Industrial development of high-strength alloy V-1469 of Al–Cu–Li–Mg system

Klochkov G.G., Grushko O.E., Klochkova Y.Y., Romanenko V.A.
Klochkov G.G., Grushko O.E., Klochkova Y.Y., Romanenko V.A. Industrial development of high-strength alloy V-1469 of Al–Cu–Li–Mg system // Proceedings of VIAM. 2014. No. 7. DOI: 10.18577/2307-6046-2014-0-7-1-1. URL: https://www.viam-works.ru/en/journal/2014/7/1
Abstract

This paper presents results of researches of industrial sheets, plates, extrusions and rolling rings from new high-strength corrosion-resistant alloy V-1469 with low density based on Al–Cu–Li–Mg–Ag system.

Reference list
  1. Fridljander I.N. Vospominanija o sozdanii aviakosmicheskoj i atomnoj tehniki iz aljuminievyh splavov [Memories of creating aerospace and nuclear technology of aluminum alloys]. M.: Nauka. 2005. 277 s.
  2. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  3. Antipov V.V., Senatorova O.G., Tkachenko E.A., Vahromov R.O. Aljuminievye deformiruemye splavy [Aluminium wrought alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 167–182.
  4. Fridljander I.N., Grushko O.E., Antipov V.V., Kolobnev N.I., Hohlatova L.B. Aljuminijlitievye splavy [Alyuminiylitievye alloys] /V sb. 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: Jubilejnyj nauchn.-tehn. sb. M.: VIAM. 2007. S. 163–171.
  5. Rioja R.J., Denzer D.K., Mooy D., Venema G. Lighter and Stiffer Materials for Use in Space Vehicles /In: Proceedings of the 13-th International Conference on Aluminum Alloys (ICAA-13). 2012. P. 593–598.
  6. Rioja R., Liu J. The evolution of Al–Li base products for aerospace and space applications //Metallurgical and Materials Transactions A. 2012. V. 43. №9. P. 3325–3337.
  7. Na J., Xiang G., Zheng Z.Q. Microstructure evolution of aluminum-lithium alloy 2195 undergoing commercial product //Transactions of nonferrous metals society of China. 2010. P. 740–745.
  8. Mukhopadhyay A.K. Compositional Characterization of Cu-Rich Phase Particles Present in As-Cast Al–Cu–Mg (Li) Alloys Containing Ag //Metallurgical and materials transactions A. 1999. V. 30a. №7. P. 1693–1704.
  9. Zheng Z.Q., Chen X.Z., Chen Z.G., Li S.C., Wei X.Y. The element effects on microstructure and mechanical properties in Al–Cu–Li alloy after thermal exposure /In: Pro-ceedings of the 10-th International Conference on Aluminum Alloys (ICAA-10). 2006. P. 1931–1936.
  10. Bakavos D., Prangnell P.B., Bes B., Eberl F. The effect of silver on microstructural evolution in two 2xxx series Al-alloys with a high Cu: Mg ratio during aging to a T8 temper //Mat. Sci. Eng. 2008. V. 491. P. 214–223.
  11. Shamraj V.F., Grushko O.E., Timofeev V.N., Lazarev Je.M., Klochkova Ju.Ju., Gordeev A.S. Strukturnye sostojanija materiala pressovok i listov splava sistemy Al–Cu–Li, legirovannogo serebrom [Structural state of the material compacts and alloy sheets of Al–Cu–Li, doped with silver] //Metally. 2009. №6. C. 53–59.
  12. Shamray V., Grushko O., Timofeev V., Lazarev E., Klochkova J. Structural Evolution in Aluminum–Copper–Lithium–Magnesium Alloy Sheets During Processing /In: The 12-th International Conference of Aluminium Alloys (ICAA-12). 2010. P. 2141–2146.
  13. Klochkova Ju.Ju., Grushko O.E., Lancova L.P., Burljaeva I.P., Ovsjannikov B.V. Osvoenie v promyshlennom proizvodstve polufabrikatov iz perspektivnogo aljuminijlitievogo splava V-1469 [Development of industrial production of semi-finished alloy in perspective alyuminiylitievogo-1469] //Aviacionnye materialy i tehnologii. 2011. №1. S. 8–12.
  14. Antipov V.V., Kolobnev N.I., Hohlatova L.B. Razvitie aljuminijlitievyh splavov i mnogostupenchatyh rezhimov termicheskoj obrabotki [Development alyuminiylitievyh alloys and multi-heat treatment] //Aviacionnye materialy i tehnologii. 2012. №S. S. 183–195.
  15. Fridljander I.N., Grushko O.E., Shamraj V.F., Klochkov G.G. Vysokoprochnyj konstrukcionnyj Al–Cu–Li–Mg splav ponizhennoj plotnosti, legirovannyj serebrom [High strength structural Al–Cu–Li–Mg alloy reduced density doped silver] //MiTOM. 2007. №6(624). S. 3–7.
  16. Kablov E.N., Antipov V.V., Senatorova O.G., Lukina N.F. Novyj klass sloistyh aljumostekloplastikov na osnove aljuminij-litievogo splava 1441 s ponizhennoj plotnost'ju [New class of layered alyumostekloplastikov based on aluminum-lithium alloy 1441 with a reduced density] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 174–183.
  17. Kablov E.N., Antipov V.V., Senatorova O.G. Sloistye aljumostekloplastiki SIAL-1441 i sotrudnichestvo s Airbus i TU Delft [Layered alyumostekloplastiki Sial-1441 and cooperation with Airbus and TU Delft] //Cvetnye metally. 2013. №9 (849). S. 50–53.
  18. Antipov V.V., Senatorova O.G., Sidel'nikov V.V. Issledovanie pozharostojkosti sloistyh gibridnyh aljumostekloplastikov klassa SIAL [Flammability Study of layered hybrid class alyumostekloplastikov Sial] //Aviacionnye materialy i tehnologii. 2011. №3. S. 36–41.
  19. Erasov V.S., Nuzhnyj G.A., Grinevich A.V., Terehin A.L. Treshhinostojkost' aviacionnyh materialov v processe ispytanija na ustalost' [Fracture toughness of aircraft materials during fatigue test] //Trudy VIAM. 2013. №10. St. 06 (viam-works.ru).
  20. Magnusen P.E., Mooy D.C., Yocum L.A., Rioja R.J. Development of high toughness sheet and extruded products for airplane fuselage structures /In: Proceedings of the 13-th International Conference on Aluminum Alloys (ICAA-13). 2012. P. 535–540.
  21. Karabin L.M., Bray G.H., Rioja R.J., Venema G. Al–Li–Cu–Mg (Ag) products for lower wing skin applications /In: Proceedings of the 12-th International Conference on Aluminum Alloys (ICAA-12). 2012. P. 529–534.
  22. Elagin V.I. Sostojanie i puti povyshenija treshhinostojkosti vysokoprochnyh aljuminievyh splavov [Condition and ways to improve fracture toughness of high-strength aluminum alloys] //MiTOM. 2002. №9. S. 10–15.
  23. Polmear I.J. Aluminium alloys – a century of age hardening //Materials forum. 2004. V. 28. P. 1–14.
  24. Kolobnev N.I., Hohlatova L.B., Oglodkov M.S., Klochkova Ju.Ju. Vysokoprochnye splavy sistemy Al–Cu–Li s povyshennoj vjazkost'ju razrushenija dlja samoletnyh konstrukcij [High-strength alloys of Al–Cu-Li with high fracture toughness for aircraft structures] //Cvetnye metally. 2013. №9. S. 66–71.
  25. Cheng Y., Feng Y.D., Xiang Y.X. Solution Treatment on Mechanical Properties and Microstructures of Al–Li–Cu Alloy //J. Material Sci. Eng. 2012. V. 1. P. 1–5.
  26. Lukina E.A., Alekseev A.A., Antipov V.V., Zajcev D.V., Klochkova Ju.Ju. Primenenie diagramm fazovyh prevrashhenij pri starenii dlja optimizacii rezhimov starenija v Al–Li splavah V-1469, 1441 //Metally. 2009. №6. S. 60–67.
  27. Lukina E.A., Alekseev A.A., Antipov V.V., Zaitsev D.V., Klochkova Y.Y. Application of the Diagrams of Phase Transformations during Aging for Optimizing the Aging Conditions for V-1469 and 1441 Al–Li Alloys [Application diagrams of phase transformations during aging for optimization of aging in Al–Li alloys B-1469, 1441] /In: Proceedings of the 12-th International Conference of Aluminium Alloys (ICAA-12). 2010. P. 1984–1989.