. T. 81. №5. S. 1068–1074.
- Shurkova E.N., Vol'nyj O.S., Izotova T.F., Barbot'ko S.L. Issledovanie vozmozhnosti snizhenija teplovydelenija pri gorenii kompozicionnogo materiala putem izmenenija ego struktury [Feasibility study for reducing the combustion heat of the composite material by modifying its structure] //Aviacionnye materialy i tehnologii. 2012. №1. S. 27–30.
- Composite materials handbook. V.1. Polymer matrix composites guidelines for characterization of structural materials, MIL-HDBK-17-1F. 2002. 586 p.
- STP 1-595-20-100–2002. Metod opredelenija tropikoustojchivosti v laboratornyh uslovijah [Method for determination of tropic in the laboratory].
- GOST 9.719–94. Edinaja sistema zashhity ot korrozii i starenija. Materialy polimernye. Metody ispytanij na starenie pri vozdejstvii vlazhnogo tepla, vodjanogo i soljanogo tumana [Unified system of corrosion and aging. Polymeric materials. Methods of test for aging when exposed to damp heat, water and salt fog].
- GOST 9.707–81. Edinaja sistema zashhity ot korrozii i starenija. Materialy polimernye. Metody uskorennyh ispytanij na klimaticheskoe starenie [Unified system of corrosion and aging. Polymeric materials. Methods for accelerated aging tests on climatic].
- Aviacionnye pravila. Glava 25. Normy letnoj godnosti samoletov transportnoj kategorii [Aviation Regulations. Chapter 25. Airworthiness standards transport category airplanes]. 3-e izd. OAO Aviaizdat. 2009. 274 s.
- Barbot'ko S.L., Kirillov V.N., Shurkova E.N. Ocenka pozharnoj bezopasnosti polimernyh kompozicionnyh materialov aviacionnogo naznachenija [Evaluation of fire safety of polymeric composite materials aviation applications] //Aviacionnaja promyshlennost'. 2013. №2. S. 55–58.
- OST 1 90094–79. Polimernye materialy. Metod opredelenija gorjuchesti dekorativno-otdelochnyh i konstrukcionnyh polimernyh materialov [Polymeric materials. Method for determining the flammability of decorative finishing and engineering plastics].
- Kirillov V.N., Efimov V.A., Shvedkova A.K., Aleksashin V.N., Zuev A.V., Nikolaev E.V. Issledovanie vlijanija klimaticheskih faktorov i mehanicheskogo nagruzhenija na strukturu i mehanicheskie svojstva ugleplastika KMU-11TR [Investigation of the influence of climatic factors and mechanical loading on the structure and mechanical properties of CFRP CMU-11TR] /V sb. dokl. VIII nauch. konf. po gidroaviacii «Gidroaviasalon-2010». Chast' II. M.: CAGI. 2010. S. 111–115.