Heat-resistant fibers and heat and sound insulating fireproof materials

Varrik N.M.
Varrik N.M. Heat-resistant fibers and heat and sound insulating fireproof materials // Proceedings of VIAM. 2014. No. 6. DOI: 10.18577/2307-6046-2014-0-6-7-7. URL: https://www.viam-works.ru/en/journal/2014/6/7
Abstract

Article contains the review and defines tendencies in the field of development of heat and sound insulating fireproof materials for aircraft. Scientific literature data on creation of the plane thermal insulation conforming to modern requirements of fire safety for aircraft are provided. Types of fibrous materials and designs of heat-insulating systems are considered.

Reference list
  1. Kablov E.N. Tendencii i orientiry innovacionnogo razvitija Rossii [Trends and bench-marking innovation development in Russia]: Sb. nauchno-informacionnyh materialov. M.: VIAM. 2013. 543 s.
  2. Dospehi dlja «Burana». Materialy i tehnologii VIAM dlja MKS «Jenergija–Buran» [Armor for the «Buran». Materials and technologies for VIAM ISS «Energia-Buran»] /Pod obshh. red. E.N. Kablova. M.: Fond «Nauka i zhizn'». 2013. 128 s.
  3. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  4. Grashhenkov D.V., Chursova L.V. Strategija razvitija kompozicionnyh i funkcional'nyh materialov [Development Strategy composite and functional materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 231–242.
  5. Barbot'ko S.L. Pozharobezopasnost' aviacionnyh materialov [Fire safety of aircraft materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 431–439.
  6. Barbot'ko S.L., Kirillov V.N., Shurkova E.N. Ocenka pozharnoj bezopasnosti polimernyh kompozicionnyh materialov aviacionnogo naznachenija [Evaluation of fire safety of polymeric composite materials aviation applications] //Aviacionnye materialy i tehnologii. 2012. №3. S. 56–63.
  7. Grashhenkov D.V., Shhetanov B.V., Tinjakova E.V., Shheglova T.M. O vozmozhnosti ispol'zovanija kvarcevogo volokna v kachestve svjazujushhego pri poluchenii legkovesnogo teplozashhitnogo materiala na osnove volokon Al2O3 [The possibility of using a silica fiber as a binder in the preparation of a lightweight heat-fiber-based material Al2O3] //Aviacionnye materialy i tehnologii. 2011. №4. S. 8–14.
  8. Aviacionnye materialy [Aircraft materials]: Spravochnik v 13-ti tomah. T. 9. Teplozashhitnye, teploizoljacionnye i kompozicionnye materialy, vysokotemperaturnye nemetallicheskie pokrytija [Heat protection, thermal insulation and composite materials, high-temperature non-metallic coatings]. M.: VIAM. 2011. S. 31.
  9. Ivahnenko Ju.A., Babashov V.G., Zimichev A.M., Tinjakova E.V. Vysokotemperaturnye teploizoljacionnye i teplozashhitnye materialy na osnove volokon tugoplavkih soedinenij [High-temperature and heat-insulating materials based on fibers of refractory compounds] //Aviacionnye materialy i tehnologii. 2012. №S. S. 380–385.
  10. Tinjakova E.V., Grashhenkov D.V. Teploizoljacionnyj material na osnove mullito-korundovyh i kvarcevyh volokon [Thermal insulation material on the basis of mullite-corundum and quartz fibers] //Aviacionnye materialy i tehnologii. 2012. №3. S. 43–46.
  11. Federal Register. 14 CFR Part 25 – Airworthness standards. Transport category airplanes /Federal Aviation Administration. Certification Specifications for Large Aero-planes – CS-25 /ED Decision 2003/2/RM Final 17/10/2003 /In: European Aviation Safety Agency. 2003. 473 p.
  12. Aviacionnye pravila. Glava 25. Normy letnoj godnosti samoletov transportnoj kategorii [Aviation Regulations. Chapter 25. Airworthiness standards transport category airplanes] /Mezhgosudarstvennyj aviacionnyj komitet. 3-e izd. s popravkami 1–6. OAO Aviaizdat. 2009. 274 s.
  13. Coated air duct insulation sheets and the like and the method of coating such sheets: pat. 6399186 US; pabl. 04.06.2002.
  14. Burn through Resistant Systems for Transportation, Especially Aircraft: pat. 6565040 US; pabl. 20.05.2003.
  15. Fiberglass Mat, Method and Laminate: pat. 6883575 US; pabl. 26.04.2005.
  16. Reinforced Insulation Product and System Suitable for Use in an Aircraft: pat. 7278608 US; pabl. 09.10.2007.
  17. Modularized Insulation, Systems, Apparatus and Methods: pat. 7083147 US; pabl. 01.08.2006.
  18. Aircraft Insulation Systems and Methods: pat. 2236412 European; pabl. 31.03.2010.
  19. www.hi-tempinsulation.com.
  20. Ognestojkij sloistyj zvukoteploizolirujushhij material [Fireproof material layered zvukoteploizoliruyuschy]: pat. 2465145 Ros. Federacija; opubl. 27.10.2012. Bjul. №30. S. 7.
  21. Kablov E.N. Himija v aviacionnom materialovedenii [Chemistry aviation materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  22. Polimernaja teplootrazhajushhaja kompozicija dlja pokrytija [Polymer heat-reflecting coating composition]: pat. 2467042 Ros. Federacija; opubl. 07.06.2011.